Microstructural features and compressive properties of SLM Ti6Al4V lattice structures
Source abstract
Abstract
Abstract Lightweight lattice structures have great potentials for the application in medical industries due to their large specific surface area and high strength-to-weight ratio. Selective laser melting (SLM) as one of the most attractive additive manufacturing processes has been widely used for the fabrication of porous structures. In this study, two Ti6Al4V lattice structures, trabecular (Trab.) and triply periodic minimal surface (TPMS), were produced through SLM to study the microstructural distribution and compressive properties with different cell types. The results show that cell type has insignificant effect on the microstructure of the SLM lattice structures studied in this work. For both lattice samples, refined near-equiaxed β phase was formed in the lattice struts, while coarse β phase was formed in the solid bulk region. However, cell type posed significant effects on the compressive properties of the lattice structures. The Trab. structure was found to have higher compressive strength and better energy absorption capacity than the TPMS structure. This work demonstrated that the elastic modulus of Trab. (5.58 GPa) and TPMS (5.51 GPa) lattices could be comparable to that of natural bones (0.022–21 GPa) through rational structural parameters design, which can avoid the stress shielding effect that always occurs on biomedical implant.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Cellular and Composite Structures
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (40)
Show source-provided references
1. Globularization using heat treatment in additively manufactured Ti-6Al-4V for high strength and toughness10.1016/j.actamat.2018.09.064 ↗
2. Microstructure evolution and high-temperature oxidation behaviour of selective laser melted TiC/TiAl composites10.1016/j.surfcoat.2019.07.059 ↗
3. Effects of post homogeneity heat treatment processes on microstructure evolution behavior and tensile mechanical properties of laser additive manufactured ultrahigh-strength AerMet100 steel10.1016/j.msea.2018.02.090 ↗
4. EBSD study of beam speed effects on Ti-6Al-4V alloy by powder bed electron beam additive manufacturing10.1016/j.jallcom.2018.03.173 ↗
5. Location-related thermal history, microstructure, and mechanical properties of arc additively manufactured 2Cr13 steel using cold metal transfer welding10.1016/j.msea.2017.12.076 ↗
6. The effect of NiB additive on surface morphology and microstructure of 316L stainless steel single tracks and layers obtained by SLM10.1016/j.surfcoat.2016.09.019 ↗
7. Thermal-induced microstructural evolution and defect distribution of wire-arc additive manufacturing 2Cr13 part: numerical simulation and experimental characterization10.1016/j.applthermaleng.2019.114335 ↗
8. Thermal expansion properties of laser melting deposited Ti-6.5 Al-2Zr-1Mo-1V alloy during α+β zone annealing10.1016/j.matchar.2017.01.019 ↗
9. Microstructural characterization of cellular AlSi10Mg alloy fabricated by selective laser melting10.1016/j.matdes.2018.08.005 ↗
10. Inconel 625 lattice structures manufactured by selective laser melting (SLM): mechanical properties, deformation and failure modes
11. Additive manufacturing of Ti-6Al-4V lattice structures with high structural integrity under large compressive deformation10.1016/j.jmst.2018.10.029 ↗
12. Investigation of effects of process parameters on microstructure and hardness of SLM manufactured SS316L10.1016/j.jallcom.2018.01.098 ↗
13. Mechanical properties and deformation behavior of additively manufactured lattice structures of stainless steel10.1016/j.matdes.2018.02.062 ↗
14. High strain rate mechanical behavior of Ti-6Al-4V octet lattice structures additively manufactured by selective laser melting (SLM)10.1016/j.msea.2018.12.101 ↗
15. Mechanical and in vitro study of an isotropic Ti6Al4V lattice structure fabricated using selective laser melting10.1016/j.jallcom.2018.12.220 ↗
16. A mechanical property evaluation of graded density Al-Si10-Mg lattice structures manufactured by selective laser melting10.1016/j.msea.2016.06.013 ↗
17. Mechanics of additively manufactured biomaterials10.1016/j.jmbbm.2017.03.018 ↗
18. Compressive failure modes and energy absorption in additively manufactured double gyroid lattices
19. Effect of heat treatment on the microstructure and mechanical properties of Ti6Al4V gradient structures manufactured by selective laser melting10.1016/j.msea.2018.08.084 ↗
20. Improved fatigue endurance ratio of additive manufactured Ti-6Al-4V lattice by hot isostatic pressing10.1016/j.matdes.2017.08.048 ↗
21. Topological design, permeability and mechanical behavior of additively manufactured functionally graded porous metallic biomaterials10.1016/j.actbio.2018.12.013 ↗
22. Additively-manufactured functionally graded Ti-6Al-4V lattice structures with high strength under static and dynamic loading: experiments10.1016/j.ijimpeng.2017.09.018 ↗
23. Evaluations of cellular lattice structures manufactured using selective laser melting10.1016/j.ijmachtools.2012.06.002 ↗
24. Ultrahigh-strength titanium gyroid scaffolds manufactured by selective laser melting (SLM) for bone implant applications10.1016/j.actamat.2018.08.005 ↗
25. Open-cellular copper structures fabricated by additive manufacturing using electron beam melting10.1016/j.msea.2011.03.053 ↗
26. The development of TiNi-based negative Poisson’s ratio structure using selective laser melting10.1016/j.actamat.2015.12.017 ↗
27. Mechanical properties and energy absorption capability of functionally graded F2BCC lattice fabricated by SLM10.1016/j.matdes.2018.01.059 ↗
28. Porous tantalum structures for bone implants: fabrication, mechanical and in vitro biological properties10.1016/j.actbio.2010.01.046 ↗
29. Inconel 625 lattice structures manufactured by selective laser melting (SLM): mechanical properties, deformation and failure modes10.1016/j.matdes.2018.06.010 ↗
30. High-strength porous biomaterials for bone replacement: a strategy to assess the interplay between cell morphology, mechanical properties, bone ingrowth and manufacturing constraints10.1016/j.actbio.2015.10.048 ↗
31. Tensile and compression properties of variously arranged porous Ti-6Al-4V additively manufactured structures via SLM10.1016/j.prostr.2018.12.025 ↗
32. Effect of geometry on the mechanical properties of Ti-6Al-4V Gyroid structures fabricated via SLM: a numerical study10.1016/j.matdes.2019.108165 ↗
33. The select of internal architecture for porous Ti alloy scaffold: a compromise between mechanical properties and permeability10.1016/j.matdes.2020.108754 ↗
34. Microstructural tailoring of As-Selective Laser Melted Ti6Al4V alloy for high mechanical properties
35. The origin of microstructural diversity, texture, and mechanical properties in electron beam melted Ti-6Al-4V10.1007/s11661-010-0397-x ↗
36. Investigation into the dynamic mechanical properties of selective laser melted Ti-6Al-4V alloy at high strain rate tensile loading10.1016/j.msea.2019.01.010 ↗
37. The role of lattice defects, element partitioning and intrinsic heat effects on the microstructure in selective laser melted Ti-6Al-4V10.1016/j.actamat.2019.01.039 ↗
38. Additive manufacturing of metals10.1016/j.actamat.2016.07.019 ↗
39. Characterization of wire arc additive manufacturing 2Cr13 part: process stability, microstructural evolution, and tensile properties10.1016/j.jallcom.2018.03.222 ↗
40. Microstructure and mechanical properties of CuSn/18Ni300 bimetallic porous structures manufactured by selective laser melting10.1016/j.matdes.2019.107583 ↗