Microstructural features and corrosion behavior of Fe-based coatings prepared by an integrated process of extreme high-speed laser additive manufacturing
Source abstract
Abstract
Abstract A kind of integrated process of extreme high-speed laser cladding (EHLC) and laser remelting (LR) was firstly proposed to comprehensively improve surface quality and internal interlayer bonding strength of pure EHLCed coatings. The influence mechanism of integrated process on microstructure and corrosion resistance was carefully studied. The integrated process effectively optimized the surface roughness (reduced >60%), and eliminated interlayer defects, especially for the multi-layer coating. Results indicated that both of the coatings manufactured by EHLC and EHLC-LR comprised dominant ultrafine grains. However, electrochemical measurements showed that the EHLC-LRed coating possessed better corrosion resistance and lower corrosion rate compared to EHLCed counterpart. It was proposed that this behavior was due to a high density of ultra-fine grains with numerous grain boundaries uniformly distributed on the coating surface forming a more stable oxide film.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Welding Techniques and Residual Stresses
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (41)
Show source-provided references
1. Materials creation adds new dimensions to 3D printing10.1007/s11434-016-1191-y ↗
2. Mechanical properties and electrochemical corrosion resistance of multilayer laser cladded Fe-based composite coatings on 4Cr5MoSiV1 steel10.1016/j.jmatprotec.2020.116736 ↗
3. High temperature chlorine-induced corrosion of Ni50Cr coating: HVOLF, HVOGF, cold spray and laser cladding10.1016/j.surfcoat.2018.01.025 ↗
4. Investigation on in-situ laser cladding coating of the 304 stainless steel in water environment10.1016/j.jmatprotec.2020.116949 ↗
5. Wear and corrosion resistance of laser cladding AISI 304 stainless steel/Al2O3 composite coatings10.1016/j.surfcoat.2013.10.028 ↗
6. Investigations on ultra-high-speed laser material deposition as alternative for hard chrome plating and thermal spraying10.2351/1.4943910 ↗
7. EHLA: extreme high-speed laser material deposition; economical and effective protection against corrosion and wear10.1002/latj.201700020 ↗
8. Investigations on ultra-high-speed laser material deposition as alternative for hard chrome plating and thermal spraying
9. A comparative study on microstructure and properties of traditional laser cladding and high-speed laser cladding of Ni45 alloy coatings
10. Extreme high-speed laser material deposition (EHLA) of AISI 430 steel10.3390/coatings9120778 ↗
11. Effect of microstructure on the corrosion resistance of coatings by extreme high speed laser cladding10.1016/j.apsusc.2020.146085 ↗
12. High-temperature oxidation behaviour of CuAlNiCrFe high-entropy alloy bond coats deposited using high-speed laser cladding process10.1016/j.surfcoat.2020.126093 ↗
13. Microstructure and corrosion properties of FeCoNiCrMn high entropy alloy coatings prepared by high speed laser cladding and ultrasonic surface mechanical rolling treatment10.1016/j.matlet.2019.126769 ↗
14. Microstructure and mechanical properties of thin-wall structure by hybrid laser metal deposition and laser remelting process10.1016/j.optlastec.2020.106087 ↗
15. Comparative study of stainless steel AISI 431 coatings prepared by extreme-high-speed and conventional laser cladding10.2351/1.5094378 ↗
16. Effect of laser remelting on the microstructure and corrosion property of the arc-sprayed AlFeNbNi coatings
17. Effects of laser additive manufacturing on microstructure and crystallographic texture of austenitic and martensitic stainless steels
18. Assessment of laser power and scan speed influence on microstructural features and consolidation of AISI H13 tool steel processed by additive manufacturing
19. High-performance integrated additive manufacturing with laser shock peening –induced microstructural evolution and improvement in mechanical properties of Ti6Al4V alloy components10.1016/j.ijmachtools.2019.103475 ↗
20. Elucidation of bubble evolution and defect formation in directed energy deposition based on direct observation
21. Laser powder-bed fusion additive manufacturing: physics of complex melt flow and formation mechanisms of pores, spatter, and denudation zones10.1016/j.actamat.2016.02.014 ↗
22. Investigation on recrystallization and precipitation behaviors of Al-4.5Cu-1.5 Mg alloy refined by Ti-supported TiC nanoparticles10.1016/j.jallcom.2019.05.323 ↗
23. A closer inspection of a grain boundary immune to intergranular corrosion in a sensitized Al-Mg alloy10.1016/j.corsci.2018.01.009 ↗
24. Crystal orientation, crystallographic texture and phase evolution in the Ti-45Al-2Cr-5Nb alloy processed by selective laser melting10.1016/j.matchar.2016.01.012 ↗
25. Lippold · 2014 · 86
26. Investigation on cored-eutectic structure in Ni60/WC composite coatings fabricated by wide-band laser cladding10.1016/j.jallcom.2015.04.136 ↗
27. Modification of surface characteristics and electrochemical corrosion behaviour of laser powder bed fused stainless-steel 316L after laser polishing
28. Corrosion behavior of AZ31 magnesium alloy in the chloride solution containing ammonim nitrate10.1016/j.electacta.2018.05.059 ↗
29. Anisotropic corrosion behavior of Sc and Zr modified Al-Mg alloy produced by selective laser melting10.1016/j.corsci.2020.108657 ↗
30. Structure and corrosion resistance properties of Ni-Fe-B-Si-Nb amorphous composite coatings fabricated by laser processing10.1016/j.jallcom.2013.06.111 ↗
31. Understanding effect of 3.5wt. % NaCl on the corrosion of Al0.1CoCrFeNi high-entropy alloy10.1016/j.jnucmat.2017.08.015 ↗
32. EIS evaluation of steady-state characteristic of 316L stainless steel passive film grown in acidic solution10.1016/j.elecom.2012.09.040 ↗
33. Electrochemical corrosion behaviour of 2A02 Al alloy under an accelerated simulation marine atmospheric environment10.1016/j.jmst.2018.09.060 ↗
34. Comparative effect of grain size and texture on the corrosion behaviour of commercially pure titanium processed by equal channel angular pressing10.1016/j.corsci.2009.08.017 ↗
35. The effects of hydrogen on anodic dissolution and passivation of iron in alkaline solutions10.1016/j.corsci.2015.09.013 ↗
36. Revealing the relationship between grain size and corrosion rate of metals10.1016/j.scriptamat.2010.08.035 ↗
37. Laser shock peening-induced surface gradient stress distribution and extension mechanism in corrosion fatigue life of AISI 420 stainless steel10.1016/j.corsci.2020.109027 ↗
38. Grain size distribution effects on the corrosion behaviour of materials10.1016/j.corsci.2012.04.040 ↗
39. An investigation on the continuous and uniform thin membrane passive film formed on sputtered nanocrystalline stainless steel10.1016/j.corsci.2015.11.031 ↗
40. The enhancement of microstructure on the passive and pitting behaviors of selective laser melting 316L SS in simulated body fluid, Appl10.1016/j.apsusc.2018.10.150 ↗
41. The passivity of selective laser melted 316L stainless steel10.1016/j.apsusc.2019.144495 ↗