Synthesis and characterization of Ti 2 AlC coatings by magnetron sputtering from three elemental targets and ex-situ annealing
Source abstract
Abstract
Abstract MAX phase materials have demonstrated great potential applications both as bulk and coating due to their unique properties. Deposition of phase-pure polycrystalline MAX phase coatings often remains a challenge. In this study, Ti-C-Al elemental nanolayer stacks deposited by non-reactive magnetron sputtering followed by ex-situ annealing was adopted to prepare Ti2AlC coatings on two different substrates, Si and SiO2/Si. No Ti2AlC phase was formed on Si substrate due to significant interdiffusion between the coating and the substrate during annealing. Phase-pure, i.e. single-phase Ti2AlC coatings with 3 μm thickness on SiO2/Si were obtained after 800 °C annealing in argon for 10 min. The crystalline transition from the non-MAX competing phases to Ti2AlC MAX phase was found to appear in the region of 600 °C–700 °C. The microstructural evolution of the coatings during annealing from 600 °C to 900 °C was systematically investigated by X-Ray diffraction (XRD), Raman spectroscopy and transmission electron microscopy (TEM). The reaction path for the formation of Ti2AlC is suggested as follows: first, aluminum reacted with titanium to form a Ti-Al intermetallic phase (i.e. Al3Ti), and the diffusion between the residue titanium and carbon produced non-stoichiometric TiCx; then, the reaction between the Al3Ti intermetallic and TiCx yielded the formation of Ti2AlC MAX phase.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: MXene and MAX Phase Materials · Metal and Thin Film Mechanics · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (64)
Show source-provided references
1. The MN+1AXN phases: a new class of solids; thermodynamically stable nanolaminates10.1016/S0079-6786(00)00006-6 ↗
2. Progress in research and development on MAX phases: a family of layered ternary compounds10.1179/1743280410Y.0000000001 ↗
3. The Mn+1AXn phases: materials science and thin-film processing10.1016/j.tsf.2009.07.184 ↗
4. Barsoum · 2013
5. Alumina forming high temperature silicides and carbides10.1016/j.ceramint.2003.12.046 ↗
6. On the effect of texture on the mechanical and damping properties of nanocrystalline Mg-matrix composites reinforced with MAX phases10.1016/j.msea.2010.01.073 ↗
7. MAX phase carbides and nitrides: properties for future nuclear power plant in-core applications and neutron transmutation analysis10.1016/j.nucengdes.2011.12.009 ↗
8. Cold spray deposition of Ti2AlC coatings for improved nuclear fuel cladding10.1016/j.jnucmat.2015.06.028 ↗
9. Tribological behavior of selected Mn+1AXn phase thin films on silicon substrates10.1016/j.surfcoat.2014.08.034 ↗
10. Synthesis and characterization of a remarkable ceramic: Ti3SiC210.1111/j.1151-2916.1996.tb08018.x ↗
11. Layered machinable and electrically conductive Ti2AlC and Ti3AlC2 ceramics: a review10.1016/S1005-0302(10)60064-3 ↗
12. Deposition of Ti2AlC and Ti3AlC2 epitaxial films by magnetron sputtering10.1063/1.1780597 ↗
13. Nanostructured plasma etched, magnetron sputtered nanolaminar Cr2AlC MAX phase thin films10.1016/j.apsusc.2013.12.099 ↗
14. Phase stability of epitaxially grown Ti2AlN thin films10.1063/1.2335681 ↗
15. Thermal stability of Ti3SiC2 thin films10.1016/j.actamat.2006.10.010 ↗
16. Microstructure evolution of V–Al–C coatings synthesized from a V2AlC compound target after vacuum annealing treatment10.1016/j.jallcom.2015.11.170 ↗
17. Sputter deposition from a Ti2AlC target: process characterization and conditions for growth of Ti2AlC10.1016/j.tsf.2009.11.059 ↗
18. MAX phase formation by intercalation upon annealing of TiCx/Al (0.4<x<1) bilayer thin films10.1016/j.actamat.2011.06.029 ↗
19. Growth and property characterization of epitaxial MAX-phase thin films from the Tin+1(Si, Ge, Sn)Cn systems10.4028/www.scientific.net/AST.45.2648 ↗
20. Characterization of Cr–Al–C and Cr–Al–C–Y films synthesized by high power impulse magnetron sputtering at a low deposition temperature10.1016/j.tsf.2015.03.008 ↗
21. Cathodic arc co-deposition of highly oriented hexagonal Ti and Ti2AlC MAX phase thin films10.1016/j.tsf.2010.09.007 ↗
22. Towards the synthesis of MAX-phase functional coatings by pulsed laser deposition10.1016/j.apsusc.2007.07.156 ↗
23. CVD of Ti3SiC210.1002/1521-3862(200011)6:6<289::AID-CVDE289>3.0.CO;2-4 ↗
