journal article·2025-09

Spatially resolved modulus measurements of photovoltaic encapsulation materials using cross-sectional nano-indentation

Stefan Mitterhofer, Soshana Smith, Ashlee Aiello, Karissa Jensen, Stephanie Moffitt, Xiaohong Gu

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Force Microscopy Techniques and Applications · Advanced Surface Polishing Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (57)

Show source-provided references
1. 2024
2. DuPont global PV reliability - 2020 Field analysis
3. Encapsulation of PV modules using ethylene vinyl acetate copolymer as a pottant: a critical review10.1016/0927-0248(95)00150-6 ↗
4. Long-term durability of transparent backsheets for bifacial photovoltaics: an in-depth degradation analysis10.1016/j.solmat.2023.112309 ↗
5. Transparent backsheets for bifacial photovoltaic (PV) modules: material characterization and accelerated laboratory testing10.1002/pip.3494 ↗
6. Drivers for the cracking of multilayer polyamide‐based backsheets in field photovoltaic modules: in‐depth degradation mapping analysis10.1002/pip.3260 ↗
7. Investigation of the crack propensity of co-extruded polypropylene backsheet films for photovoltaic modules10.1016/j.solmat.2023.112438 ↗
8. Modeling outdoor service lifetime prediction of PV modules: effects of combined climatic stressors on PV module power degradation10.1109/JPHOTOV.2019.2916197 ↗
9. Novel EPE co-extruded encapsulating films with UV down-conversion power gain effect for highly efficient solar cells10.1016/j.solmat.2023.112373 ↗
10. Habersberger · 2023
11. Liu · 2024
12. Diffusion of UV additives in ethylene-vinyl acetate copolymer encapsulants and the impact on polymer reliability10.1109/JPHOTOV.2023.3333198 ↗
13. Depth profiling of degradation of multilayer photovoltaic backsheets after accelerated laboratory weathering: cross-sectional Raman imaging10.1016/j.solmat.2015.09.021 ↗
14. A spatially resolved evaluation of accelerated environmental aging on emerging polypropylene-based photovoltaic backsheets using raman spectroscopy10.1002/pip.3904 ↗
15. Fluorescence imaging analysis of depth‐dependent degradation in photovoltaic laminates: insights to the failure10.1002/pip.3212 ↗
16. Nanoindentation of polymers: an overview10.1002/1521-3900(200103)167:1<15::AID-MASY15>3.0.CO;2-T ↗
17. A review of recent research on nanoindentation of polymer composites and their constituents10.1016/j.compscitech.2014.09.016 ↗
18. Nanoindentation in polymer nanocomposites10.1016/j.pmatsci.2014.06.002 ↗
19. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
20. Measurement of hardness and elastic modulus by instrumented indentation: advances in understanding and refinements to methodology10.1557/jmr.2004.19.1.3 ↗
21. E28 Committee, Practice for Instrumented Indentation Testing, (n.d.). https://doi.org/10.1520/E2546-15.10.1520/E2546-15 ↗
22. Review of nanoindentation size effect: experiments and atomistic simulation10.3390/cryst7100321 ↗
23. Christöfl · 2024
24. Error estimation of nanoindentation mechanical properties near a dissimilar interface via finite element analysis and analytical solution methods10.1557/jmr.2010.0295 ↗
25. Experimental method to account for structural compliance in nanoindentation measurements10.1557/jmr.2008.0131 ↗
26. Nanoindentation near the edge10.1557/jmr.2009.0076 ↗
27. Cross-sectional nanoindentation: a new technique for thin film interfacial adhesion characterization10.1016/S1359-6454(99)00254-2 ↗
28. A review of nanoindentation continuous stiffness measurement technique and its applications10.1016/S1044-5803(02)00192-4 ↗
29. Evaluation of surface crack formation in photovoltaic backsheets using fragmentation and finite element simulations10.1109/JPHOTOV.2024.3356119 ↗
30. Palmiotti · 2024
31. Improved nanoindentation methods for polymer based multilayer film cross-sections
32. Use of indentation to study the degradation of photovoltaic backsheets10.1016/j.solmat.2019.110082 ↗
33. Nanomechanical and fluorescence characterizations of weathered PV module encapsulation10.1109/JPHOTOV.2021.3053657 ↗
34. Nanoindentation reveals crosslinking behavior of solar encapsulants—the methodological advantages over bulk methods10.3390/polym13193328 ↗
35. Accelerated UV weathering device based on integrating sphere technology10.1063/1.1808916 ↗
36. Indenter geometry effects on the measurement of mechanical properties by nanoindentation with sharp indenters10.1557/PROC-436-147 ↗
37. Tearing and reliability of photovoltaic module backsheets10.1002/pip.3144 ↗
38. The role of crystalline, mobile amorphous and rigid amorphous fractions in the performance of recycled poly (ethylene terephthalate) (PET)10.1016/j.polymdegradstab.2011.10.008 ↗
39. Degradation of photovoltaic backsheets: comparison of the aging induced changes on module and component level10.1002/app.42093 ↗
40. Characterization of mechanical behavior of UV cured urethane acrylate nanocomposite films loaded with silane treated nanosilica by the aid of nanoindentation and nanoscratch experiments10.1016/j.triboint.2013.08.010 ↗
41. Properties and degradation behaviour of polyolefin encapsulants for photovoltaic modules10.1002/pip.3323 ↗
42. Effect of cross-linking on the microstructure and mechanical properties of ultra-high molecular weight polyethylene10.1097/01.blo.0000185310.59202.e5 ↗
43. Cross-linking–Effect on physical properties of polymers10.1080/15583726908545897 ↗
44. Determining the degree of crosslinking of ethylene vinyl acetate photovoltaic module encapsulants—a comparative study10.1016/j.solmat.2013.04.022 ↗
45. Properties of crosslinked polyolefin-based materials10.1016/0079-6700(95)98859-N ↗
46. Plasticization and antiplasticization in polycarbonates: the role of diluent motion10.1021/ma980205g ↗
47. 2004
48. The effects of UV light on the chemical and mechanical properties of a transparent epoxy-diamine system in the presence of an organic UV absorber10.3390/ma10020180 ↗
49. Effects of UV stabilizers on polypropylene outdoors10.3390/ma13071626 ↗
50. Quantification of UV protecting additives in ethylene-vinyl acetate copolymer encapsulants for photovoltaic modules with pyrolysis-gas chromatography-mass spectrometry10.1016/j.polymertesting.2022.107913 ↗
51. Additive diffusion coefficients in polyolefins. II. Effect of swelling and temperature on the D = f(M) correlation10.1002/app.2094 ↗
52. Transport of small molecules in polyolefins. I. Diffusion of irganox 1010 in polyethylene10.1002/app.1992.070460317 ↗
53. Transport of small molecules in polyolefins. II. Diffusion and solubility of irganox 1076 in ethylene polymers10.1002/app.1993.070481104 ↗
54. Transport of small molecules in polyolefins. III. Diffusion of topanol CA in ethylene polymers10.1002/app.1994.070510908 ↗
55. A review of small molecule diffusion in polyolefins10.1016/0032-3861(92)91089-K ↗
56. FTIR investigation of EVA chemical bonding environment and its impact on debond energy10.1109/JPHOTOV.2019.2904219 ↗
57. Chemical and mechanical interfacial degradation in bifacial glass/glass and glass/transparent backsheet photovoltaic modules10.1002/pip.3602 ↗