journal article·2025-02Open access

Mechanical properties of DCMS and HiPIMS deposited Ti1-xMoxB2±z coatings

Anna Hirle, Philipp Dörflinger, Christoph Fuger, Christian Gutschka, Tomasz Wojcik, Maximilian Podsednik, Andreas Limbeck, Szilárd Kolozsvári, Peter Polcik, Carmen Jerg, Helmut Riedl, Rainer Hahn

Abstract

A promising strategy for enhancing the mechanical properties of sputtered transition metal diboride (TMB 2 ) thin films, including hardness and fracture toughness, is the formation of ternary diborides. Theoretical calculations indicate that incorporating Mo on the metallic sublattice of TiB₂ enhances the overall mechanical properties; however, no experimental data are available. Accordingly, two series (DCMS & HiPIMS) of Ti 1-x Mo x B 2±z coatings with varying Mo contents (x = 0 to 12 for DCMS and x = 0 to 9 for HiPIMS) were deposited using TiB 2 /MoB composite targets containing different MoB contents to investigate their structural and mechanical properties, focusing on fracture characteristics. HiPIMS growth processes have been proven to significantly enhance hardness, fracture toughness, and fracture strength compared to DCMS. Specifically, a hardness increase from 38.8 ± 1.7 GPa to 43.7 ± 1.2 GPa (nanoindentation) with a simultaneous fracture toughness increase of 0.4 MPa√m (~17 %; using microcantilever bending tests) and an increase in fracture strength, R p0.2 of approximately 2 GPa (micropillar compression) was observed for HiPIMS deposited coatings. Compared, our DCMS coatings showed a steady decrease in mechanical properties from H = 38.3 ± 1.5 GPa, K IC = 2.6 ± 0.15 MPa√m and R p0.2 = 13.7 ± 1 GPa to H = 27.2 ± 0.4 GPa, K IC = 1.7 ± 0.06 MPa√m and R p0.2 = 9.3 ± 0.3 GPa with increasing Mo content. Our research emphasizes the significance of energetics during film growth, particularly for new ternary diboride systems. • Successful deposition of Ti 1-x Mo x B 2±z thin films by using DCMS and HiPIMS • Influences of Mo and deposition technique on Ti 1-x Mo x B 2±z thin films were shown. • Enhanced micromechanical properties for HiPIMS deposited coatings
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Boron and Carbon Nanomaterials Research · MXene and MAX Phase Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (77)

