Abstract
Mechanical tests for evaluating the fracture resistance of ceramics on chipping rectangular specimen edges were first performed with conical diamond indenters of 11–800 μm tip radii. In the experiments elastic silicon-nitride Si3N4 ceramics and inelastic zirconia TS ceramics, displaying a phase transition on fracture, were used, soda lime glass served as the object for comparison. The fracture resistance of those materials was shown to increase similarly when the above indenters are employed. Chip scars formed on the specimen edges of Si3N4 ceramics do not actually differ from those observed in glass tests (pseudoconical, nail-like, arbitrary). With an increase in the tip radius, the first ones grow in number. It does not take place in the tests of TS ceramics. Comparative fracture resistance estimates obtained with the edge chipping method using different fracturing tools were established to be invalid.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Tunneling and Rock Mechanics · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (11)
Show source-provided references
1. E. Almond and N. McCormick, “Constant geometry edge flaking of brittle materials,” Nature, 321, 53–55 (1986).10.1038/321053a0 ↗
2. N. McCormick and E. Almond, “Edge flaking of brittle materials,” J. Hard Mater., 1, 25–51 (1990).
3. G. A. Gogotsi and V. I. Galenko, “Edge fracture resistance of glasses: different conical indenters and the fracture initiation barrier,” Strength Mater., 48, No. 3, 365–370 (2016).10.1007/s11223-016-9772-1 ↗
4. G. A. Gogotsi, “Fracture resistance of ceramics: base diagram and R-line,” Strength Mater., 38, No. 3, 261–270 (2006).10.1007/s11223-006-0039-0 ↗
5. O. A. Batanova, G. A. Gogotsi, and Yu. G. Matvienko, “Numerical modeling edge chipping tests of ceramics,” Eng. Fract. Mech., 132, 38–47 (2014).10.1016/j.engfracmech.2014.10.014 ↗
6. ÑEN/TS 843-9. Advanced Technical Ceramics – Mechanical Properties of Monolithic Ceramics at Room Temperature – Part 9: Method of Test for Edge-Chip Resistance, CEN, Brussels (2010).
7. G. D. Quinn, A. A. Giuseppetti, and K. H. Hoffman, “Chipping fracture resistance of dental CAD/CAM restorative materials: Part I – Procedures and results,” Dental Mater., 30, 99–111 (2014).10.1016/j.dental.2014.02.010 ↗
8. A. Mohajerani and J. K. Spelt, “Edge chipping of borosilicate glass by blunt indentation,” Mech. Mater., 42, 1064–1080 (2010).10.1016/j.mechmat.2010.10.002 ↗
9. G. A. Gogotsi, “Edge chipping resistance of ceramics: Problems of test method,” J. Adv. Ceram., 2, 370–377 (2013).10.1007/s40145-013-0085-6 ↗
10. G. A. Gogotsi, “Classification of ceramics and glass (edge chipping and fracture toughness),” Ceram. Int., 40, 5591–5596 (2014).10.1016/j.ceramint.2013.10.151 ↗
11. R. C. Garvie, R. H. J. Hannink, and R. T. Pascoe, “Ceramic steel?,” Nature, 258, 703–704 (1975).10.1038/258703a0 ↗