Estimation of the Degree of Hydrogen Embrittlement of the Heat-Resistant KHN55MVTS Nickel Alloy
Bibliographic record
Abstract
No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.
Source: Not provided · Quality: missing
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Material Properties and Failure Mechanisms · Nuclear Materials and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (49)
Show source-provided references
1. R. B. Bhavsar, A. Collins, and S. Silverman, Use of alloy 718 and 725 in oil and gas industry, in: E. A. Loria (Ed.), Superalloys 718, 625, 706 and Various Derivatives (Proc. of the International Symposium on Superalloys 718, 625, 706 and Various Derivatives, Pittsburgh), TMS, Pennsylvania, USA (2001), pp. 47−55. https://doi.org/10.7449/2001/ Superalloys_2001_47_5510.7449/2001 ↗
2. J. Li, H. Wang, X. Yu, et al., Temperature-driven mechanisms of hydrogen embrittlement and electrochemical corrosion in Ni-based superalloy 600, J Mater Res Technol, 35, 6715–6727 (2025). https://doi.org/10.1016/j.jmrt.2025.03.04310.1016/j.jmrt.2025.03.043 ↗
3. B. Rivolta, R. Gerosa, D. Panzeri, et al., Optimization of the mechanical and corrosion resistance of alloy 625 through aging treatments, Crystals, 14, 139 (2024). https://doi.org/10.3390/cryst1402013910.3390/cryst14020139 ↗
4. O. I. Balitskii, Y. H. Kvasnytska, L. M. Ivaskevych, et al., Fatigue fracture of the blades of gas-turbine engines made of a new refractory nickel alloy, Mater Sci, 57, No. 4, 475–483 (2022). https://doi.org/10.1007/s11003-022-00568-z10.1007/s11003-022-00568-z ↗
5. T. Michler, J. Naumann, and M. P. Balogh, Hydrogen environment embrittlement of solution treated Fe–Cr–Ni superalloys, Mat Sci Eng A, 607, 71–80 (2014). https://doi.org/10.1016/j.msea.2014.03.13410.1016/j.msea.2014.03.134 ↗
6. T. Michler, Influence of gaseous hydrogen on the tensile properties of Fe-36Ni INVAR alloy, Int J Hydrogen Energy, 39, No. 22, 11807–11809 (2014). https://doi.org/10.1016/j.ijhydene.2014.05.13310.1016/j.ijhydene.2014.05.133 ↗
7. J. Jürgensen, A. Frehn, K. Ohla, et al., Effect of hydrogen charging on the mechanical properties of highstrength copper-base alloys, austenitic stainless steel AISI 321, Inconel 625 and ferritic steel 1.4511, Metals, 14, No. 5, 588 (2024). https://doi.org/10.3390/met1405058810.3390/met14050588 ↗
8. O. I. Balyts’kyi, L. M. Ivas’kevych, V. M. Mochul’s’kyi, et al., Influence of hydrogen on the crack resistance of 10Kh15N27T3V2MR steel, Mater Sci, 45, No. 2, 258–267 (2009). https://doi.org/10.1007/s11003-009-9184-510.1007/s11003-009-9184-5 ↗
9. O. I. Balyts’kyi, L. M. Ivas’kevich, and V. M. Mochulskyi, Temperature dependences of age-hardening austenitic steels mechanical properties in gaseous hydrogen, in: 12th International Conference on Fracture 2009 - ICF-12, Vol. 8, Curran Associates Inc., Canada (2009), pp. 5786–5792.
