New generation concentrated solar power (CSP) plants require new solar receiver materials with selective optical properties and excellent corrosion resistance against molten salts. MAX phases are promising materials for CSP applications due to their optical properties and resistance to thermal shocks. Herein, we report a solar absorptance >/= 0.5 and a thermal emittance of 0.17-0.31 between 600 and 1500 K for Cr2AlC, Ti2AlC, and Ti3AlC2. These compositions were also exposed to solar salt corrosion at 600°C for up to 4 weeks. Cr2AlC exhibited superior corrosion resistance due to the formation of a protective nanometric layer.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: MXene and MAX Phase Materials · 2D Materials and Applications · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (39)

Show source-provided references
1. Tantalum diboride-based ceramics for bulk solar absorbers10.1016/j.solmat.2014.07.012 ↗
2. An overview of ultra-refractory ceramics for thermodynamic solar energy generation at high temperature10.1016/j.renene.2018.08.036 ↗
3. Porous and dense hafnium and zirconium ultra-high temperature ceramics for solar receivers10.1016/j.optmat.2013.08.020 ↗
4. Process and composition dependence of optical properties of zirconium, hafnium and tantalum borides for solar receiver applications10.1016/j.solmat.2016.06.028 ↗
5. Femtosecond laser treatments to tailor the optical properties of hafnium carbide for solar applications10.1016/j.solmat.2014.09.037 ↗
6. From colloidal precursors to metal carbides nanocomposites MC (M=Ti, Zr, Hf and Si): synthesis, characterization and optical spectral selectivity studies10.1016/j.solmat.2015.07.039 ↗
7. Effect of TiC incorporation on the optical properties and oxidation resistance of SiC ceramics10.1016/j.solmat.2020.110536 ↗
8. Evaluation of porous silicon carbide monolithic honeycombs as volumetric receivers/collectors of concentrated solar radiation10.1016/j.solmat.2006.10.021 ↗
9. Processing of MAX phases: from synthesis to applications10.1111/jace.17544 ↗
10. The Mn + 1AXn phases: materials science and thin-film processing10.1016/j.tsf.2009.07.184 ↗
11. The MAX phases: unique new carbide and nitride materials10.1511/2001.28.334 ↗
12. MAX phases: bridging the gap between metals and ceramics
13. Yttrium incorporation in Cr2AlC: on the metastable phase formation and decomposition of (Cr,Y)2AlC MAX phase thin films
14. Deposition of MAX phase-containing thin films from a (Ti,Zr)2AlC compound target10.1016/j.apsusc.2021.149370 ↗
15. Tunca · Chemically complex double solid solution MAX phase-based ceramics in the (Ti,Zr,Hf,V,Nb)-(Al,Sn)-C system · 2022 · 10 · 52
16. Corrosion behavior of Al-containing MAX-phase coatings exposed to oxygen containing molten Pb at 600 °C10.1016/j.corsci.2022.110275 ↗
17. High-temperature oxidation and hot corrosion of Cr2AlC10.1016/j.actamat.2007.07.024 ↗
18. Ti 2 AlC MAX phase for resistance against CMAS attack to thermal barrier coatings10.1016/j.ceramint.2019.01.059 ↗
19. Early stages of dissolution corrosion in 316 L and DIN 1.4970 austenitic stainless steels with and without anticorrosion coatings in static liquid lead-bismuth eutectic (LBE) at 500 °C10.1016/j.matchar.2021.111234 ↗
20. Tribological and mechanical properties of Ti2AlC coating at room temperature and 800 °C10.1016/j.ceramint.2017.10.045 ↗
21. Oxidation of Cr2AlC coatings in the temperature range of 1230 to 1410°C10.1016/j.surfcoat.2011.03.086 ↗
22. Environmental resistance of Cr2AlC MAX phase under thermal gradient loading using a burner rig10.1111/jace.15425 ↗
23. Assessment of Ti3SiC2 MAX phase as a structural material for high temperature receivers
24. Characterization of thermal performance, flux transmission performance and optical properties of MAX phase materials under concentrated solar irradiation10.1016/j.solmat.2018.03.018 ↗
25. Suitability of layered Ti3SiC2 and Zr3[Al(Si)]4C6 ceramics as high temperature solar absorbers for solar energy applications10.1016/j.solmat.2014.12.008 ↗
26. Compatibility of SiC–and MAX phase-based ceramics with a KNO3 -NaNO3 molten solar salt10.1016/j.solmat.2019.03.007 ↗
27. Synthesis, sintering, and effect of surface roughness on oxidation of submicron Ti2AlC ceramics10.1111/jace.17582 ↗
28. High-temperature oxidation and compressive strength of Cr2AlC MAX phase foams with controlled porosity10.1111/jace.15224 ↗
29. A new approach to low-cost, solar salt-resistant structural materials for concentrating solar power (CSP) and thermal energy storage (TES)10.3390/met11121970 ↗
30. Effects of pellet surface roughness and pre-oxidation temperature on CMAS corrosion behavior of Ti2AlC10.1007/s40145-022-0588-0 ↗
31. Improving the Na2SO4-induced corrosion resistance of Ti3AlC2 by pre-oxidation in air10.1016/j.corsci.2005.11.005 ↗
32. Hot corrosion and protection of Ti2AlC against Na2SO4 salt in air10.1016/j.jeurceramsoc.2005.12.004 ↗
33. Suitability of ultra-refractory diboride ceramics as absorbers for solar energy applications10.1016/j.solmat.2012.10.004 ↗
34. Spectral emittance of ceramics for high temperature solar receivers10.1016/j.solener.2021.05.019 ↗
35. Tailoring optical properties of surfaces in wide spectral ranges by multi-scale femtosecond-laser texturing: a case-study for TaB2 ceramics10.1016/j.optmat.2020.110347 ↗
36. Multi-scale femtosecond-laser texturing for photothermal efficiency enhancement on solar absorbers based on TaB2 ceramics10.3390/nano13101692 ↗
37. Tailoring optical properties of surfaces in wide spectral ranges by multi-scale femtosecond-laser texturing: a case-study for TaB2 ceramics10.1016/j.optmat.2020.110347 ↗
38. Mechanism for breakaway oxidation of the Ti2AlC MAX phase10.1016/j.actamat.2021.117025 ↗
39. Evolution of corrosion products on ASTM A36 and AISI 304L steels formed in exposure to molten NaNO3–KNO3 eutectic salt: Electrochemical study10.1016/j.corsci.2021.110047 ↗