journal article·2026-01Open access

UV-induced degradation in TOPCon solar cells: Hydrogen dynamics and impact of UV wavelength

Muhammad Umair Khan, Chandany Sen, Michael Pollard, Ting Huang, Munan Gao, Ruirui Lv, Yuanjie Yu, Xinyuan Wu, Haoran Wang, Xutao Wang, Bram Hoex

Abstract

Tunnel oxide passivated contact (TOPCon) solar cells dominate the worldwide photovoltaic market due to their high efficiency and low manufacturing costs. However, recent reliability studies have shown that TOPCon solar cells and modules can degrade significantly under ultraviolet (UV) radiation, known as UV-induced degradation (UVID). The effect of UV radiation on TOPCon solar cells, particularly concerning the role of hydrogen and wavelength dependence in the UV range, remains ambiguous, highlighting the need for further investigation. This study uses UV-A and UV-B exposure to understand the impact of UV on TOPCon precursors and lifetime structures. We demonstrate that UV-B and UV-A exposures lead to the same extent of degradation, although the process occurs significantly faster under UV-B, indicating that UV-B can be used for accelerated UV degradation testing. Notably, no Light- and elevated Temperature-Induced Degradation (LeTID) was observed when samples were exposed to UV radiation; in contrast, LeTID was observed when samples were exposed to the same temperatures without UV radiation. This suggests that UV radiation not only alters the surface but also influences hydrogen dynamics within the bulk, consistent with LeTID being a hydrogen-related bulk defect. Time of flights secondary ion mass spectrometry analysis further supports these findings by revealing an increased hydrogen concentration at the AlO x /(p + )Si interface after UV exposure. This can be attributed to the fact that UV radiation is able to break Si-H bonds, where the free hydrogen can redistribute into a bonded or unbonded state in the sample. In addition, the breaking of Si-H bonds at the silicon interface increases the interface defect density and, thus, surface recombination. The rear side of the TOPCon precursor exhibited no significant degradation, as the poly-Si layer effectively absorbs UV radiation below 370 nm, shielding the tunnel oxide layer and rendering the rear side relatively resistant to UVID. This work contributes to the understanding of UVID mechanisms in TOPCon solar cells and provides insights for developing effective mitigation strategies. • UV-B radiation is shown to accelerate degradation in TOPCon cells compared to UV-A, enabling rapid reliability testing. • The TOPCon rear side exhibits high resistance to UVID, because of the UV-shielding effect of the thick polysilicon layer. • UV exposure is found to suppress the formation of the bulk degradation mechanism known as LeTID. • UVID is linked to a redistribution of hydrogen towards the AlO x /(p + )Si interface, as confirmed by ToF-SIMS analysis.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Silicon and Solar Cell Technologies · Photovoltaic System Optimization Techniques · solar cell performance optimization

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (33)

Show source-provided references
1. A review on p-Type tunnel oxide passivated contact (TOPCon) solar cell10.1007/s42341-023-00433-z ↗
2. Fischer · 2024
3. Photovoltaic failure and degradation modes10.1002/pip.2866 ↗
4. magazine · 2023
5. Review of Degradation and Failure Phenomena in Photovoltaic Modules, (n.d.).
6. 2024
7. UV-Induced degradation of industrial PERC, TOPCon, and HJT solar cells: the next big reliability challenge?10.1002/solr.202400628 ↗
8. A comprehensive review and outlook of bifacial photovoltaic (bPV) technology10.1016/j.enconman.2020.113283 ↗
9. P. Gebhardt, U. Kräling, E. Fokuhl, I. Haedrich, D. Philipp, Reliability of Commercial Topcon PV Modules-An Extensive Comparative Study, n.d.
10. Categorization of weathering stresses for photovoltaic modules10.1002/ese3.189 ↗
11. Kiwa PVEL, https://scorecard.pvel.com/uvid/, (n.d.).
12. UV radiation hardness of photovoltaic modules featuring crystalline Si solar cells with AlOx/p ‐type Si and SiNy/n+‐type Si interfaces10.1002/pssr.201700178 ↗
13. UV-induced degradation of high-efficiency silicon PV modules with different cell architectures10.1002/pip.3606 ↗
14. Negative charge and charging dynamics in Al2O3 films on Si characterized by second-harmonic generation10.1063/1.2985906 ↗
15. Short wavelength photons destroying Si–H bonds and its influence on high-efficiency silicon solar cells and modules10.1002/solr.202370153 ↗
16. Short wavelength photons destroying Si–H bonds and its influence on high-efficiency silicon solar cells and modules10.1002/solr.202370153 ↗
17. Plasma damage effect on ultraviolet-induced degradation of PECVD sinx:h passivation
18. UV-induced degradation of high-efficiency silicon PV modules with different cell architectures10.1002/pip.3606 ↗
19. Bifacial solar photovoltaics - a technology review10.1016/j.rser.2016.03.041 ↗
20. A critical review of the environmental performance of bifacial photovoltaic panels
21. Dielectric surface passivation for silicon solar cells: a review
22. Terrestrial photovoltaic (PV) modules - design qualification and type approval
23. Generalized analysis of quasi-steady-state and quasi-transient measurements of carrier lifetimes in semiconductors generalized analysis of quasi-steady-state and quasi-transient measurements of carrier lifetimes in semiconductors10.1063/1.371633 ↗
24. Improved parameterization of auger recombination in silicon10.1016/j.egypro.2012.07.034 ↗
25. Studying light-induced degradation by lifetime decay analysis: excellent fit to solution of simple second-order rate equation10.1109/JPHOTOV.2013.2278663 ↗
26. Measurement of the emitter saturation current by a contactless photoconductivity decay method
27. Degradation of carrier lifetime in Cz silicon solar cells10.1016/S0927-0248(00)00098-2 ↗
28. Khan · 2021
29. PV lighthouse, SunSolve, (n.d.). https://www.pvlighthouse.com.au/sunsolve.
30. Evidence of an identical firing-activated carrier-induced defect in monocrystalline and multicrystalline silicon10.1016/j.solmat.2017.08.003 ↗
31. Degradation and recovery of n-Type multi-crystalline silicon under illuminated and dark annealing conditions at moderate temperatures10.1109/JPHOTOV.2018.2885711 ↗
32. Influence of hydrogen on the mechanism of permanent passivation of boron-oxygen defects in p-Type czochralski silicon10.1109/JPHOTOV.2015.2466457 ↗
33. UV-stable surface passivation for crystalline silicon cells in solar modules with UV light transmitting encapsulation materials