journal article·2016-05

Structure, adhesion and corrosion behavior of CrN/TiN superlattice coatings deposited by the combined deep oscillation magnetron sputtering and pulsed dc magnetron sputtering

Y.X. Ou, J. Lin, S. Tong, W.D. Sproul, M.K. Lei

Publisher page

Abstract

Abstract Deep oscillation magnetron sputtering (DOMS) is a novel high power impulse magnetron sputtering technique, which offers large voltage oscillation packets to generate a stable high-power discharge plasma with high ionization under virtually arc-free conditions. CrN/TiN superlattice coatings with various modulated periods (Λ) were deposited by the combined DOMS and pulsed dc magnetron sputtering. CrN/TiN superlattice coatings with the Cr/(Cr + Ti) ratio ranging from 0.177 to 0.496 exhibited a single phase face-centered cubic structure with a strong (111) texture. As the Λ was increased from 5.7 to 10.2 nm, the residual stress was increased from − 2.1 to − 5.6 GPa. The increase in Λ led to an initial increase, followed by a decrease in hardness, and the H/E* and H3/E*2 ratios. The coating at Λ = 6.3 nm showed the highest adhesion with the highest HF level in Rockwell C tests and critical loads in scratch tests due to the highest hardness of 36 GPa, H/E* ratio of 0.093 and H3/E*2 ratio of 0.316. The predominant adhesive failure mode in scratch tests was buckling failure independent of the changes of Λ and substrate hardness. However, the increase in substrate hardness resulted in an increase in critical loads (LC1, LC2, LC3 and LC4), especially for a significant increase in LC3, due to the increased cooperative deformation of a coating/substrate system by increasing toughness of coatings, cohesion/adhesion and substrate hardness. The increased adhesion was responsible for the increased pitting and stress corrosion cracking resistance in 3.5 wt.% NaCl aqueous solution due to the optimized Cr/(Cr + Ti) ratio and Λ.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research · Ion-surface interactions and analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (47)