10. O. I. Zvirko, M. I. Hredil, O. T. Tsyrulnyk, et al., Method of assessing the influence of gaseous hydrogen on corrosion and hydrogenation of steels, Mater Sci, 59, No. 5, 524–531 (2024). https://doi.org/10.1007/s11003-024-00807-510.1007/s11003-024-00807-5 ↗
11. B. A. Abebe and E. Altuncu, A review on hydrogen embrittlement behavior of steel structures and measurement methods, Int Adv Res Eng J, 8, No. 2, 91–101 (2024). https://doi.org/10.35860/iarej.141408510.35860/iarej.1414085 ↗
12. A. Behvar, M. Haghshenas, and M. B. Djukic, Hydrogen embrittlement and hydrogen-induced crack initiation in additively manufactured metals: A critical review on mechanical and cyclic loading, Int J Hydrogen Energy, 58, No. 90, 1214–1239 (2024). https://doi.org/10.1016/j.ijhydene.2024.01.23210.1016/j.ijhydene.2024.01.232 ↗
13. J. Liu, M. Zhao, and L. Rong, Overview of hydrogen-resistant alloys for high-pressure hydrogen environment: on the hydrogen energy structural materials, Clean Energy, 7, No. 1, 99–115 (2023). https://doi.org/10.1093/ce/zkad00910.1093/ce/zkad009 ↗
14. A. I. Balitskii and L. M. Ivaskevich, Effect of alloying and heat treatment on embrittlement of Fe-Cr-Ni alloys in high-pressure hydrogen, Strength Mater, 55, No. 1, 79–89 (2023). https://doi.org/10.1007/s11223-023-00504-910.1007/s11223-023-00504-9 ↗
15. A. Krella, Hydrogen-induced degradation of metallic materials – a short review, Materials, 18, 597 (2025). https://doi.org/10.3390/ma1803059710.3390/ma18030597 ↗
16. Q. Li, H. Ghadiani, V. Jalilvand, et al., Hydrogen impact: A review on diffusibility, embrittlement mechanisms, and characterization, Materials, 17, 965 (2024). https://doi.org/10.3390/ma1704096510.3390/ma17040965 ↗
17. X. Li, J. Zhang, Y. Cui, et al., Review of the hydrogen embrittlement and interactions between hydrogen and microstructural interfaces in metallic alloys: Grain boundary, twin boundary, and nano-precipitate, Int J Hydrogen Energy, 72, No. 27, 74–109 (2024). https://doi.org/10.1016/j.ijhydene.2024.05.25710.1016/j.ijhydene.2024.05.257 ↗
18. V. G. Gavriljuk, V. M. Shyvaniuk, and S. M. Teus, Hydrogen in metallic alloys – embrittlement and enhanced plasticity: a review, Corros Rev, 42, No. 3, 267–301 (2024). https://doi.org/10.1515/corrrev-2022-006010.1515/corrrev-2022-0060 ↗
19. O. I. Balyts’kyi, L. M. Ivas’kevich, and V. M. Mochulskyi, Mechanical properties of martensitic steels in gaseous hydrogen, Strength Mater, 44, No. 1, 64–71 (2012). https://doi.org/10.1007/s11223-012-9350-010.1007/s11223-012-9350-0 ↗
20. G. G. Maksimovich, I. Yu. Tretyak, L. M. Ivas'kevich, et al., Role of the martensite transformation in hydrogen embrittlement of unstable austenitic steels, Sov Mater Sci, 21, No. 4, 320–323 (1986). https://doi.org/10.1007/BF0072655410.1007/BF00726554 ↗
21. V. I. Vitvitskii, V. I. Tkachev, M. F. Berezhnitskaya, et al., Assessment of mechanical properties and phasestructural state in corrosion-resistant steels under static and low-cycle loading, Strength Mater, 39, No. 5, 466–474 (2007). https://doi.org/10.1007/s11223-007-0052-y10.1007/s11223-007-0052-y ↗
22. M. Okayasu, H. Wen, and R. Kondo, Hydrogen embrittlement of austenitic stainless steels with different surface treatments, Int J Steel Struct, 24, 477–487 (2024). https://doi.org/10.1007/s13296-024-00829-410.1007/s13296-024-00829-4 ↗
23. I. M. Dmytrakh, O. D. Smiyan, and A. M. Syrotyuk, Experimental study of fatigue crack growth in pipeline steel under hydrogenating conditions, in: 18th Eur. Conf. on Fracture. Fracture of Materials and Structures from Micro to Macro Scale, (Dresden, Aug.-Sept. 2010), DVM, Dresden (2010). https://www.scopus.com/pages/publications/ 84870964956
24. I. M. Dmytrakh, A. M. Syrotyuk, and R. L. Leshchak, Specific features of the deformation and fracture of low-alloy steels in hydrogen-containing media: Influence of hydrogen concentration in the metal, Mater Sci, 54, No. 3, 295–308 (2018). https://doi.org/10.1007/s11003-018-0186-z10.1007/s11003-018-0186-z ↗
25. Yu. G. Bachynskyi, P. V. Basistyi, V. V. Fedorov, et al., The effect of heat treatment in hydrogen on the physical and mechanical properties of alloys of the iron-nickel system (up to 36% Ni), Solid State Physics and Chemistry (in Ukrainian), 3, No. 2, 355–360 (2002).