Show source-provided references
1. Material properties of titanium diboride10.6028/jres.105.057 ↗
2. Evaluation of magnetron-sputtered TiB2 intended for tribological applications10.1016/S0257-8972(99)00638-6 ↗
3. Material selection for hard coatings10.1116/1.573700 ↗
4. Borides in thin film technology10.1006/jssc.1997.7456 ↗
5. Self-organized nanocolumnar structure in superhard TiB2 thin films10.1063/1.1887824 ↗
6. Revisiting the origins of super-hardness in TiB2+z thin films – impact of growth conditions and anisotropy10.1016/j.surfcoat.2022.128806 ↗
7. Tissue phase affected fracture toughness of nano-columnar TiB2 + z thin films10.1080/21663831.2023.2204120 ↗
8. Mechanical properties of superhard TiB2 coatings prepared by DC magnetron sputtering10.1016/j.vacuum.2007.07.036 ↗
9. Excess of boron in TiB2 superhard thin films: a combined experimental and ab initio study10.1088/0022-3727/44/38/385402 ↗
10. Experiment and simulation of the compositional evolution of Ti–B thin films deposited by sputtering of a compound target10.1063/1.2978211 ↗
11. Synthesis and characterization of TiBx (1.2 ≤ x ≤ 2.8) thin films grown by DC magnetron co-sputtering from TiB2 and Ti targets10.1016/j.surfcoat.2022.128110 ↗
12. Controlling the B/Ti ratio of TiBx thin films grown by high-power impulse magnetron sputtering10.1116/1.5026445 ↗
13. Improved oxidation properties from a reduced B content in sputter-deposited TiBx thin films10.1016/j.surfcoat.2021.127353 ↗
14. Microstructure and materials properties of understoichiometric TiBx thin films grown by HiPIMS10.1016/j.surfcoat.2020.126537 ↗
15. Influence of pulse frequency and bias on microstructure and mechanical properties of TiB2 coatings deposited by high power impulse magnetron sputtering10.1016/j.surfcoat.2016.06.086 ↗
16. Microstructure-driven strengthening of TiB2 coatings deposited by pulsed magnetron sputtering10.1016/j.surfcoat.2019.04.042 ↗
17. Design of hard coatings deposited by HiPIMS and dcMS10.1016/j.matlet.2020.128540 ↗
18. High-power impulse magnetron sputter deposition of TiBx thin films: effects of pressure and growth temperature10.1016/j.vacuum.2019.108884 ↗
19. Electronic mechanism for toughness enhancement inTixM1−xN(M=Moand W)10.1103/PhysRevB.81.104107 ↗
20. Supertoughening in B1 transition metal nitride alloys by increased valence electron concentration10.1016/j.actamat.2010.12.013 ↗
21. Valence electron concentration as an indicator for mechanical properties in rocksalt structure nitrides, carbides and carbonitrides10.1016/j.actamat.2018.04.033 ↗
22. Electronic mechanism of hardness enhancement in transition-metal carbonitrides10.1038/20148 ↗
23. Toughness enhancement in hard ceramic thin films by alloy design10.1063/1.4822440 ↗
24. Wear resistant TiMoN coatings deposited by magnetron sputtering10.1016/j.wear.2005.07.008 ↗
25. Vacancy-induced toughening in hard single-crystal V 0.5 Mo 0.5 N x /MgO(001) thin films10.1016/j.actamat.2014.06.025 ↗
26. Sorting transition-metal diborides: new descriptor for mechanical properties10.1016/j.actamat.2021.116685 ↗
27. Ab initio inspired design of ternary boride thin films10.1038/s41598-018-27426-w ↗
28. Designing thin film materials - ternary borides from first principles10.1016/j.tsf.2015.03.035 ↗
29. Effects of Mo target power on the structure and tribological properties of AlB2 Ta1-xMoxB films by magnetron sputtering10.1016/j.ijrmhm.2024.106623 ↗
30. Thermally induced planar defect formation in sputtered V1-xMoxB2-Δ films10.1016/j.scriptamat.2023.115365 ↗
31. Properties of spark plasma sintered compacts and magnetron sputtered coatings made from Cr, Mo, re and Zr alloyed tungsten diboride10.3390/coatings11111378 ↗
32. Influence of tantalum on phase stability and mechanical properties of WB210.1557/mrc.2019.5 ↗
33. Strategy for simultaneously increasing both hardness and toughness in ZrB2-rich Zr1−xTaxBythin films10.1116/1.5093170 ↗
34. Thermally-induced structure evolution in ternary Ti1−xYxB2+Δ films10.1016/j.scriptamat.2019.01.042 ↗
35. High-temperature oxidation resistance of ternary and quaternary Cr-(Mo)-Si-B2-z coatings — influence of Mo addition10.1016/j.surfcoat.2023.129733 ↗
36. Quantitative analysis of the platinum surface decoration on lanthanum strontium iron oxide thin films via online-LASIL-ICP-MS10.1016/j.microc.2021.106236 ↗
37. The HighScore suite10.1017/S0885715614000840 ↗
