Molten salt corrosion mechanisms of nitrate based thermal energy storage materials for concentrated solar power plants: A review
Source abstract
Abstract
Corrosion mechanisms for current heat transfer fluid and storage media used in CSP plants working at temperatures from 300°C to 600°C are reviewed in this paper. The studies found in the literature show that these mechanisms are influenced by the impurities present in the salt and the relation between Mg(NO3)2, moisture, CO2, perchlorates, and sulphates with the corrosion process. Corrosion mechanisms were identified along with a discussion of the corrosion products and their influence on the corrosion layers formed.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Phase Change Materials Research · Adsorption and Cooling Systems · Solar Thermal and Photovoltaic Systems
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (58)
Show source-provided references
1. Concentrating solar power Gen3 demonstration roadmap
2. High-temperature phase change materials for thermal energy storage10.1016/j.rser.2009.11.011 ↗
3. Bradford · 1987
4. Corrosion in molten nitrate-nitrite salts
5. Hot corrosion of materials: a fluxing mechanism?10.1016/S0010-938X(01)00057-9 ↗
6. P.F. Tortorelli, J.R. Distefano, Selection of corrosion-resistant materials for use in molten nitrate salts. Oak Ridge National Laboratory Report, 1989.10.2172/5236321 ↗
7. Heat transfer fluids for concentrating solar power systems: a review10.1016/j.apenergy.2015.01.125 ↗
8. High-temperature and corrosion behavior of nitrate nitrite molten salt mixtures regarding their application in concentrating solar power plants10.1016/j.egypro.2015.03.071 ↗
9. Multicomponent molten salt mixtures based on nitrate/nitrite anions10.1115/1.4003418 ↗
10. The thermal stability of molten nitrite/nitrates salt for solar thermal energy storage in different atmospheres10.1016/j.solener.2012.05.025 ↗
11. Thermal analysis of molten ternary lithium-sodium-potassium nitrates10.1016/j.renene.2016.12.015 ↗
12. Screening tests of sodium nitrate and potassium nitrate decomposition10.1016/0038-092X(82)90082-2 ↗
13. The thermal stability of binary alkali metal nitrates10.1016/0040-6031(84)87150-6 ↗
14. High-temperature stability of ternary nitrate molten salts for solar thermal energy systems10.1016/0165-1633(90)90042-Y ↗
15. The thermal stability of molten lithium–sodium–potassium carbonate and the influence of additives on the melting point10.1115/1.4006895 ↗
16. Roles of double salt formation and NaNO3 in Na2CO3 promoted MgO absorbent for intermediate temperature CO2 removal10.1016/j.ijggc.2012.11.013 ↗
17. Effect of the impurity magnesium nitrate in the thermal decomposition of the solar salt
18. Solubility and detection (down to 30 p.p.b.) of oxygen in molten alkali nitrates10.1016/S0022-0728(72)80347-4 ↗
19. Solubility and detection of water in the (Na,K)NO3 eutectic melt10.1016/S0022-0728(70)80118-8 ↗
20. Oxides/oxygen systems in molten alkali nitrates: remarks and hypotheses concerning recent literature findings10.1016/S0022-0728(73)80055-5 ↗
21. Catalytic currents in fused salts: discharge mechanism of nitrite in molten alkali nitrates10.1016/S0022-0728(77)80381-1 ↗
22. Oxygen electrodes in fused salts: investigation and mechanistic remarks on the system (Ni)O2, H2O/OH in the (Na, K) NO3 eutectic melt10.1016/S0022-0728(79)80298-3 ↗
23. On the presence of NO2+ in molten nitrates10.1016/S0022-0728(71)80245-0 ↗
24. Catalytic currents in fused salts: discharge mechanism of nitrite in molten alkali nitrates(II)10.1016/S0022-0728(78)80193-4 ↗
25. Peleg · J. Phys. Chem. · 1967 · 71 · 86810.1021/j100872a066 ↗
26. Thermal influence in corrosion properties of Chilean solar nitrates10.1016/j.solener.2014.07.027 ↗
27. Corrosion on mild steel in molten sodium nitrate-potassium nitrate eutectic10.1179/bcj.1976.11.1.44 ↗
28. A reversible oxygen electrode in an equimolar KNO3 NaNO3 melt saturated with sodium peroxide II. A voltammetric study10.1016/0013-4686(76)85062-1 ↗
29. Thermochemistry of anion mixtures in simple fused salt systems. II Solutions of some salts of MO4- and MO42- anions in the corresponding alkali nitrates10.1021/j100806a057 ↗
