Removing loose oxide layer and producing dense α-phase layer simultaneously to improve corrosion resistance of Ti-6Al-4V titanium alloy by coupling electrical pulse and ultrasonic treatment
Source abstract
Abstract
Abstract The loose oxide layer on the surface of Ti-6Al-4V titanium alloy can be removed and a dense α-phase layer with the thickness of 11 μm can be produced simultaneously by coupling electrical pulse and ultrasonic treatment (CEPUT). In addition, after CEPUT, the surface grain is refined, the surface roughness is reduced to 0.529 μm, and the surface hardness reaches to 627 HV, showing significant gradient change. During the CEPUT, the processability of the α-phase oxygen-rich layer is improved by the electroplasticity of high peak currents, and the α-phase oxygen-rich layer produces large plastic deformation. Most of the α-phase oxygen-rich layer is removed after the CEPUT, and the remaining coarse α-phase grains are refined to form a dense α-phase layer. The corrosion resistance of the dense oxide layer on the surface has been studied. The results show that the self-corrosion current density of the sample in the NaCl solution decreases to −8.4922E-08 A/cm2 after CEPUT. Compared with the untreated sample, the self-corrosion current density is reduced by two orders of magnitude. The reason for the increased corrosion resistance of titanium alloys may be that the electrolyte is blocked by the dense and intact α-phase layer on the surface and cannot penetrate further into the titanium alloy.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electromagnetic Effects on Materials · Surface Treatment and Residual Stress · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (50)
Show source-provided references
1. 3-D finite element process simulation of micro-end milling Ti-6Al-4V titanium alloy: experimental validations on chip flow and tool wear10.1016/j.jmatprotec.2015.02.019 ↗
2. Alpha casing and superplastic behavior of Ti-6Al-4V10.1016/S0924-0136(00)00849-9 ↗
3. Tool wear prediction of machining hydrogenated titanium alloy Ti6Al4V with uncoated carbide tools10.1007/s00170-013-4788-1 ↗
4. Tool life and surface integrity in turning titanium alloy10.1016/S0924-0136(01)00926-8 ↗
5. Effect of surface reaction layer on grindability of cast titanium alloys10.1016/j.dental.2005.04.020 ↗
6. Surface characterization of cast Ti-6Al-4V in hydrofluoric-nitric pickling solutions10.1016/S0257-8972(03)00747-3 ↗
7. Material morphological characteristics in laser ablation of alpha case from titanium alloy10.1016/j.apsusc.2012.04.173 ↗
8. Parametric effects on grit embedment and surface morphology in an innovative hybrid waterjet cleaning process for alpha case removal from titanium alloys10.1016/j.procir.2013.03.077 ↗
9. Removal of heat-formed coating from a titanium alloy using high pressure waterjet: influence of machining parameters on surface texture and residual stress10.1016/j.jmatprotec.2015.03.053 ↗
10. Surface analysis and corrosion resistance of a new titanium base alloy in simulated body fluids10.1016/j.corsci.2012.08.042 ↗
11. Corrosion of titanium alloys in aqueous solutions of hydrochloric acid10.1007/BF02539094 ↗
12. High pressure waterjets – an innovative means of alpha case removal for superplastically formed titanium alloys10.4028/www.scientific.net/KEM.433.103 ↗
13. Effect of different acid treatment on surface characteristics of titanium alloy10.4028/www.scientific.net/MSF.694.490 ↗
14. Improvement of the fatigue characteristics of VT1-0 titanium alloy by the surface mechanical and rapid thermal treatment10.1007/s11003-006-0092-7 ↗
15. Wear and corrosion behaviour of various surface treated medical grade titanium alloy in bio-simulated environment10.1016/j.wear.2009.01.056 ↗
16. Preparation of titanium oxide and hydroxyapatite on Ti-6Al-4V alloy surface and electrochemical behaviour in bio-simulated fluid solution10.1016/j.corsci.2013.11.059 ↗
17. Formation of titanium oxide by thermal-electrochemical process on the blasted titanium alloys substrate10.4028/www.scientific.net/AMR.650.12 ↗
18. Effect of pickling and mechanical surface treatment methods on adhesion strength of Ti oxide layer formed on titanium alloy substrate
19. Effect of cold rolling treatment on the formation of titanium oxide layer on Ti6Al4V alloys by thermal-electrochemical anodizing processes10.4028/www.scientific.net/MSF.737.54 ↗
