Abstract

This paper presents a correlative analysis of the performance and degradation of advanced silicon photovoltaic (PV) technologies, including silicon heterojunction technology (HJT) and tunnel oxide passivated contact (TOPCon), benchmarked against mainstream passivated emitter rear contact (PERC) installed in hot arid environments. The field performance of novel encapsulant materials tailored for these different cell architectures under combined stresses will be presented. After three years of operation in an arid desert climate, the results indicate technology-dependent degradation trends, with HJT and TOPCon modules showing different susceptibility to encapsulant aging, while PERC modules do not show aging. Ultraviolet fluorescence (UVF) imaging reveals early-stage encapsulant degradation that correlates with power loss. Front and rear ethylene-vinyl acetate (EVA) on both HJT-1 and HJT-2 showed UVF degradation patterns. Front polyolefin elastomer (POE) on TOPCon showed distinct UVF degradation patterns. In terms of specific energy yield, TOPCon-2 technology is the best performer, followed closely by PERC-2 and HJT-2. HJT modules exhibit the highest indoor maximum power P max loss, reaching up to −1.7%/year and showing the largest performance variability. PERC modules demonstrate intermediate degradation rates of −1.0 to −1.7%/year, whereas TOPCon modules consistently achieve the lowest P max losses, ranging from −0.3 to −1.1%/year. Field degradation analysis shows that PERC and TOPCon strings exhibit consistently moderate and tightly bound degradation rates (−1.1 to −1.3%/year), whereas HJT strings display markedly higher variability, with accelerated degradation of −4.3%/year. This highlights the robust field stability of PERC and TOPCon technologies and the greater sensitivity of HJT to degradation. The comparison between indoor P max loss and field-derived degradation rates shows a consistent correlation across module types, while HJT-1 exhibits higher outdoor degradation due to field-induced encapsulant degradation and string-level losses.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Silicon and Solar Cell Technologies · Photovoltaic System Optimization Techniques · Silicon Carbide Semiconductor Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (16)

Show source-provided references
1. High-efficiency n-TOPCon cells ensured by an emitter preparation process without post-oxidation10.1016/j.solmat.2024.113223 ↗
2. Energy yield analysis of different bifacial PV (photovoltaic) technologies: topcon, HJT, PERC in Hainan10.1016/j.solener.2022.03.038 ↗
3. Nanocrystalline silicon oxide stacks for silicon heterojunction solar cells for hot climates10.1063/1.5049262 ↗
4. UV-induced degradation in TOPCon solar cells: hydrogen dynamics and impact of UV wavelength10.1016/j.solmat.2025.113895 ↗
5. Insights into mechanism of UV-induced degradation in silicon heterojunction solar cells10.1016/j.solmat.2024.113022 ↗
6. Predicting the lifetime of HJT modules towards the outdoor real-world environment10.1016/j.solmat.2024.112885 ↗
7. A novel damp heat-induced failure mechanism in PV modules (with case study in TOPCon)10.1016/j.solmat.2026.114195 ↗
8. Corrosion effects in bifacial crystalline silicon PV modules; interactions between metallization and encapsulation10.1016/j.solmat.2023.112321 ↗
9. Three failure modes in silicon heterojunction glass-backsheet modules10.1016/j.solmat.2023.112358 ↗
10. A reliability study of silicon heterojunction photovoltaic modules exposed to damp heat testing10.1016/j.mee.2019.111081 ↗
11. Early degradation of silicon heterojunction PV modules installed on horizontal single-axis trackers in desert climate10.1016/j.solmat.2025.113899 ↗
12. Unveiling the origin of metal contact failures in TOPCon solar cells through accelerated damp-heat testing10.1016/j.solmat.2024.113188 ↗
13. Enhancing the reliability of TOPCon technology by laser-enhanced contact firing10.1016/j.solmat.2024.112846 ↗
14. PV degradation methodology comparison — a basis for a standard
15. Robust PV degradation methodology and application10.1109/JPHOTOV.2017.2779779 ↗
16. Performance Index assessment for the PV fleet performance data initiative