30. Corrosion of alloys and metals by molten nitrates
31. Corrosion of stainless steels and carbon steel by molten mixtures of commercial nitrate salts10.1361/10599490417542 ↗
32. Effect of chloride content of molten nitrate salt on corrosion of A516 carbon steel
33. Corrosion behavior of stainless and low-chromium steels and IN625 in molten nitrate salts at 600 °C10.1016/j.solmat.2015.08.011 ↗
34. A.M. Kruizenga, D.D. Gill, M. Laford, G. McConohy, Corrosion of high temperature alloys in solar salt at 400, 500 and 680 C. SANDIA National Laboratories Report. 2013, Sand 2013-8256, 2013.10.2172/1104752 ↗
35. Molten nitrate salts at 600 and 680 °C: thermophysical property changes and corrosion of high-temperature nickel alloys10.1016/j.solener.2014.01.028 ↗
36. Corrosion of iron stainless steels in molten nitrate salt10.1016/j.egypro.2014.03.095 ↗
37. Constant extension rate testing of IN625LCF in molten nitrate salt10.1016/S0010-938X(98)00175-9 ↗
38. Two-tank molten salts thermal energy storage system for solar power plants at pilot plant scale: lessons learnt and recommendations for its design, start-up and operation10.1016/j.renene.2018.01.026 ↗
39. High temperature corrosion behavior on molten nitrate salt-based nanofluids for CSP plants10.1016/j.renene.2018.07.018 ↗
40. Unexpected effect of nanoparticles doping on the corrosivity of molten nitrate salt for thermal energy storage10.1016/j.solmat.2018.01.002 ↗
41. Investigation of the corrosion behavior of NiVAl multilayer coatings in hot salt melts10.1016/j.surfcoat.2015.07.045 ↗
42. Slurry aluminizing: a solution for molten nitrate salt corrosion in concentrated solar power plants10.1016/j.solmat.2015.11.024 ↗
43. Corrosion testing of diffusion-coated steel in molten salt for concentrated solar power tower systems10.1016/j.surfcoat.2018.08.097 ↗
44. Materials selection for thermal energy storage systems in parabolic trough collector solar facilities using high chloride content nitrate salts10.1016/j.solmat.2017.01.028 ↗
45. Corrosion properties of a ternary nitrate/nitrite molten salt in concentrated solar technology10.1016/j.renene.2015.01.072 ↗
46. Corrosion ability of a novel heat transfer fluid for energy storage in CSP plants10.1007/s11085-014-9494-3 ↗
47. Corrosion of stainless steels and low-Cr steel in molten Ca(NO3)2 NaNO3 KNO3 eutectic salt for direct energy storage in CSP plants10.1016/j.solmat.2015.05.004 ↗
48. A simple method for the inhibition of the corrosion of carbon steel by molten nitrate salt for thermal storage in concentrating solar power applications
49. High-temperature corrosion of CrMo steel in molten LiNO3 NaNO3 KNO3 eutectic salt for thermal energy storage10.1016/j.solmat.2014.10.007 ↗
50. Molten salt corrosion of stainless steels and low-Cr steel in CSP plants10.1007/s11085-012-9310-x ↗
51. Saad · 2013
52. Improvement of the corrosion properties in ternary molten nitrate salts for direct energy storage in CSP plants10.1016/j.solener.2016.05.030 ↗
53. A. Bonk, M. Braun, A. Hanke, J. Forstner, D. Rückle, S. Kaesche, V.A. Sötz, T. Bauer, Influence of different atmospheres on molten salt chemistry and its effect on steel corrosion. In: AIP Conference Proceedings, 2033, 2018, pp. 0900031–0900039.10.1063/1.5067097 ↗
54. Evaluation of corrosion resistance of A516 Steel in a molten nitrate salt mixture using a pilot plant facility for application in CSP plants10.1016/j.solmat.2016.12.002 ↗
55. A.G. Fernández, M. Henriquez, A. Mallco, B. Muñoz-Sánchez, J. Nieto-Maestre. Dynamic corrosion tests comparison: dynamic reactor vs high temperature pilot plant scale setup for Chilean LiNO3 containing molten salt. In: AIP Conference Proceedings, 2033, 2018, pp. 0900091–0900096.10.1063/1.5067103 ↗
56. Study of corrosion by dynamic gravimetric analysis (DGA) methodology. Influence of chloride content in solar salt10.1016/j.solmat.2016.07.027 ↗
57. International ASTM G1-03, Standard practice for preparing, cleaning, and evaluating corrosion test specimens, 2003.
58. The effect of humidity, impurities and initial state on the corrosion of carbon and stainless steels in molten HitecXL salt for CSP application10.1016/j.solmat.2017.08.026 ↗