Corrosion behavior of Ni-P-nano-Al 2 O 3 composite coating in the presence of anionic and cationic surfactants
Source abstract
Abstract
Abstract Ni-P-nano-Al2O3 composite coatings on the mild steel were obtained by adding Al2O3 nanoparticles into the traditional electroless Ni-P bath. Cationic and anionic surfactants were used to prevent the agglomeration of the incorporated nano-Al2O3. Surface morphology, compositions and microstructures of the coating were studied using scanning electron microscopy (SEM), energy dispersive spectrometer (EDS), and X-ray diffraction (XRD) as well. Corrosion resistances of the modified mild steel samples were evaluated in 3.5 wt.% NaCl solution by electrochemical impedance spectroscopy (EIS). The results showed that compared to the pure Ni-P coating on the mild steel, the coating formed in the bath with 6 g/L nano-Al2O3 performed the highest resistance. Under the optimal conditions, the adding of anionic surfactant (SDBS) improved the anti-corrosion performance of the samples further, while the addition of cationic surfactant led to a worse corrosion resistance. The potential mechanism was that anionic surfactant molecules would contact with active sites of Ni-P composite coating and nano-Al2O3 in the bath, which would improve the dispersion of nano-Al2O3, thus leading to a homogeneous coating with better corrosion resistance.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electrodeposition and Electroless Coatings · Electrochemical Analysis and Applications · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (24)
Show source-provided references
1. Crobu · Electrochim. Acta · 2008 · 53 · 336410.1016/j.electacta.2007.11.071 ↗
2. Afroukhteh · Appl. Surf. Sci. · 2012 · 258 · 259710.1016/j.apsusc.2011.10.101 ↗
3. Ashassi-Sorkhabi · Corros. Sci. · 2013 · 77 · 18510.1016/j.corsci.2013.07.046 ↗
4. Xu · Surf. Coat. Technol. · 2005 · 191 · 16110.1016/j.surfcoat.2004.03.045 ↗
5. Farzaneh · Appl. Surf. Sci. · 2013 · 276 · 69710.1016/j.apsusc.2013.03.156 ↗
6. Wang · Thin Solid Films · 2011 · 519 · 590510.1016/j.tsf.2011.03.007 ↗
7. Amell · Surf. Coat. Technol. · 2010 · 205 · 35610.1016/j.surfcoat.2010.06.059 ↗
8. Karthikeyan · Appl. Surf. Sci. · 2014 · 307 · 65410.1016/j.apsusc.2014.04.092 ↗
9. Hamdy · Surf. Coat. Technol. · 2007 · 202 · 16210.1016/j.surfcoat.2007.05.030 ↗
10. Balaraju · Surf. Coat. Technol. · 2006 · 200 · 393310.1016/j.surfcoat.2005.03.007 ↗
11. Afroukhteh · Prog. Nat. Sci.-Mater. · 2012 · 22 · 31810.1016/j.pnsc.2012.06.006 ↗
12. de Hazan · J. Colloid Interface Sci. · 2008 · 328 · 10310.1016/j.jcis.2008.08.033 ↗
13. Sadreddini · Appl. Surf. Sci. · 2015 · 324 · 39310.1016/j.apsusc.2014.10.144 ↗
14. Rabizadeh · Mater. Des. · 2011 · 32 · 13310.1016/j.matdes.2010.06.021 ↗
15. Islam · Surf. Coat. Technol. · 2015 · 261 · 14110.1016/j.surfcoat.2014.11.044 ↗
16. He · Ceram. Int. · 2014 · 40 · 1665310.1016/j.ceramint.2014.08.027 ↗
17. Afroukhteh · Prog. Nat. Sci.-Mater. · 2012 · 22 · 48010.1016/j.pnsc.2012.10.005 ↗
18. Zielinska · J. Colloid Interface Sci. · 2012 · 377 · 36210.1016/j.jcis.2012.03.049 ↗
19. de Hazan · J. Colloid Interface Sci. · 2012 · 365 · 16310.1016/j.jcis.2011.09.032 ↗
20. Calderón · Electrochim. Acta · 2014 · 124 · 19010.1016/j.electacta.2013.08.185 ↗
21. Man · Surf. Coat. Technol. · 2014 · 249 · 11810.1016/j.surfcoat.2014.03.054 ↗
22. Yin · Surf. Coat. Technol. · 2013 · 228 · 3410.1016/j.surfcoat.2013.04.001 ↗
23. Ji · J. Taiwan Inst. Chem. E. · 2016 · 66 · 30110.1016/j.jtice.2016.07.007 ↗
24. Sudagar · Prog. Org. Coat. · 2012 · 74 · 78810.1016/j.porgcoat.2011.10.022 ↗