26. M. Elaieb, F. M. Shuaeib, R. O. Saied, et al., The influence of thermal cycling on the corrosion and hardness of the low carbon steel, Libya Appl Technol Sci, 2, No. 1, 24–28 (2013).
27. A. S. Afokhainu, Comparative analysis of the effect of thermal cycling on fatigue behavior of low and medium carbon steel, AJMIE, 2, No. 3, 130–136 (2017). https://doi.org/10.11648/j.ajmie.20170203.1310.11648/j.ajmie.20170203.13 ↗
28. B. R. Kumar, S. K. Das, S. Sharma, et al., Effect of thermal cycles on heavily cold deformed AISI 304L austenitic stainless steel, Mater Sci Eng A, 527, 875–882 (2010). https://doi.org/10.1016/j.msea.2009.08.07510.1016/j.msea.2009.08.075 ↗
29. T. Nanda, R. Kumar, and V. Singh, A thermal cycling route for processing nano-grains in AISI 316L stainless steel for improved tensile deformation behaviour, Defence Sci J, 66, No. 5, 529–535 (2016). https://doi.org/10.14429/dsj.66.994810.14429/dsj.66.9948 ↗
30. J. B. Coulibaly, M. Shah, and A. F. Rotta Loria, Thermal cycling effects on the structure and physical properties of granular materials, Granul Matter, 22, No. 80 (2020). https://doi.org/10.1007/s10035-020-01054-610.1007/s10035-020-01054-6 ↗
31. M. Oñoro, J. Macías-Delgado, M. A. Auger, et al., Mechanical properties and stability of precipitates of an ODS steel after thermal cycling and aging, Nucl Mater Energy, 24, 100758 (2020). https://doi.org/10.1016/j.nme.2020.10075810.1016/j.nme.2020.100758 ↗
32. K. Fu, C. Zhong, L. Zhang, et al., Effect of multiple thermal cycling on the microstructure and microhardness of Inconel 625 by high-speed laser cladding, J Mater Res Technol, 24, 1093–1107 (2023). https://doi.org/10.1016/j.jmrt.2023.03.06410.1016/j.jmrt.2023.03.064 ↗
33. D. Ducret, C. Laquerbe, A. Ballanger, et al., Separation of hydrogen isotopes by thermal cycling absorption process: An experimental device, Fusion Sci Technol, 41, 1092–1096 (2002). https://doi.org/10.13182/FST02-A2275210.13182/FST02-A22752 ↗
34. O. V. Kronshtal and V. S. Kharin, Effect of heterogeneity of materials and heat cycles on diffusion of hydrogen as a factor of the risk of development of hydrogen degradation of metals, Mater Sci, 28, No. 6, 475–486 (1992). https://doi.org/10.1007/BF0072445610.1007/BF00724456 ↗
35. Y. L. Ivanyts’kyi, O. V. Hembara, and O. Y. Chepil’, Determination of the durability of elements of power-generating equipment with regard for the influence of working media, Mater Sci, 51, No. 1, 104–113 (2015). https://doi.org/10.1007/s11003-015-9815-y10.1007/s11003-015-9815-y ↗
36. O. Z. Student, Accelerated method of hydrogen degradation of structural steels, Mater Sci, 34, No. 4, 497–507 (1998). https://doi.org/10.1007/BF0236070110.1007/BF02360701 ↗
37. A. V. Fishgoit and B. A. Kolachev, Strength tests in hydrogen in the aerospace industry, Mater Sci, 33, No. 4, 568–573 (1997). https://doi.org/10.1007/BF0253755510.1007/BF02537555 ↗
