Influence of preliminary metal-ion etching on the topography and mechanical behavior of TiAlN coatings on cemented carbides
Source abstract
Abstract
Metal-ion etching is widely used in substrate surface modification before coating by physical vapor deposition . In this work, TiAlN coatings were synthesized onto cemented carbides with Ti-, Cr-, and Zr-ion pre-etching by cathodic arc evaporation and investigated concerning surface topography and mechanical failure. The pre-etching of energetic metal ions introduces droplet defects and increases surface roughness through uneven bombardment . The high interface roughness and deposition of nanoscale metal interlayers contributed to the upgraded adhesion between the coating and the substrate. As a result, the adhesion strength of TiAlN coatings advances to more than 95 N by applying Cr- and Zr-ion pre-etching. The rough substrate surface also gives rise to a rough coating surface associated with the pre-etching time. Under normal loading, the microscopic pit-like surface morphology , stemming from ion etching, interrupts the transverse propagation of the circumferential cracks but does not affect the longitudinal crack propagation inside the coating. In addition, the higher roughness of coatings with ion pre-etching causes a shorter run-in stage during ball-on-disc tests due to the higher contact stress between the friction pair .
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (49)
Show source-provided references
1. Performance of PVD TiN, TiCN, and TiAlN coated cemented carbide tools in turning10.1016/S0263-4368(99)00008-6 ↗
2. Coated tools for metal cutting-features and applications10.1016/S0007-8506(07)63231-4 ↗
3. Tool life and wear mechanisms of TiN coated tools in an intermittent cutting operation10.1016/S0924-0136(01)00852-4 ↗
4. Advanced PVD-TiAlN coatings on carbide and cermet cutting tools10.1016/S0257-8972(97)00503-3 ↗
5. The influence of metallic interlayers on the adhesion of PVD TiN coatings on high-speed steel10.1016/j.wear.2006.11.053 ↗
6. High temperature oxidation and cutting performance of AlCrN, TiVN and multilayered AlCrN/TiVN hard coatings10.1016/j.surfcoat.2017.06.080 ↗
7. Effect of interlayers on the structure and properties of TiAlN based coatings on WC-co cemented carbide substrate10.1016/j.ijrmhm.2012.10.017 ↗
8. Scratch adhesion and tribological behaviour of graded Cr/CrN/CrTiN coatings synthesized by closed-field unbalanced magnetron sputtering10.1016/j.wear.2017.03.020 ↗
9. Improvement of PVD coated inserts cutting performance, through appropriate mechanical treatments of substrate and coating surface10.1016/S0257-8972(01)01485-2 ↗
10. Influence of surface integrity on performance of coated cutting tools10.1016/S0040-6090(97)00571-3 ↗
11. Influence of subsurface properties on the adhesion strength of sputtered hard coatings10.1016/S0257-8972(99)00226-1 ↗
12. Influence of substrate pre-treatments on residual stresses and tribo-mechanical properties of TiAlN-based PVD coatings10.1016/j.surfcoat.2014.08.075 ↗
13. SEM study of defects in PVD hard coatings10.1016/j.vacuum.2007.07.005 ↗
14. Influence of ar ion etching on the surface topography of cemented carbide cutting inserts10.1016/j.ijrmhm.2017.08.015 ↗
15. Development of a superlattice (Ti, hf, Cr)N coating for cold metal forming applications10.1016/S0257-8972(03)00935-6 ↗
16. Study of macrodroplet and growth mechanisms with and without ion etchings on the properties of TiN coatings deposited on HSS using cathodic arc physical vapour deposition technique10.1016/j.msea.2007.04.030 ↗
17. Effect of cathodic arc PVD parameters on roughness of TiN coating on steel substrate10.1016/j.cap.2009.07.007 ↗
18. Optimization of in situ substrate surface treatment in a cathodic arc plasma: a study by TEM and plasma diagnostics10.1116/1.1349726 ↗
