journal article·2002-04

Atmospheric corrosion of bare and anodised aluminium in a wide range of environmental conditions. Part II: Electrochemical responses

V López, J.A González, E Otero, E Escudero, M Morcillo

Surface and Coatings Technology· Volume 153· Issue 2-3
Publisher page

Abstract

This study compares the behaviour of aluminium in the bare condition and when protected with anodic films of approximately 7, 17 and 28 μm thickness for up to 42 months of exposure in 11 atmospheres of very different agressivities, with salinity values ranging between 2.1 and 684 mg Cl- m-2 d-1. The results of a previous study based on visual inspection and traditional gravimetric techniques are complemented by the application, essentially, of electrochemical impedance spectroscopy (EIS). The specimens were characterised by EIS when recently obtained and after 12, 24 and 42 months of exposure in the different testing stations. Exposure leads to an improvement in all the quality indices of anodic films, irrespective of their thickness or the degree of environmental pollution. Anodising and sealing prevents localised corrosion - which is characteristic of aluminium in marine or industrial atmosphere - even in the most unfavourable situations, except in the case of 7 μm films, the lowest thickness tested. © 2002 Elsevier Science B.V. All rights reserved.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Anodic Oxide Films and Nanostructures · Concrete Corrosion and Durability · Smart Materials for Construction

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (24)

Show source-provided references
1. J.A. González, M. Morcillo, E. Escudero, V. López, E. Otero, Submitted to Surf. Coat. Technol. (Part I of this work).
2. Pietschman · Aluminium · 1983 · 69 · 1019
3. Pietschman · Aluminium · 1983 · 69 · 1081
4. Pietschman · Aluminium · 1984 · 70 · 82
5. Bautista · Prog. Org. Coat. · 1996 · 28 · 54810.1016/0300-9440(95)00555-2 ↗
6. Spoelstra · Mater. Corros. · 2000 · 51 · 15510.1002/(SICI)1521-4176(200003)51:3<155::AID-MACO155>3.0.CO;2-3 ↗
7. Nordlien · Mater. Corros. · 2000 · 51 · 47310.1002/1521-4176(200007)51:7<473::AID-MACO473>3.0.CO;2-C ↗
8. Lizarbe · Pinturas y Acabados Industriales · 1998 · 40 · 45
9. López · Corros. Sci. · 1998 · 40 · 69310.1016/S0010-938X(97)00171-6 ↗
10. Oelsner · Aluminium · 1978 · 54 · 530
11. Spooner · 1963 · 127
12. Carter · J. Inst. Metals · 1972 · 100 · 208
13. Skerrey · 1982 · 329
14. González · Corros. Sci. · 1997 · 39 · 110910.1016/S0010-938X(97)00019-X ↗
15. Hoar · Electrochim. Acta · 1962 · 7 · 33310.1016/0013-4686(62)87009-1 ↗
16. Hitzing · Corros. Sci. · 1984 · 24 · 94510.1016/0010-938X(84)90115-X ↗
17. Hitzing · J. Electrochem. Soc. · 1986 · 103 · 88710.1149/1.2108756 ↗
18. Debuyck · Surf. Coat. Technol. · 1988 · 34 · 31110.1016/0257-8972(88)90121-1 ↗
19. Mansfeld · Werk. Korr. · 1985 · 36 · 47310.1002/maco.19850361102 ↗
20. Lizarbe · Rev. Metal. Madrid · 1990 · 26 · 359
21. Lizarbe · Aluminium · 1992 · 68 · 140
22. UNE standards, UNE-EN 12373-4:1999, UNE-EN 12373-5:1999.
23. González · J. Appl. Electrochem. · 1999 · 29 · 22910.1023/A:1003481418291 ↗
24. González · J. Electrochem. Soc. · 2000 · 147 · 98410.1149/1.1393301 ↗