38. J. Moriyama, O. Takakuwa, M. Yamaguchi, et al., The contribution of Cr and Ni to hydrogen absorption energy in Fe-Cr-Ni austenitic systems: A first-principles study, Comput Mater Sci, 232, 112650 (2024). https://doi.org/10.1016/j.commatsci.2023.11265010.1016/j.commatsci.2023.112650 ↗
39. Y. Ogawa, H. Hosoi, K. Tsuzaki, et al., Hydrogen, as an alloying element, enables a greater strength-ductility balance in an Fe-Cr-Ni-based, stable austenitic stainless steel, Acta Mater, 199, 181–192 (2020). https://doi.org/10.1016/j.actamat.2020.08.02410.1016/j.actamat.2020.08.024 ↗
40. A. I. Balitskii, L. M. Ivaskevich, and O. A. Balitskii, Rotor steels crack resistance and fracture behavior for hydrogen targeted materials ever-widening database, Eng Fract Mech, 260, 108168 (2022). https://doi.org/10.1016/j.engfracmech.2021.10816810.1016/j.engfracmech.2021.108168 ↗
41. T. Michler, C. San Marchi, J. Naumann, et al., Hydrogen environment embrittlement of stable austenitic steels, Int J Hydrogen Energy, 37, No. 21, 16231–16246 (2012). https://doi.org/10.1016/j.ijhydene.2012.08.07110.1016/j.ijhydene.2012.08.071 ↗
42. V. I. Tkachov, L. M. Ivas’kevych, and V. I. Vytvyts’kyi, Methodological aspects of determination of hydrogen resistance of steels, Mater Sci, 38, No. 4. 484–493 (2002). https://doi.org/10.1023/A:102295021368610.1023/A:1022950213686 ↗
43. I. M. Dmytrakh, A. M Syrotyuk, and R. L. Leshchak, Effect of preliminary hydrogenation–dehydrogenation of low-alloy steel on its ability to absorb electrochemical hydrogen, Mater Sci, 57, No. 3. 387–396 (2021). https://doi.org/10.1007/s11003-021-00553-y10.1007/s11003-021-00553-y ↗
44. V. V. Panasyuk, O. Y. Andreykiv, and O. V. Gembara, Hydrogen degradation of materials under long-term operation of technological equipment, Int J Hydrogen Energy, 25, No. 1, 67–74 (2000). https://doi.org/10.1016/S0360-3199(99)00006-310.1016/S0360-3199(99)00006-3 ↗
45. V. I. Tkachov, L. M. Ivas'kevych, and O. M. Voznychak, Degradation of steel in gaseous hydrogen with inhibiting admixtures, Mater Sci, 43, No. 3, 377–382 (2007). https://doi.org/10.1007/s11003-007-0043-y10.1007/s11003-007-0043-y ↗
46. A. N. Romaniv, Influence of low-cycle loading frequency on the life of steels in a hydrogen atmosphere, Fiz-Khim Mekh Mater, 15, No. 3. 109–110 (1979).
47. A. Lee, Hydrogen embrittlement of nickel, cobalt and iron-based superalloys, in: R. P. Gangloff and B. P. Somerday (Eds.), Gaseous Hydrogen Embrittlement of Materials in Energy Technologies. Vol. 1. The Problem, its Characterization and Effects on Particular Alloy Classes, Woodhead Publ. Limited, Oxford- Cambridge-Philadelphia-New Delhi (2012), pp. 624–667. https://doi.org/10.1533/9780857093899.3.62410.1533/9780857093899.3.624 ↗
48. T. P. Groeneveld and A. R. Eisea, Mechanical testing methods, in: Hydrogen Embrittlement Testing, ASTM STP 543, ASTM, Philadelphia (1974), pp. 11–19.10.1520/STP38925S ↗
49. H. R. Gray, Testing for hydrogen environment embrittlement: experimental variables, in: Hydrogen Embrittlement Testing, ASTM STP 543, ASTM, Philadelphia (1974), pp. 133–151.10.1520/STP38935S ↗