Show source-provided references
1. Nanometer scale multilayered coatings10.1016/S0042-207X(99)00148-7 ↗
2. Dry sliding wear of magnetron sputtered TiN/CrN superlattice coatings10.1016/S0257-8972(03)00516-4 ↗
3. Corrosion resistance of multi-layered plasma-assisted physical vapour deposition TiN and CrN coatings10.1016/S0257-8972(01)01267-1 ↗
4. Corrosion of CrN and CrN/TiN coated heat-resistant steels in molten A356 aluminum alloy10.1016/S0257-8972(01)01484-0 ↗
5. Influence of lamellae thickness on the corrosion behaviour of multilayered PVD TiN/CrN coatings10.1016/S0040-6090(99)00192-3 ↗
6. Structure, hardness and thermal stability of nanolayered TiN/CrN multilayer coatings10.1016/j.vacuum.2003.08.003 ↗
7. CrN/AlN superlattice coatings synthesized by pulsed closed field unbalanced magnetron sputtering with different CrN layer thicknesses10.1016/j.tsf.2009.02.136 ↗
8. A review of adhesion test methods for thin hard coatings10.1116/1.573616 ↗
9. Endurance of TiAlSiN coatings: effect of Si and bias on wear and adhesion10.1016/j.wear.2011.01.009 ↗
10. Improvement of the corrosion resistance of CrN coated steel by an interlayer10.1016/S0257-8972(98)00646-X ↗
11. High rate thick film growth10.1146/annurev.ms.07.080177.001323 ↗
12. The inter-relationship between coating microstructure and the tribological performance of PVD coatings
13. Recent advances in modulated pulsed power magnetron sputtering for surface engineering10.1007/s11837-011-0092-4 ↗
14. Baglin · 1989
15. Investigation of high power impulse magnetron sputtering pretreated interfaces for adhesion enhancement of hard coatings on steel10.1016/j.surfcoat.2005.11.082 ↗
16. Mechanical and tribological properties of multilayered PVD TiN/CrN10.1016/S0043-1648(99)00149-0 ↗
17. Residual stress, surface defects and corrosion resistance of CrN hard coatings10.1016/S0257-8972(98)00731-2 ↗
18. Corrosion protection of CrN/TiN multi-coating for bipolar plate of polymer electrolyte membrane fuel cell10.1016/j.tsf.2011.01.207 ↗
19. Anatase and rutile TiO2 films deposited by arc-free deep oscillation magnetron sputtering10.1088/0022-3727/46/8/084008 ↗
20. Wear and corrosion resistance of CrN/TiN superlattice coatings deposited by a combined deep oscillation magnetron sputtering and pulsed dc magnetron sputtering10.1016/j.apsusc.2015.05.110 ↗
21. Practical measurement of the residual stress in coatings10.1016/0257-8972(95)02531-6 ↗
22. Noyan · 1987
23. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
24. Lieberman · 2005
25. Recent progress in large scale manufacturing of multilayer superlattice hard coatings10.1016/S0257-8972(00)00959-2 ↗
26. Lide · 1991
27. Phase formation and structure of magnetron sputtered chromium nitride films: in-situ and ex-situ studies10.1016/j.surfcoat.2003.12.026 ↗
28. Structure and mechanical properties of polycrystalline CrN/TiN superlattices10.1116/1.581439 ↗
29. Attwood · 1999
30. Ion-assisted growth of Ti1−xAlxN/Ti1−yNbyN multilayers by combined cathodic-arc/magnetron-sputter deposition10.1016/S0040-6090(96)09524-7 ↗
31. Multilayer PVD coatings for wear protection10.1016/0257-8972(95)02555-3 ↗
32. Structure and stress of TiAlN/CrN superlattice coatings as a function of CrN layer thickness10.1016/S0257-8972(99)00132-2 ↗
33. Effect of the Cr content on the mechanical properties of nanostructured TiN/CrN coatings10.1016/j.surfcoat.2003.09.020 ↗
34. Mechanical and tribological properties of CrN/TiN multilayer coatings deposited by pulsed dc magnetron sputtering10.1016/j.surfcoat.2015.06.064 ↗
35. Model of superlattice yield stress and hardness enhancements10.1063/1.359467 ↗
36. Hardening by spinodal modulated structure10.1016/0001-6160(80)90163-7 ↗
37. Multilayer, multicomponent, and multiphase physical vapor deposition coatings for enhanced performance10.1116/1.579361 ↗
38. Structure and properties of high power impulse magnetron sputtering and DC magnetron sputtering CrN and TiN films deposited in an industrial scale unit10.1016/j.tsf.2010.05.062 ↗
39. Failure mode maps in the thin film scratch adhesion test10.1016/S0301-679X(97)00012-1 ↗
40. An overview of the potential of quantitative coating adhesion measurement by scratch testing10.1016/j.triboint.2005.04.013 ↗
41. The study of the adhesion of a TiN coating on steel and titanium alloy substrates using a multi-mode scratch tester10.1016/j.triboint.2005.04.011 ↗
42. The correlation of scratch adhesion with composite hardness for TiN coatings10.1016/S0257-8972(00)00541-7 ↗
43. Toughness of hard nanostructure ceramic thin films10.1016/j.surfcoat.2006.07.020 ↗
44. The effect of the substrate on the mechanical properties of TiN coatings10.1016/S0257-8972(02)00652-7 ↗
45. Fracture mechanics of diamond-like carbon (DLC) films coated on flexible polymer substrates10.1016/j.surfcoat.2006.12.008 ↗
46. Wear and corrosion properties of plasma-based low-energy nitrogen ion implanted titanium10.1016/j.surfcoat.2011.03.141 ↗
47. Combined cathodic arc/unbalanced magnetron grown CrN/NbN superlattice coatings for corrosion resistant applications10.1016/S0257-8972(99)00439-9 ↗