journal article·2017-12

Evidence of an identical firing-activated carrier-induced defect in monocrystalline and multicrystalline silicon

Daniel Chen, Moonyong Kim, Bruno V. Stefani, Brett J. Hallam, Malcolm D. Abbott, Catherine E. Chan, Ran Chen, David N.R. Payne, Nitin Nampalli, Alison Ciesla, Tsun H. Fung, Kyung Kim, Stuart R. Wenham

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Silicon and Solar Cell Technologies · Thin-Film Transistor Technologies · Silicon Nanostructures and Photoluminescence

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (64)

Show source-provided references
1. J. Knobloch, S.W. Glunz, D. Biro, W. Warta, E. Schaffer, W. Wettling, Solar cells with efficiencies above 21% proccessed from Czochroalski grown silicon, in: Proceedings of the 25th IEEE Photovoltaic Specialists Conference Washington, DC IEEE, (1996) 405–408. http://dx.doi.org/10.1109/PVSC.1996.564029.10.1109/PVSC.1996.564029 ↗
2. K. Petter, K. Hubener, F. Kersten, M. Bartzsch, F. Fertig, B. Kloter, J. Muller, Dependence of LeTID on brick height for different wafer suppliers with several resistivities and dopants, in: Proceedings of the 9th Int. Work. Cryst. Silicon Sol. Cells, (2016).
3. K. Ramspeck, S. Zimmermann, H. Nagel, A. Metz, Y. Gassenbauer, B. Brikmann, A. Seidl, Light induced degradation of rear passivated mc-Si solar cells, in: Proceedings of the 27th European Photovoltaic Solar Energy Conference, (2012) 861–865. http://dx.doi.org/10.4229/27THEUPVSEC2012-2DO.3.4.
4. Engineering solutions and root-cause analysis for light-induced degradation in p-type multicrystalline silicon PERC modules10.1109/JPHOTOV.2016.2556981 ↗
5. Rapid stabilization of high-performance multicrystalline P-type silicon PERC cells10.1109/JPHOTOV.2016.2606704 ↗
6. Understanding the light-induced lifetime degradation and regeneration in multicrystalline silicon10.1016/j.egypro.2016.07.060 ↗
7. Lifetime spectroscopy investigation of light-induced degradation in p-type multicrystalline silicon PERC10.1109/JPHOTOV.2016.2606699 ↗
8. Evolution of LeTID defects in p-type multicrystalline silicon during degradation and regeneration
9. A. Zuschlag, D. Skorka, G. Hahn, Degradation and regeneration analysis in mc-Si, in: Proceedings of the Conf. Rec. IEEE Photovolt. Spec. Conf., (2016) 1051–1054. http://dx.doi.org/10.1109/PVSC.2016.7749772.10.1109/PVSC.2016.7749772 ↗
10. F. Kersten, P. Engelhart, H.C. Ploigt, A. Stekolnikov, T. Lindner, F. Stenzel, M. Bartzsch, A. Szpeth, K. Petter, J. Heitmann, J.W. Muller, A new mc-Si degradation effect called LeTID, in: Proceedings of the 2015 IEEE 42nd Photovoltaic Specialists Conference (PVSC 2015), (2015). http://dx.doi.org/10.1109/PVSC.2015.7355684.10.1109/PVSC.2015.7355684 ↗
11. Modulation of carrier-induced defect kinetics in multi-crystalline silicon PERC cells through dark annealing10.1002/solr.201600028 ↗
12. Acceleration and mitigation of carrier-induced degradation in p-type multi-crystalline silicon10.1002/pssr.201510437 ↗
13. Recombination activity of light-activated copper defects in p -type silicon studied by injection- and temperature-dependent lifetime spectroscopy10.1063/1.4963121 ↗
14. Impact of the firing temperature profile on light induced degradation of multicrystalline silicon
15. Lifetime degradation and regeneration in multicrystalline silicon under illumination at elevated temperature10.1063/1.4944839 ↗
16. Statistics of the recombination of holes and electrons10.1103/PhysRev.87.835 ↗
17. multicrystalline silicon for solar cells recombination parameters of lifetime-limiting carrier-induced defects in multicrystalline silicon for solar cells
18. Rapid passivation of carrier-induced defects in p-type multi-crystalline silicon10.1016/j.solmat.2016.05.022 ↗