20. Effect of electron-beam processing on structure of electroexplosive electroerosion resistant coatings of CuO-Ag system
21. Effect of electron-beam treatment on wear-resistant coatings applied by electroexplosive sputtering10.3103/S0967091217120105 ↗
22. Structure and properties of electro-explosive TiC-Ni-Mo coatings of die steel after electron-beam treatment10.1134/S2075113319030365 ↗
23. Surface characteristics and electrochemical corrosion behavior of a pre-anodized microarc oxidation coating on titanium alloy10.1016/j.msec.2013.05.011 ↗
24. Surface modification of titanium alloy orthopaedic implants via novel powder immersion reaction assisted coating nitriding method10.1016/S0921-5093(99)00111-2 ↗
25. Enhancing surface hardness of titanium alloy Ti-6Al-4V by combined nitriding and CVD coating10.1179/026708402225006187 ↗
26. Effect of multi-pass ultrasonic surface rolling on the mechanical and fatigue properties of HIP Ti-6Al-4V alloy10.3390/ma10020133 ↗
27. Effect of ultrasonic surface rolling at low temperatures on surface layer microstructure and properties of HIP Ti-6Al-4V alloy10.1016/j.surfcoat.2017.01.099 ↗
28. Influence of the ultrasonic surface rolling process on stress corrosion cracking susceptibility of high strength pipeline steel in neutral pH environment10.4028/www.scientific.net/KEM.433.103 ↗
29. Surface nanocrystallization of 17-4 precipitation-hardening stainless steel subjected to ultrasonic surface rolling process10.1016/j.msea.2018.04.033 ↗
30. Influence of the regime of electropulsing-assisted machining on the plastic deformation of the layer being cut10.3390/ma11060886 ↗
31. Microstructure homogenization of 7075 alloy by a novel electric pulse rheo-rolling process10.1080/10426914.2014.984204 ↗
32. Experimental study of electroplastic effect on stainless steel wire 304L10.1016/S0921-5093(99)00708-X ↗
33. Influence of grain size and grain boundaries on the thermal and mechanical behavior of 70/30 brass under electrically-assisted deformation10.1016/j.msea.2013.02.066 ↗
34. Nanocrystallization and enhanced surface mechanical properties of commercial pure titanium by electropulsing-assisted ultrasonic surface rolling10.1016/j.matdes.2018.04.027 ↗
35. Surface nanocrystallization and enhanced surface mechanical properties of nickel-based superalloy by coupled electric pulse and ultrasonic treatment10.1016/j.surfcoat.2019.07.037 ↗
36. Efficient fabrication of gradient nanostructure layer on surface of commercial pure copper by coupled electric pulse and ultrasonic treatment10.1016/j.jallcom.2018.06.042 ↗
37. Effect of electropulsing on surface mechanical properties and microstructure of AISI 304 stainless steel during ultrasonic surface rolling process10.1016/j.msea.2016.03.097 ↗
38. Effect of electropulsing-assisted ultrasonic nanocrystalline surface modification on the surface mechanical properties and microstructure of Ti-6Al-4V alloy10.1007/s11665-018-3248-3 ↗
39. Surface modification of D36 steel by ultrasonic impact with electropulsing10.1080/02670836.2017.1288310 ↗
40. Design and fabrication of a bending rotation fatigue test rig for in situ electrochemical analysis during fatigue testing of NiTi shape memory alloy wires10.1063/1.4793488 ↗
41. Potentiodynamic polarization study of the corrosion behavior of palladium-silver dental alloys10.1016/j.prosdent.2017.06.026 ↗
42. Tension-induced softening and hardening in gradient nanograined surface layer in copper10.1016/j.scriptamat.2014.01.006 ↗
43. Pulse current auxiliary bulging and deformation mechanism of AZ31 magnesium alloy10.1016/j.matdes.2011.08.007 ↗
44. Effect of ceramic conversion surface treatment on fatigue properties of Ti6Al4V alloy10.1016/j.ijfatigue.2006.11.016 ↗
45. A gradient nanostructure generated in pure copper by platen friction sliding deformation10.1016/j.scriptamat.2016.02.007 ↗
46. Corrosion behaviour of a new Ti-6Al-2Nb-1Ta alloy in various solutions10.1002/maco.201006041 ↗
47. Microstructure design to improve the corrosion and cavitation corrosion resistance of a nickel-aluminum bronze10.1016/j.corsci.2018.04.043 ↗
48. Mechanical properties and corrosion resistance of low rigidity quaternary titanium alloy for biomedical applications10.1016/S1003-6326(08)60365-9 ↗
49. Improving corrosion resistance of nickel-aluminum bronzes by surface modification with chromium ion implantation10.1016/j.surfcoat.2017.11.066 ↗
50. Improving corrosion resistance of a nickel- aluminum bronze alloy via nickel ion implantation10.5006/2097 ↗