24. Microstructure of high velocity oxy-fuel sprayed Ti2AlC coatings10.1007/s10853-010-4263-4 ↗
25. Cold-spray deposition of Ti2AlC coatings10.1016/j.vacuum.2013.01.023 ↗
26. Influence of water vapor on the oxidation behavior of Ti3AlC2 and Ti2AlC10.1016/j.scriptamat.2007.09.011 ↗
27. Oxidation behavior of Ti3AlC2 at 1000–1400°C in air10.1016/S0010-938X(02)00177-4 ↗
28. A critical review of the oxidation of Ti2AlC, Ti3AlC2 and Cr2AlC in air10.1080/21663831.2013.806364 ↗
29. Effect of neutron irradiation on defect evolution in Ti3SiC2 and Ti2AlC10.1016/j.jnucmat.2015.10.030 ↗
30. Investigations on Radiation Tolerance of Mn+1AXn Phases: Study of Ti3SiC2, Ti3AlC2,Cr2AlC, Cr2GeC, Ti2AlC, and Ti2AlN10.1111/jace.13450 ↗
31. Growth and characterization of MAX-phase thin films10.1016/j.surfcoat.2004.08.174 ↗
32. Deposition and characterization of ternary thin films within the Ti–Al–C system by DC magnetron sputtering10.1016/j.jcrysgro.2006.03.008 ↗
33. Synthesis and characterization of Ti2AlC and Ti2AlN MAX phase coatings manufactured in an industrial-size coater10.4028/www.scientific.net/AMR.89-91.208 ↗
34. Oxidation behaviour of Ti–Al–C films composed mainly of a Ti2AlC phase10.1016/j.corsci.2011.05.033 ↗
35. Preparation of Ti2AlC MAX phase coating by DC magnetron sputtering deposition and vacuum heat treatment10.1016/j.jmst.2015.10.014 ↗
36. The scaling behavior and mechanism of Ti2AlC MAX phase coatings in air and pure water vapor10.1016/j.surfcoat.2015.03.037 ↗
37. Towards large area MAX phase coatings on steel10.1002/srin.200506000 ↗
38. Temperature-dependent microstructural evolution of Ti2AlN thin films deposited by reactive magnetron sputtering10.1016/j.apsusc.2016.01.229 ↗
39. Oxygen incorporation in Ti2AlC thin films10.1063/1.2838456 ↗
40. Substrate orientation effects on the nucleation and growth of the Mn+1AXn phase Ti2AlC10.1063/1.3527960 ↗
41. Ti2AlC coatings deposited by high velocity oxy-fuel spraying10.1016/j.surfcoat.2008.06.184 ↗
42. Oxidation of Ti2AlC bulk and spray deposited coatings10.1016/j.corsci.2010.08.004 ↗
43. Thin film synthesis of Ti3SiC2 by rapid thermal processing of magnetron-sputtered Ti-C-Si multilayer systems10.1002/adem.201200180 ↗
44. Diamond-like amorphous carbon10.1016/S0927-796X(02)00005-0 ↗
45. Investigations on the oxidation behavior of MAX-phase based Ti2AlC coatings on γ-TiAl10.1002/9780470944103.ch16 ↗
46. Interpretation of Raman spectra of disordered and amorphous carbon10.1103/PhysRevB.61.14095 ↗
47. Vibrational behavior of the Mn+1AXn phases from first-order Raman scattering (M=Ti,V,Cr, A=Si, X=C,N)10.1103/PhysRevB.71.012103 ↗
48. Ion sputter-deposition and in-air crystallisation of Cr2AlC films10.1016/j.vacuum.2013.07.045 ↗
49. Raman study of phase transformation of TiO2 rutile single crystal irradiated by infrared femtosecond laser10.1016/j.apsusc.2007.03.047 ↗
50. Raman scattering induced by carbon vacancies in TiCx10.1103/PhysRevB.17.1546 ↗
51. First-order Raman scattering of the MAX phases: Ti2AlN, Ti2AlC0.5N0.5, Ti2AlC, (Ti0.5V0.5)2AlC, V2AlC, Ti3AlC2, and Ti3GeC210.1002/jrs.3036 ↗
52. Linear thermal expansion coefficient of silicon from 293 to 1000K10.1023/B:IJOT.0000022336.83719.43 ↗
53. Thermal and electrical properties of Nb2AlC, (Ti, Nb)2AlC and Ti2AlC10.1007/s11661-002-0262-7 ↗
54. Crystallization kinetics of amorphous Cr2AlC thin films10.1016/j.surfcoat.2011.06.003 ↗
55. Rapid synthesis of bulk Ti2AlC by self-propagating high temperature combustion synthesis with a pseudo–hot isostatic pressing process10.1557/jmr.2009.0327 ↗
56. Solid±liquid reaction synthesis and simultaneous densification of polycrystalline Ti2AlC
57. Synthesis and microstructure of layered-ternary Ti2AlC ceramic by high energy milling and hot pressing10.1016/j.msea.2008.01.017 ↗
58. Thermodynamic description of the Al–C–Ti system10.1016/j.jallcom.2014.10.119 ↗
59. Mn+1AXn phases in the Ti-Si-C system studied by thin-film synthesis and ab initio calculations10.1103/PhysRevB.70.165401 ↗
60. Deposition of single-crystal Ti2AlN thin films by reactive magnetron sputtering from a 2Ti:Al compound target10.1063/1.2785958 ↗
61. Magnetron sputtered epitaxial single-phase Ti3SiC2 thin films10.1063/1.1494865 ↗
62. Microstructural evolution during film growth10.1116/1.1601610 ↗
63. Microstructure and mechanism of damage tolerance for Ti3SiC2 bulk ceramics10.1007/s100190050114 ↗
64. Stable M2AlC(0001) surfaces (M=Ti, V and Cr) by first-principles investigation10.1088/0953-8984/20/22/225006 ↗