19. Intra-grain versus grain boundary degradation due to illumination and annealing behavior of multi-crystalline solar cells10.1016/j.solmat.2016.05.061 ↗
20. Temperature and light induced changes in bulk and passivation quality of boron-doped float-zone silicon coated with SiNx:H
21. F. Fertig, R. Lantzsch, A. Mohr, M. Schaper, M. Bartzsch, D. Wissen, F. Kersten, A. Mette, S. Peters, A. Eidner, J. Cieslak, K. Duncker, M. Junghänel, E. Jarzembowski, M. Kauert, D. Meißner, B. Reiche, S. Geißler, S. Hörnlein, C. Klenke, L. Niebergall, A. Schönmann, A. Weihrauch, F. Stenzel, A. Hofmann, T. Rudolph, A. Schwabedissen, M. Gundermann, M. Fischer, J.W. Müller, D.J.W. Jeong, Mass production of p-type Cz silicon solar cells approaching average stable conversion efficiencies of 22%, in: Proceedings of the 7th International Conference Silicon Photovoltaics, SiliconPV, ScienceDirect, 2017 (in press).10.1016/j.egypro.2017.09.308 ↗
22. N. Nampalli, H. Li, M. Kim, B. Stefani, S. Wenham, B. Hallam, M.D. Abbott, Multiple pathways for permanent deactivation of boron-oxygen defects in p-type silicon, in: Proceedings of the 7th International Conference Cryst. Silicon Photovoltaics, 2017 (in press).10.1016/j.solmat.2017.06.041 ↗
23. Light-induced activation and deactivation of bulk defects in boron-doped float-zone silicon10.1063/1.4983024 ↗
24. Z. Hameiri, N. Borojevic, L. Mai, N. Nandakumar, K. Kim, S. Winderbaum, Should the Refractive Index at 633nm be used to Characterize Silicon Nitride Films?, (2016) 2900–2904.10.1109/PVSC.2016.7750187 ↗
25. Low-absorbing and thermally stable industrial silicon nitride films with very low surface recombination10.1109/JPHOTOV.2017.2706424 ↗
26. Generalized analysis of quasi-steady-state and quasi-transient measurements of carrier lifetimes in semiconductors generalized analysis of quasi-steady-state and quasi-transient measurements of carrier lifetimes in semiconductors10.1063/1.371633 ↗
27. Improved parameterization of Auger recombination in silicon10.1016/j.egypro.2012.07.034 ↗
28. Degradation of carrier lifetime in Cz silicon solar cells10.1016/S0927-0248(00)00098-2 ↗
29. Statistical analysis of recombination properties of the boron-oxygen defect in p-type Czochralski silicon10.1007/s11708-016-0442-6 ↗
30. Electronically activated boron-oxygen-related recombination centers in crystalline silicon10.1063/1.2140584 ↗
31. Generation and annihilation of boron? Oxygen-related recombination centers in compensated p- and n-type silicon10.1063/1.3511741 ↗
32. Grown-in defects limiting the bulk lifetime of p -type float-zone silicon wafers10.1063/1.4907804 ↗
33. D. Macdonald, A. Cuevas, The trade-off between phosphorus gettering and thermal degradation in multicrystalline silicon, in: Proceedings of the 16th European Photovoltaic Solar Energy Conference, (2000) 1707–1710.
34. Dissolution and gettering of iron during contact co-firing10.1016/j.egypro.2011.06.133 ↗
35. Impact of thermal processes on multi-crystalline silicon10.1007/s11708-016-0427-5 ↗
36. D. Macdonald, A. Cheung, A. Cuevas, Gettering and poisoning of silicon wafers by phosphorus diffused layers, in: Proceedings of the 3rd World Conference on Photovoltaic Energy Conversion, 2 (2003) 11–14.
37. The impact of different diffusion temperature profiles on iron concentrations and carrier lifetimes in multicrystalline silicon wafers10.1109/JPHOTOV.2012.2231726 ↗
38. Degradation of multicrystalline silicon solar cells and modules after illumination at elevated temperature10.1016/j.solmat.2015.06.015 ↗
39. T.H. Fung, C.E. Chan, B.J. Hallam, D.N.R. Payne, M.D. Abbott, S.R. Wenham, Impact of annealing on the formation and mitigation of carrier-induced defects in multi-crystalline silicon, in: Proceedings of the 7th International Conference Silicon Photovoltaics, SiliconPV, 2017 (in press).10.1016/j.egypro.2017.09.087 ↗
