journal article·2023-11Open access

Plasma Treated AR-Glass Fibres in Experimental Reinforced Composites with Three Silanes: A Study on Mechanical Properties

Madeline J. Y. Yon, Jukka P. Matinlinna, James K. H. Tsoi, Pekka K. Vallittu, Lippo V. J. Lassila

Silicon· Volume 15· Issue 16

Abstract

Purpose To compare and contrast mechanical properties of experimental alkali-resistant (AR) glass fibre-reinforced composites (FRCs) silanised with one of three functional trialkoxysilanes: 3-methacryloxypropyltrimethoxysilane (3-MPS), 8-methacryloxypropyltrimethoxysilane (8-MOS) and 3-acryloxypropyltrimethoxysilane (3-APS). The experimental AR-FRCs were silanised with or without plasma pretreatment. Materials and Methods Continuous unidirectional AR-glass fibres (ARcoteX® 5326 2400tex, Owen Corning) were cleansed ultrasonically, treated either with or without cold plasma (Piezobrush® PZ2, Relyon Plasma, Germany), then silanised by immersion for 10 min in activated, hydrolysed silane solution containing either 3-MPS, 8-MOS or 3-APS. The fibre bundles were next air-dried (24 h), and dried in vacuum oven (80 °C, 5 kPa, 2 h), producing 6 types of silanised AR-glass fibres. Next, silanised AR-glass fibres were laminated with a resin matrix, bis-GMA:TEGDMA at 60:40 wt%, CQ at 0.7 wt%, DMAEMA at 0.7 wt% for 10 min and paired randomly in rovings of two in stainless steel moulds (2 mm × 2 mm × 25 mm) to prepare an AR-FRC beam specimen (n = 16). All specimens were light-cured from the top and bottom directions for 60 s (Elipar S10, 3 M ESPE). Half of the samples (n = 8) underwent accelerated artificial ageing by immersion in boiling water (100 °C, for 16 h). Finally, 12 experimental AR-FRC groups were produced. All specimens were subjected to the three-point bending test with the upper surface (facing curing light) towards the cross-head. After testing, fibres, silanised and non-silanised, were inspected under a scanning electron microscope (SU1510, Hitachi, Tokyo, Japan). Statistical analysis was performed with three-way ANOVA and the Tukey post hoc test at α = 0.05. Results The flexural modulus, flexural strength, and fracture work of the materials were significantly affected by silane type (p < 0.05) and artificial ageing (p < 0.001). Plasma treatment on AR-glass fibres significantly reduces flexural modulus of FRCs (p < 0.001) and slows the plasticising effect of artificial ageing on FRCs. Conclusion Long chain silanes impart higher flexural strength and lower flexural modulus to AR-FRCs. While artificial ageing halves flexural strength and plasticises them, plasma surface pre-treatment of AR-glass fibres before silanisation reduces the plasticising effect.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing and 3D Printing Technologies · Dental materials and restorations · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (45)

Show source-provided references
1. Behl S, Raju Rajan G, Ellakwa A, Farrar P, Prusty BG (2020) Physical and mechanical characterisation of flowable dental composites reinforced with short aspect ratio micro-sized S-Glass fibres. Mater Sci Eng C Mater Biol Appl 111:110771. https://doi.org/10.1016/j.msec.2020.11077110.1016/j.msec.2020.110771 ↗
2. Vallittu PK (1998) Some aspects of the tensile strength of undirectional glass fibre-polymethyl methacrylate composite used in dentures. J Oral Rehabil 25(2):100–105. https://doi.org/10.1046/j.1365-2842.1998.00235.x10.1046/j.1365-2842.1998.00235.x ↗