38. Measurement of thin film mechanical properties using nanoindentation10.1557/S0883769400041634 ↗
39. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
40. Critical review of analysis and interpretation of nanoindentation test data10.1016/j.surfcoat.2005.03.018 ↗
41. Celebrating the 100th anniversary of the Stoney equation for film stress: developments from polycrystalline steel strips to single crystal silicon wafers10.1016/j.tsf.2008.07.014 ↗
42. Direct observation of crack arrest after bridge notch failure: a strategy to increase statistics and reduce FIB-artifacts in micro-cantilever testing10.1016/j.matdes.2023.112188 ↗
43. Stress intensity factor dependence on anisotropy and geometry during micro-fracture experiments10.1016/j.scriptamat.2016.08.027 ↗
44. On the influence of microcantilever pre-crack geometries on the apparent fracture toughness of brittle materials10.1016/j.actamat.2017.07.014 ↗
45. Mode dependent evaluation of fracture behaviour using cantilever bending10.1016/j.tafmec.2021.103069 ↗
46. A comparative micro-cantilever study of the mechanical behavior of silicon based passivation films10.1016/j.tsf.2009.07.143 ↗
47. Numerical analysis of micropillar compression behaviour and stress-strain curve estimation verified on glass fused silica
48. Elevated temperature, nano-mechanical testing in situ in the scanning electron microscope10.1063/1.4795829 ↗
49. The relation between load and penetration in the axisymmetric boussinesq problem for a punch of arbitrary profile10.1016/0020-7225(65)90019-4 ↗
50. Efficient iterative schemes for ab initio total-energy calculations using a plane-wave basis set10.1103/PhysRevB.54.11169 ↗
51. From ultrasoft pseudopotentials to the projector augmented-wave method10.1103/PhysRevB.59.1758 ↗
52. Projector augmented-wave method10.1103/PhysRevB.50.17953 ↗
53. Available Pseudopotentials - VASP Wiki, (n.d.). https://www.vasp.at/wiki/index.php/Available_pseudopotentials (accessed October 21, 2024).
54. Special quasirandom structures10.1103/PhysRevLett.65.353 ↗
55. Models of configurationally-complex alloys made simple10.1016/j.cpc.2023.108664 ↗
56. Generalized gradient approximation made simple10.1103/PhysRevLett.77.3865 ↗
57. Geometry optimization of periodic systems using internal coordinates10.1063/1.1864932 ↗
58. Calculations of single-crystal elastic constants made simple10.1016/j.cpc.2009.11.017 ↗
59. The closest elastic tensor of arbitrary symmetry to an elasticity tensor of lower symmetry10.1007/s10659-006-9082-0 ↗
60. Computation of the yield point of mixed crystals due to hiring for single crystals
61. Average elastic constants and tensor invariants10.1002/pssa.2210990212 ↗
62. VESTA: a three-dimensional visualization system for electronic and structural analysis10.1107/S0021889808012016 ↗
63. Wasa · 2012
64. Angle-resolved evolution of the composition of Cr–Al–C thin films deposited by sputtering of a compound target10.1088/0022-3727/46/13/135501 ↗
65. 2016
66. PDF-5+: a comprehensive powder diffraction file™ for materials characterization10.1017/S0885715624000150 ↗
67. On the film density using high power impulse magnetron sputtering10.1016/j.surfcoat.2010.07.041 ↗
68. High power pulsed magnetron sputtering: a review on scientific and engineering state of the art10.1016/j.surfcoat.2009.11.013 ↗
69. Recent advances of superhard nanocomposite coatings: a review10.1016/S0257-8972(02)00903-9 ↗
70. Size and plasticity effects in zirconia micropillars compression10.1016/j.actamat.2015.10.047 ↗
71. Ductile–brittle transition in micropillar compression of GaAs at room temperature10.1080/14786435.2010.509286 ↗
72. Discussion of the dependence of the effect of size on the yield stress in hard materials studied by microcompression of MgO10.1080/14786435.2010.505179 ↗
73. Assessment of ductile character in superhard ta-C-N thin films10.1016/j.actamat.2019.08.015 ↗
74. Assessing the fracture and fatigue resistance of nanostructured thin films10.1016/j.actamat.2022.118260 ↗
75. Hardness and fracture toughness enhancement in transition metal diboride multilayer films with structural variations10.1016/j.mtla.2024.102070 ↗
76. Unraveling the superlattice effect for hexagonal transition metal diboride coatings10.1016/j.scriptamat.2023.115599 ↗
77. Effect of titanium and deposition parameters on microstructure and mechanical properties of W-Ti-B thin films deposited by high power impulse magnetron sputtering10.1016/j.surfcoat.2024.130915 ↗