40. Manipulation of hydrogen charge states for passivation of P-type wafers in photovoltaics10.1109/JPHOTOV.2014.2339494 ↗
41. Hydrogen passivation of defects in multicrystalline silicon solar cells10.1016/j.solmat.2003.08.015 ↗
42. Influence of Al2O3 and SiNx Passivation Layers on LeTID10.1016/j.egypro.2016.07.079 ↗
43. M. Sheoran, D.S. Kim, A. Rohatgi, H.F.W. Dekkers, G. Beaucarne, M. Young, S. Asher, Hydrogen diffusion in silicon from PECVD silicon nitride, in: Proceedings of the 2008 33rd IEEE Photovoltaic Specialists Conference, IEEE, (2008) 1–4. http://dx.doi.org/10.1109/PVSC.2008.4922638.10.1109/PVSC.2008.4922638 ↗
44. Study of the composition of hydrogenated silicon nitride SiNx:H for efficient surface and bulk passivation of silicon10.1016/j.solmat.2009.01.023 ↗
45. Influence of the high-temperature ?Firing? Step on high-rate plasma deposited silicon nitride films used as bulk passivating antireflection coatings on silicon solar cells10.1116/1.1609481 ↗
46. Hydrogen induced passivation of Si interfaces by Al2O3 films and SiO2/Al2O3 stacks10.1063/1.3497014 ↗
47. Influence of hydrogen effusion from hydrogenated silicon nitride layers on the regeneration of boron-oxygen related defects in crystalline silicon10.1063/1.4833243 ↗
48. Light-induced degradation of silicon solar cells with aluminiumoxide passivated rear side10.1016/j.egypro.2015.07.086 ↗
49. Multicrystalline PERC solar cells: is light-induced degradation challenging the efficiency gain of rear passivation?
50. T. Luka, S. Eiternick, S. Frigge, C. Hagendorf, H. Mehlich, M. Turek, Investigation of light induced degradation of multi-crystalline PERC cells, in: Proceedings of the 31st European Photovoltaic Solar Energy Conference and Exhibition, (2015) 826–828.
51. Light-induced degradation of PECVD aluminium oxide passivated silicon solar cells10.1002/pssr.201409424 ↗
52. The role of hydrogenation and gettering in enhancing the efficiency of next-generation Si solar cells: an industrial perspective
53. A. Cuevas, D. Macdonald, M. Kerr, C. Samundsett, A. Sloan, S. Shea, A. Leo, M. Mrcarica, S. Winderbaum, Evidence of impurity gettering by industrial phosphorus diffusion, in: Proceedings of the Conference Rec. Twenty-Eighth IEEE Photovolt. Spec. Conference – 2000 (Cat. No.00CH37036), IEEE, (2000) 244–247. http://dx.doi.org/10.1109/PVSC.2000.915803.10.1109/PVSC.2000.915803 ↗
54. Impact of phosphorus gettering parameters and initial iron level on silicon solar cell properties10.1002/pip.2215 ↗
55. Building intuition of iron evolution during solar cell processing through analysis of different process models10.1007/s00339-015-9317-7 ↗
56. Accelerated formation of the boron-oxygen complex in p-type Czochralski silicon10.1002/pssr.201510064 ↗
57. Fast and slow lifetime degradation in boron-doped Czochralski silicon described by a single defect10.1002/pssr.201600096 ↗
58. Modulating the extent of fast and slow boron-oxygen related degradation in Czochralski silicon by thermal annealing: evidence of a single defect10.1063/1.4975685 ↗
59. Light-induced degradation in multicrystalline silicon: the role of copper10.1016/j.egypro.2016.07.073 ↗
60. Dynamics of light-induced FeB pair dissociation in crystalline silicon10.1063/1.1823587 ↗
61. Electronic properties of iron-boron pairs in crystalline silicon by temperature- and injection-level-dependent lifetime measurements10.1063/1.1897489 ↗
62. Quantification of characteristic parameters for the dissociation kinetics of iron-boron pairs in Czochralski silicon10.1016/j.scriptamat.2010.10.021 ↗
63. A. Herguth, G. Hahn, Boron-Oxygen Related Defects in Cz-Silicon Solar Cells Degradation, Regeneration and Beyond, 2 (2009) 974–976. http://dx.doi.org/10.4229/24thEUPVSEC2009-2AO.3.4.
64. Investigations on the long time behavior of the metastable boron–oxygen complex in crystalline silicon10.1002/pip.779 ↗