3. Perea-Lowery L, Vallittu PK (2018) Framework design and pontics of fiber-reinforced composite fixed dental prostheses - An overview. J Prosthodont Res 62(3):281–286. https://doi.org/10.1016/j.jpor.2018.03.00510.1016/j.jpor.2018.03.005 ↗
4. Matinlinna JP, Lung CYK, Tsoi JKH (2018) Silane adhesion mechanism in dental applications and surface treatments: A review. Dent Mater 34(1):13–28. https://doi.org/10.1016/j.dental.2017.09.00210.1016/j.dental.2017.09.002 ↗
5. Rosen MR (1978) From treating solution to filler surface and beyond: the life history of a silane coupling agent. J Coatings Technol 50(644):70–82
6. Garoushi S, Vallittu PK, Lassila LV (2007) Short glass fiber reinforced restorative composite resin with semi-inter penetrating polymer network matrix. Dent Mater 23(11):1356–1362. https://doi.org/10.1016/j.dental.2006.11.01710.1016/j.dental.2006.11.017 ↗
7. Tezvergil A, Lassila LV, Vallittu PK (2003) The effect of fiber orientation on the thermal expansion coefficients of fiber-reinforced composites. Dent Mater 19(6):471–477. https://doi.org/10.1016/s0109-5641(02)00092-110.1016/s0109-5641(02)00092-1 ↗
8. Callaghan DJ, Vaziri A, Nayeb-Hashemi H (2006) Effect of fiber volume fraction and length on the wear characteristics of glass fiber-reinforced dental composites. Dent Mater 22(1):84–93. https://doi.org/10.1016/j.dental.2005.02.01110.1016/j.dental.2005.02.011 ↗
9. Lassila LV, Nohrström T, Vallittu PK (2002) The influence of short-term water storage on the flexural properties of unidirectional glass fiber-reinforced composites. Biomaterials 23(10):2221–2229. https://doi.org/10.1016/s0142-9612(01)00355-610.1016/s0142-9612(01)00355-6 ↗
10. Miettinen VM, Narva KK, Vallittu PK (1999) Water sorption, solubility and effect of post-curing of glass fibre reinforced polymers. Biomaterials 20(13):1187–1194. https://doi.org/10.1016/s0142-9612(99)00003-410.1016/s0142-9612(99)00003-4 ↗
11. Arksornnukit M, Takahashi H, Nishiyama N (2004) Effects of silane coupling agent amount on mechanical properties and hydrolytic durability of composite resin after hot water storage. Dent Mater J 23(1):31–36. https://doi.org/10.4012/dmj.23.3110.4012/dmj.23.31 ↗
12. Matinlinna JP, Vallittu PK (2007) Bonding of resin composites to etchable ceramic surfaces - an insight review of the chemical aspects on surface conditioning. J Oral Rehabil 34(8):622–630. https://doi.org/10.1111/j.1365-2842.2005.01569.x10.1111/j.1365-2842.2005.01569.x ↗
13. Thomason JL (2019) Glass fibre sizing: A review. Compos Part A: Appl Sci Manuf 127:105619. https://doi.org/10.1016/j.compositesa.2019.10561910.1016/j.compositesa.2019.105619 ↗
14. Matinlinna JP, Özcan M, Lassila L, Kalk W, Vallittu P (2008) Effect of the cross-linking silane concentration in a novel silane system on bonding resin-composite cement. Acta Odontol Scand 66(4):250–255. https://doi.org/10.1080/0001635080224713110.1080/00016350802247131 ↗
15. Fuchigami K, Fujimura H, Teramae M, Nakatsuka T (2016) Precision synthesis of a long-chain silane coupling agent using micro flow reactors and its application in dentistry. J Encapsulation Adsorpt Sci 6(1):35–46. https://doi.org/10.4236/jeas.2016.6100410.4236/jeas.2016.61004 ↗
16. Maruo Y, Nishigawa G, Yoshihara K, Minagi S, Matsumoto T, Irie M (2017) Does 8-methacryloxyoctyl trimethoxy silane (8-MOTS) improve initial bond strength on lithium disilicate glass ceramic? Dent Mater 33(3):e95–e100. https://doi.org/10.1016/j.dental.2016.11.00410.1016/j.dental.2016.11.004 ↗
