High-cycle fatigue of 10M Ni–Mn–Ga magnetic shape memory alloy in reversed mechanical loading
Source abstract
Abstract
Application of Ni?Mn?Ga magnetic shape memory alloys in magnetic-field-induced actuation relies on their performance in long-term high-cycle fatigue. In this paper the performance and changes in the microstructure of a Ni?Mn?Ga 10M martensite single crystal material are reported in a long-term mechanically induced shape change cycling. The longest test was run for 2 ? 109 cycles at a frequency of 250?Hz and a strain amplitude of ? 1%. After the test a clear increase of the dynamic stiffness of the material was detected. Three specimens out of ten were cycled until fracture occurred and their fracture mechanism was studied. It was observed that the macroscopic crack growth took place roughly at a 45? angle with respect to the loading direction that was along the 100 crystallographic direction of the sample. The macroscopic fracture plane seemed to correspond roughly to the {111} crystal planes. On a microscopic scale the fracture propagated in a step-like manner at least partly along crystallographic planes. The steps at the fracture plane correspond to the {101} twin planes, with the height of steps along the 101 direction. The final fracture of the samples occurred in a brittle manner after the critical stress was exceeded.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Shape Memory Alloy Transformations · Titanium Alloys Microstructure and Properties · Microstructure and Mechanical Properties of Steels
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (21)
Show source-provided references
1. 10.1002/0471216275.esm07210.1002/0471216275.esm072 ↗
2. Söderberg O · Handbook of Magnetic Materials · 2006 · 16 · 1
3. Aaltio I · Smart Materials · 2009
4. Müllner P · Mater. Res. Soc. Symp. Proc. · 2004 · 785 · 415
5. 10.1140/epjst/e2008-00657-310.1140/epjst/e2008-00657-3 ↗
6. Tellinen J Suorsa I Jääskelainen A Aaltio I Ullakko K · Proc. ACTUATOR 2002 · 2002 · 566
7. 10.1117/12.59981410.1117/12.599814 ↗
8. 10.1016/j.scriptamat.2009.09.01210.1016/j.scriptamat.2009.09.012 ↗
9. Aaltio I Ge Y Liu X Söderberg O Tellinen J Sozinov A Hannula S-P · Int. Conf. on Martensitic Transformations · 2008
10. 10.1177/1045389X0606609410.1177/1045389X06066094 ↗
11. 10.1016/j.jmmm.2004.08.01110.1016/j.jmmm.2004.08.011 ↗
12. 10.1016/S1359-6462(03)00219-710.1016/S1359-6462(03)00219-7 ↗
13. Müllner P · Z. Metallkd. · 2006 · 97 · 20510.3139/146.101244 ↗
14. 10.1016/0079-6425(94)00007-710.1016/0079-6425(94)00007-7 ↗
15. Gottstein G · Physical Foundations of Materials Science · 2004 · 502
16. 10.1016/j.scriptamat.2008.07.03710.1016/j.scriptamat.2008.07.037 ↗
17. 10.4028/www.scientific.net/MSF.394-395.53710.4028/www.scientific.net/MSF.394-395.537 ↗
18. 10.1063/1.337360810.1063/1.3373608 ↗
19. Ullakko K Straka L Sozinov A Lanska N Soroka A Aaltio I Hannula S-P Kilpeläinen S Tuomisto F · ICFSMA’09: 2nd Int. Conf. on Ferromagnetic Shape Memory Alloys · 2009
20. 10.1063/1.162680010.1063/1.1626800 ↗
21. 10.1016/S1359-6462(03)00360-910.1016/S1359-6462(03)00360-9 ↗