19. Ion charge state distributions of vacuum arc plasmas: the origin of species10.1103/PhysRevE.55.969 ↗
20. Multiply stripped ion generation in the metal vapor vacuum arc10.1063/1.340429 ↗
21. Interface microstructure engineering by high power impulse magnetron sputtering for the enhancement of adhesion10.1063/1.2697052 ↗
22. Enhanced adhesion through local epitaxy of transition-metal nitride coatings on ferritic steel promoted by metal ion etching in a combined cathodic arc/unbalanced magnetron deposition system10.1116/1.582414 ↗
23. Chromium nitride coatings grown by unbalanced magnetron (UBM) and combined arc/unbalanced magnetron (ABS™) deposition techniques10.1016/S0257-8972(96)02949-0 ↗
24. The interface between TiAlN hard coatings and steel substrates generated by high energetic Cr+ bombardment10.1016/S0257-8972(99)00552-6 ↗
25. Ion flux from vacuum arc cathode spots in the absence and presence of a magnetic field10.1063/1.1459619 ↗
26. Droplet formation on steel substrates during cathodic steered arc metal ion etching10.1016/S0042-207X(96)00307-7 ↗
27. SEM image analysis of droplet formation during metal ion etching by a steered arc discharge10.1016/S0257-8972(97)00137-0 ↗
28. Defects in TiN and TiAIN coatings grown by combined cathodic arc/unbalanced magnetron technology10.1016/0042-207X(94)E0029-X ↗
29. Microstructures of TiN films grown by various physical vapour deposition techniques10.1016/0257-8972(91)90128-J ↗
30. In situ lift-out: steps to improve yield and a comparison with other FIB TEM sample preparation techniques10.1016/j.micron.2008.02.006 ↗
31. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
32. Growth defect density in PVD hard coatings prepared by different deposition techniques10.1016/j.surfcoat.2013.09.020 ↗
33. Growth defects in PVD hard coatings10.1016/j.vacuum.2009.05.018 ↗
34. Combined filtered cathodic arc etching pretreatment–magnetron sputter deposition of highly adherent CrN films10.1116/1.2730512 ↗
35. Time-averaged and time-resolved ion fluxes related to reactive HiPIMS deposition of ti-Al-N films10.1016/j.surfcoat.2021.127638 ↗
36. X-ray diffraction studies of physically vapour-deposited coatings10.1016/0257-8972(89)90124-2 ↗
37. Failure mode analysis of TiN-coated high speed steel: in situ scratch adhesion testing in the scanning electron microscope10.1016/0257-8972(90)90128-Y ↗
38. An overview of the potential of quantitative coating adhesion measurement by scratch testing10.1016/j.triboint.2005.04.013 ↗
39. Effect of contact geometry on the failure modes of thin coatings in the scratch adhesion test10.1016/S0257-8972(02)00064-6 ↗
40. Scratch adhesion characteristics of PVD TiAlN deposited on high speed steel, cemented carbide and PCBN substrates10.1016/j.wear.2013.08.025 ↗
41. Residual stresses in PVD hard coatings10.1016/0257-8972(95)02581-2 ↗
42. Tribology of thin coatings10.1016/S0272-8842(00)00015-8 ↗
43. Tribological aspects related to the morphology of PVD hard coatings10.1016/j.surfcoat.2017.09.084 ↗
44. Origin of friction in running-in sliding wear of nitride coatings10.1007/s11249-009-9548-x ↗
45. The influence of growth defects in sputter-deposited TiAlN hard coatings on their tribological behavior10.1016/j.surfcoat.2016.01.021 ↗
46. Influence of substrate roughness and coating thickness on adhesion, friction and wear of TiN films10.1016/S0257-8972(97)00182-5 ↗
47. Influence of surface roughness of PVD coatings on tribological performance in sliding contacts10.1016/j.surfcoat.2006.08.103 ↗
48. Influence of surface topography of arc-deposited TiN and sputter-deposited WC/C coatings on the initial material transfer tendency and friction characteristics under dry sliding contact conditions10.1016/j.surfcoat.2008.12.011 ↗
49. Effect of the modulation geometry on mechanical and tribological properties of TiSiN/TiAlN nano-multilayer coatings10.1016/j.surfcoat.2021.127586 ↗