journal article·2022-11

Discontinuous oxidation in wet air of T91 with a novel Al2O3-forming NiCrAl nanocomposite coating in as-deposited and pre-oxidized states

Huijuan Zhen, Yun Xie, Lixi Tian, Xiao Peng

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Catalytic Processes in Materials Science · Electrophoretic Deposition in Materials Science

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (42)

Show source-provided references
1. A review of the oxidation behaviour of structural alloys in steam10.1179/095066010X12646898728165 ↗
2. Water vapor–mediated volatilization of high-temperature materials10.1146/annurev-matsci-071312-121636 ↗
3. Enhanced oxidation of the 9%Cr steel P91 in water vapour containing environments10.1016/j.corsci.2006.02.002 ↗
4. The effect of water vapor on the oxidation behavior of 9%Cr steels in simulated combustion gases10.1007/s002160050942 ↗
5. Parameters determining the breakaway oxidation behaviour of ferritic martensitic 9%Cr steels in environments containing H2O10.1179/147842204225016921 ↗
6. Evolution of oxide film of T91 steel in water vapor atmosphere at 750 °C10.1007/s11085-013-9448-1 ↗
7. High temperature oxidation of Fe–Al and Fe–Cr–Al alloys: the role of Cr as a chemically active element10.1016/j.corsci.2010.06.019 ↗
8. Alloy design strategies for promoting protective oxide-scale formation10.1007/s11837-000-0109-x ↗
9. High temperature oxidation behavior of SIMP steel10.1007/s11085-015-9532-9 ↗
10. Influence of water vapor and flow rate on the high-temperature oxidation of 304L; effect of chromium oxide hydroxide evaporation10.1023/A:1004642310974 ↗
11. Evaporation of Cr2O3 in atmospheres containing H2O10.1023/A:1023671206976 ↗
12. Effect of grain refinement on the resistance of 304 stainless steel to breakaway oxidation in wet air10.1016/j.actamat.2005.07.019 ↗
13. Creep-resistant, Al2O3-forming austenitic stainless steels10.1126/science.1137711 ↗
14. Volatility of common protective oxides in high-temperature water vapor: current understanding and unanswered questions10.4028/www.scientific.net/MSF.461-464.765 ↗
15. The effect of water vapor on the oxidation behavior of CVD iron-aluminide coatings10.1023/B:OXID.0000038788.02094.cb ↗
16. Formation of aluminide coatings on Fe-based alloys by chemical vapor deposition10.1016/j.surfcoat.2008.01.023 ↗
17. Oxidation of uncoated and aluminized 9–12% Cr boiler steels at 550–650 °C10.1007/s11665-010-9675-4 ↗
18. Formation and oxidation performance of low-temperature pack aluminide coatings on ferritic–martensitic steels10.1016/j.surfcoat.2009.09.063 ↗
19. Comparison of the dry and wet oxidation at 900 °C of η-Fe2Al5 and δ-Ni2Al3 coatings10.1016/j.corsci.2010.10.003 ↗
20. Corrosion resistance of chromised and aluminised coatings in wet CO2 gas at 650°C10.1016/j.surfcoat.2017.03.028 ↗
21. Long exposure steam oxidation testing and mechanical properties of slurry aluminide coatings for steam turbine components10.1016/j.surfcoat.2005.07.080 ↗
22. Cyclic oxidation and mechanical behaviour of slurry aluminide coatings for steam turbine components10.1016/j.surfcoat.2006.11.033 ↗
23. A new approach to manufacture oxidation-resistant NiCrAl overlay coatings by electrodeposition10.1016/j.corsci.2019.01.039 ↗
24. Oxidation-resistant CoCrAl coatings fabricated by electrodeposition in combination with electrophoretic deposition10.1016/j.surfcoat.2018.08.036 ↗
25. A novel strategy to apply metallic nanoparticles to manufacture NiCrAl composite coatings smartly growing chromia and alumina10.1016/j.compositesb.2022.109721 ↗
26. Comparison of the oxidation of high-sulfur Ni–25Cr–5Al alloys in as-cast and as-sputtered states10.1016/j.corsci.2009.12.005 ↗
27. Piezospectroscopic analysis of interface debonding in thermal barrier coatings10.1111/j.1151-2916.2000.tb01349.x ↗
28. Reaktionstypen bei der oxydation von legierungen
29. Oxidation of Ni-Cr-Al alloys between 1000° and 1200°C10.1149/1.2407837 ↗
30. The third-element effect in the oxidation of Ni–xCr–7Al (x=0, 5, 10, 15at.%) alloys in 1atm O2 at 900–1000°C10.1016/j.corsci.2006.03.008 ↗
31. Young · 2016
32. The oxidation behaviour of metals and alloys at high temperatures in atmospheres containing water vapour: a review10.1016/j.pmatsci.2007.11.001 ↗
33. Effect of Mn on oxide formation by Fe-Cr and Fe-Cr-Ni alloys in dry and wet CO2 gases at 650 °C10.1016/j.corsci.2016.07.014 ↗
34. Growth and adherence of chromia based surface scales on Ni-base alloys in high- and low-pO2 gases10.1016/j.msea.2007.05.035 ↗
35. Transient oxidation of single-crystal β-NiAl10.1007/BF02653930 ↗
36. The oxidation behaviour of NiAl-I. Phase transformations in the alumina scale during oxidation of NiAl and NiAl-Cr alloys10.1016/0010-938X(92)90002-K ↗
37. Microstructural study of the theta-alpha transformation in alumina scales formed on nickel-aluminides10.1179/mht.2000.011 ↗
38. Transient-alumina transformations during the oxidation of magnetron-sputtered CoCrAl nanocrystalline coatings10.1023/A:1026015101783 ↗
39. The promoted formation of an α-Al2O3 scale on a nickel aluminide with surface Cr2O3 particles10.1016/j.corsci.2016.07.029 ↗
40. A new method to develop a NiRe-Al2O3 diffusion barrier between single crystal Ni-base superalloy and NiAl coating10.1016/j.matchemphys.2021.125350 ↗
41. The reactive element effect of ceria particle dispersion on alumina growth: a model based on microstructural observations10.1038/srep29593 ↗
42. Nitridation of alloys