17. Yon MJY, Matinlinna JP, Tsoi JKH, Vallittu PK, Lassila LVJ (2023) Effect of long-chain silane on mechanical properties of experimental resin composites. Silicon. https://doi.org/10.1007/s12633-023-02462-y10.1007/s12633-023-02462-y ↗
18. Jin X, Tsoi JK, Matinlinna JP (2019) A novel silane system for amalgam repair with resin composite: an in vitro Study. Silicon 11(5):2321–2331. https://doi.org/10.1007/s12633-015-9292-910.1007/s12633-015-9292-9 ↗
19. Matinlinna JP, Lassila LV, Vallittu PK (2006) The effect of three silane coupling agents and their blends with a cross-linker silane on bonding a bis-GMA resin to silicatized titanium (a novel silane system). J Dent 34(10):740–746. https://doi.org/10.1016/j.jdent.2006.01.00810.1016/j.jdent.2006.01.008 ↗
20. Matinlinna JP, Özcan M, Lassila LV, Vallittu PK (2004) The effect of a 3-methacryloxypropyltrimethoxysilane and vinyltriisopropoxysilane blend and tris(3-trimethoxysilylpropyl)isocyanurate on the shear bond strength of composite resin to titanium metal. Dent Mater 20(9):804–813. https://doi.org/10.1016/j.dental.2003.10.00910.1016/j.dental.2003.10.009 ↗
21. Hon AK, Matinlinna JK, Shibata Y, Miyazaki T, Pow EHN (2019) Evaluation of five silane coupling agents on resin-titanium adhesion. Int J Adhes Adhes 90:132–137. https://doi.org/10.1016/j.ijadhadh.2019.02.00710.1016/j.ijadhadh.2019.02.007 ↗
22. Matinlinna JP, Lassila LV, Kangasniemi I, Vallittu PK (2005) Isocyanato- and methacryloxysilanes promote Bis-GMA adhesion to titanium. J Dent Res 84(4):360–364. https://doi.org/10.1177/15440591050840041310.1177/154405910508400413 ↗
23. Furtos G, Tomoaia-Cotisel M, Prejmerean C (2013) Resin composites reinforced by glass fibers with potential biomedical applications. Structure and mechanical properties. Part Sci Technol 31(4):332–339. https://doi.org/10.1080/02726351.2012.73645810.1080/02726351.2012.736458 ↗
24. Khan AS, Azam MT, Khan M, Mian SA, Ur Rehman I (2015) An update on glass fiber dental restorative composites: a systematic review. Mater Sci Eng C Mater Biol Appl 47:26–39. https://doi.org/10.1016/j.msec.2014.11.01510.1016/j.msec.2014.11.015 ↗
25. British Standards Institution, Precast concrete products — Specification of glassfibres for reinforcement of mortars and concretes. 2008. https://knowledge.bsigroup.com/products/precast-concrete-products-specification-of-glassfibres-for-reinforcement-of-mortars-and-concretes/standard. Accessed 18 Mar 2023
26. (2011) Owens corning composite solutions business composite solutions reinforcement guide. https://www.owenscorning.com/en-us/composites/documents. Accessed 18 Mar 2023
27. Relyon Plasma GmbH (2022) Effective plasma device for manual use. https://www.relyon-plasma.com/piezobrush-pz3/?lang=en. Accessed 18 Mar 2023
28. Cech V, Inagaki N, Vanek J, Prikryl R, Grycova A, Zemek J (2006) Plasma-polymerized versus polycondensed thin films of vinyltriethoxysilane. Thin Solid Films 502(1):181–187. https://doi.org/10.1016/j.tsf.2005.07.27110.1016/j.tsf.2005.07.271 ↗
29. Ito Y, Okawa T, Fujii T, Tanaka M (2016) Influence of plasma treatment on surface properties of zirconia. J Osaka Dent Univ 79–84. https://doi.org/10.18905/jodu.50.2_7910.18905/jodu.50.2_79 ↗
30. Ito Y, Okawa T, Fukumoto T, Tsurumi A, Tatsuta M, Fujii T, Tanaka J, Tanaka M (2016) Influence of atmospheric pressure low-temperature plasma treatment on the shear bond strength between zirconia and resin cement. J Prosthodont Res 60(4):289–293. https://doi.org/10.1016/j.jpor.2016.02.00110.1016/j.jpor.2016.02.001 ↗
