Abstract Laser cladding has been developed to be an important surface modification technique in re-manufacturing and maintenance fields. However, few components can be fabricated directly to their final shape and simultaneously met the dimension and accuracy requirements by laser cladding method. A ball burnishing process has been adopted as an alternative finishing approach to grinding process. The effects of sequential turning and burnishing process on surface topography, residual stress, microhardness, porosity content and bonding strength of the Cr–Ni-based stainless steel cladding were systematically investigated in this research. Surface topography, residual stress and microhardness were improved by the sequential burnishing process due to the plastic deformation caused by rolling ball. Biaxial compressive residual stress states were generated in the cladding layer. Both the porosity and bonding strength of cladding layer were improved because of the generation of compressive residual stress. The bonding strength of the cladding layer showed several times higher than other coatings formed by high velocity oxy-fuel (HVOF) as well as plasma spraying. The surface integrities of the cladding layers were further evaluated with five-axial polar diagrams. Burnishing process showed a dependency on the pre-procedure, while smooth surfaces would weaken the burnishing effect induced by the rolling ball. The processing chain, sequential turning with wiper insert adopting a high feed rate and burnishing process, is optimized based on the required surface integrity.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High Entropy Alloys Studies · High-Temperature Coating Behaviors · Additive Manufacturing Materials and Processes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. Abrasive wear behaviour of laser clad and flame sprayed-melted NiCrBSi coatings10.1016/j.surfcoat.2005.10.032 ↗
2. Hot corrosion behavior of a centimeter Fe-based amorphous composite coating prepared by laser cladding in molten Na2SO4+K2SO4 salts10.1016/j.surfcoat.2015.03.022 ↗
3. Solidification behaviour in laser cladding of AlCoCrCuFeNi high-entropy alloy on magnesium substrates10.1016/j.jallcom.2013.10.254 ↗
4. Microstructure and properties of laser cladding FeCrBSi composite powder coatings with higher Cr content10.1016/j.jmatprotec.2013.12.009 ↗
5. Experimental investigations of cutting parameters influence on cutting forces in turning of Fe-based amorphous overlay for remanufacture10.1007/s00170-012-4212-2 ↗
6. Experimental observations on surface roughness, chip morphology, and tool wear behavior in machining Fe-based amorphous alloy overlay for remanufacture10.1007/s00170-012-4588-z ↗
7. Cutting force models for Fe–Al-based coating processed by a compound NC machine tool
8. Study on chip morphology and milling characteristics of laser cladding layer10.1007/s00170-014-6483-2 ↗
9. Effect of rare earth oxide on the properties of laser cladding layer and machining vibration suppressing in side milling10.1016/j.apsusc.2014.09.195 ↗
10. Investigation on the cutting process of plasma sprayed iron base alloys10.4028/www.scientific.net/KEM.447-448.821 ↗
11. Study on the machining of iron-based thermal spray coating for sleeveless engine cylinder10.4028/www.scientific.net/AMR.472-475.991 ↗
12. Grinding force, specific energy and material removal mechanism in grinding of HVOF-sprayed WC–Co–Cr coating10.1080/10426914.2013.872261 ↗
13. Effect of grinding on the residual stress and adhesion strength of HVOF thermally sprayed WC–10Co–4Cr coating10.1080/10426914.2014.930893 ↗
14. Effects of grinding process on residual stresses in nanostructured ceramic coatings10.1023/A:1016174731658 ↗
15. Grinding of nanostructured ceramic coatings: surface observations and material removal mechanisms10.1016/S0890-6955(02)00115-3 ↗
16. Grinding of nanostructural ceramic coatings: damage evaluation10.1016/S0890-6955(02)00157-8 ↗
17. Surface integrity improvement of laser cladded parts by ball burnishing
18. P.S. Prevey III, Burnishing method and apparatus for providing a layer of compressive residual stress in the surface of a workpiece, US Patent 5,826,453, 1998.
19. Comparison of surface textures produced by finish cutting, abrasive and burnishing operations in terms of their functional properties
20. Surface improvement of shafts by the deep ball-burnishing technique10.1016/j.surfcoat.2011.11.045 ↗
21. Influence of low-plasticity ball burnishing on the high-cycle fatigue strength of medium carbon AISI 1045 steel10.1016/j.ijfatigue.2013.06.024 ↗
22. Thermally sprayed finestructured WC–12Co coatings finished by ball burnishing and grinding as an innovative approach to protect forming tools against wear10.1016/j.surfcoat.2014.06.039 ↗
23. Friction analysis of thermally sprayed coatings finished by ball burnishing and grinding10.1007/s11740-013-0485-z ↗
24. Prediction of roughness after ball burnishing of thermally coated surfaces10.1016/j.jmatprotec.2014.11.008 ↗
25. Some studies on design and performance analysis of a new low plasticity burnishing tool
26. Fracture toughness determinations by indentation10.1111/j.1151-2916.1976.tb10991.x ↗
27. Determination of interfacial fracture toughness of thermal spray coatings by indentation10.1007/s11666-013-9961-4 ↗
28. Effect of thermal treatments on adhesive properties of a NiCr thermal sprayed coating10.1016/S0040-6090(00)01450-4 ↗
29. Surface integrity enhancement of Inconel 718 by using roller burnishing process
30. Comparative assessment of wiper and conventional ceramic tools on surface roughness in hard turning AISI 4140 steel10.1016/j.measurement.2013.06.018 ↗
31. Surface finish generated in hard turning of quenched alloy steel parts using conventional and wiper ceramic inserts10.1016/j.ijmachtools.2006.01.009 ↗
32. Removal of heat-formed coating from a titanium alloy using high pressure waterjet: influence of machining parameters on surface texture and residual stress10.1016/j.jmatprotec.2015.03.053 ↗
33. Analysis of residual stresses induced by dry turning of difficult-to-machine materials10.1016/j.cirp.2008.03.076 ↗
34. Residual stress measurements in laser clad repaired low pressure turbine blades for the power industry10.1016/j.msea.2006.04.065 ↗
35. Comparative evaluation of conventional and wiper ceramic tools on cutting forces, surface roughness, and tool wear in hard turning AISI D2 steel10.1243/09544054JEM762 ↗
36. Machinability investigations in hard turning of AISI D2 cold work tool steel with conventional and wiper ceramic inserts10.1016/j.ijrmhm.2008.12.007 ↗
37. Ultrafine-grained surface layer on Mg–Al–Zn alloy produced by cryogenic burnishing for enhanced corrosion resistance10.1016/j.scriptamat.2011.06.013 ↗
38. Grain refined and basal textured surface produced by burnishing for improved corrosion performance of AZ31B Mg alloy10.1016/j.corsci.2011.12.018 ↗
39. Temperature variation in the workpiece and in the cutting tool when dry milling Inconel 71810.1007/s00170-014-6006-1 ↗
40. Residual stress effect on hardness and yield strength of Ni thin film10.1016/j.surfcoat.2012.07.002 ↗
41. Adhesive and cohesive properties by indentation method of plasma-sprayed hydroxyapatite coatings10.1016/j.apsusc.2006.11.002 ↗
42. Methodology for evaluating effects of material characteristics on machinability-theory and statistics-based modelling applied on Alloy 71810.1007/s00170-011-3503-3 ↗