31. Korzec D, Hoppenthaler F, Nettesheim S (2021) Piezoelectric direct discharge: Devices and applications. Plasma 4(1):1–4110.3390/plasma4010001 ↗
32. Kusano Y, Cederløf D, Fæster S (2020) Plasma surface modification of glass fibre sizing for manufacturing polymer composites. Key Eng Mater 843:159–164. https://doi.org/10.4028/www.scientific.net/KEM.843.15910.4028/www.scientific.net/KEM.843.159 ↗
33. Matinlinna JP, Lassila LV, Vallittu PK (2006) Evaluation of five dental silanes on bonding a luting cement onto silica-coated titanium. J Dent 34(9):721–726. https://doi.org/10.1016/j.jdent.2006.01.00510.1016/j.jdent.2006.01.005 ↗
34. Zhang M, Matinlinna JP (2011) The effect of resin matrix composition on mechanical properties of E-glass fiber-reinforced composite for dental use. J Adhes Sci Technol 25(19):2687–2701. https://doi.org/10.1163/016942411X55605110.1163/016942411X556051 ↗
35. Oja J, Lassila L, Vallittu PK, Garoushi S (2021) Effect of accelerated aging on some mechanical properties and wear of different commercial dental resin composites. Materials (Basel) 14(11). https://doi.org/10.3390/ma1411276910.3390/ma14112769 ↗
36. Matinlinna JP, Vallittu PK, Lassila LV (2011) Effects of different silane coupling agent monomers on flexural strength of an experimental filled resin composite. J Adhes Sci Technol 25:179–192. https://doi.org/10.1163/016942410X50330210.1163/016942410X503302 ↗
37. Lassila L, Säilynoja E, Vallittu P (2014) A composite material and its uses, EP Office (ed). Stick Tech Oy, Finland
38. Darvell BW (2006) A glossary of terms for dental materials science, 9th edn. BW Darvell, Hong Kong
39. Bouillaguet S, Schütt A, Alander P, Schwaller P, Buerki G, Michler J, Cattani-Lorente M, Vallittu PK, Krejci I (2006) Hydrothermal and mechanical stresses degrade fiber-matrix interfacial bond strength in dental fiber-reinforced composites. J Biomed Mater Res B Appl Biomater 76(1):98–105. https://doi.org/10.1002/jbm.b.3034910.1002/jbm.b.30349 ↗
40. Matinlinna JP, Lassila LV, Vallittu PK (2007) The effect of five silane coupling agents on the bond strength of a luting cement to a silica-coated titanium. Dent Mater 23(9):1173–1180. https://doi.org/10.1016/j.dental.2006.06.05210.1016/j.dental.2006.06.052 ↗
41. Kusano Y (2014) Atmospheric pressure plasma processing for polymer adhesion: A review. J Adhes 90(9):755–777. https://doi.org/10.1080/00218464.2013.80440710.1080/00218464.2013.804407 ↗
42. Relyon Plasma GmbH (2018) Plasma technology for surface cleaning. https://www.relyon-plasma.com/plasma-technology/surface-cleaning/?lang=en. Accessed 18 Mar 2023
43. Trofimov NN, Natrusov VI, Shatskaya EA, Smirnov YN, Bal’ MB, Kuznetsov AA, Gil’man AB, Drachev AI (2005) Effect of plasma treatment of glass fibre reinforcing materials on the strength and water resistance of glass fibre reinforced plastics based on them. Int Polym Sci Technol 32(12):55–61. https://doi.org/10.1177/0307174x050320121110.1177/0307174x0503201211 ↗
44. Matinlinna JP, Choi AH, Tsoi JK (2013) Bonding promotion of resin composite to silica-coated zirconia implant surface using a novel silane system. Clin Oral Implants Res 24(3):290–296. https://doi.org/10.1111/j.1600-0501.2012.02525.x10.1111/j.1600-0501.2012.02525.x ↗
45. Cheng HCK, Tsoi JKH, Zwahlen RA, Matinlinna JP (2014) Effects of silica-coating and a zirconate coupling agent on shear bond strength of flowable resin–zirconia bonding. Int J Adhes Adhes 50:11–16. https://doi.org/10.1016/j.ijadhadh.2013.12.02510.1016/j.ijadhadh.2013.12.025 ↗