Corrosion and tribocorrosion resistance of superhydrophobic LPBF-NiTi alloys surface fabricated by nanosecond laser and ultrasonic fluorination
Bibliographic record
Abstract
No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.
Source: Not provided · Quality: missing
Research context
OpenAlex topics: Diamond and Carbon-based Materials Research · Metal and Thin Film Mechanics · Tribology and Wear Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (53)
Show source-provided references
1. Achieving illustrious friction and corrosion resistance on a laser powder bed fusion nitinol rare earth alloy10.1016/j.mtadv.2023.100350 ↗
2. Anti-tribocorrosion resistance of NiTi–CeO2 alloys fabricated by laser powder bed fusion10.1016/j.coco.2023.101512 ↗
3. Microstructures and mechanical properties of NiTi shape memory alloys fabricated by wire arc additive manufacturing10.1016/j.jallcom.2021.162193 ↗
4. Laser powder bed fusion of defect-free NiTi shape memory alloy parts with superior tensile superelasticity10.1016/j.actamat.2022.117781 ↗
5. Achieve superior interfacial bonding force with excellent corrosion resistance on polycaprolactone coating by nanosecond laser machining of LPBF-NiTi alloy10.1016/j.matlet.2022.132774 ↗
6. Micro laser powder bed fusion of NiTi alloys with superior mechanical property and shape recovery function
7. The martensitic transformation behavior and shape memory effect of laser powder bed fusion NiTi alloys influenced by rare earth addition10.1016/j.msea.2022.143350 ↗
8. Graded functionality obtained in NiTi shape memory alloy via a repetitive laser processing strategy10.1016/j.jmatprotec.2021.117177 ↗
9. Microstructure, phase transformation behavior and tensile superelasticity of NiTi shape memory alloys fabricated by the wire-based vacuum additive manufacturing10.1016/j.msea.2021.141077 ↗
10. Laser beam powder bed fusion of nitinol shape memory alloy (SMA)10.1016/j.jmrt.2021.07.126 ↗
11. Selective laser melting of NiTi alloy with superior tensile property and shape memory effect10.1016/j.jmst.2019.05.015 ↗
12. Microhardness and microabrasion behaviour of NiTi shape memory alloy after femtosecond laser shock peening without coating in air
13. Graphene enhanced anti-corrosion and biocompatibility of NiTi alloy10.1016/j.impact.2016.10.003 ↗
14. Improving surface finish and wear resistance of additive manufactured nickel-titanium by ultrasonic nano-crystal surface modification10.1016/j.jmatprotec.2017.06.038 ↗
15. Study on corrosion behavior of the selective laser melted NiTi alloy with superior tensile property and shape memory effect10.1016/j.corsci.2020.108891 ↗
16. Effect of stress aging induced precipitates on corrosion behavior of NiTi shape memory alloys10.1007/s12540-020-00935-y ↗
17. Design and characterization of a novel Cu2.3Al1.3Ni1.7SnCr0.3 multi-principal element alloy coating on magnesium alloy by laser cladding10.1016/j.jmst.2022.11.064 ↗
18. Microstructure, corrosive-wear and electrochemical properties of laser cladded CoCrFeNiMo-B4C coatings in 3.5%NaCl solution10.1016/j.optlastec.2022.108999 ↗
19. Study of cracking mechanism and wear resistance in laser cladding coating of Ni-based alloy10.1186/s10033-021-00599-8 ↗
20. Fabrication of antibacterial Zr-BMG biomimetic surfaces by femtosecond laser10.1016/j.surfin.2023.102740 ↗
21. A review of smart superwetting surfaces based on shape-memory micro/nanostructures10.1002/smll.202206463 ↗
22. Effect of picosecond laser cleaning on surface morphology and properties of stainless steel10.1016/j.optlastec.2022.109041 ↗
23. Fabrication of antireflection surfaces with superhydrophobic property for titanium alloy by nanosecond laser irradiation10.1016/j.optlastec.2020.106129 ↗
24. Nanosecond laser fabrication of superhydrophobic Ti6Al4V surfaces assisted with different liquids10.1016/j.colcom.2020.100256 ↗
25. Hybrid laser ablation and chemical modification for fast fabrication of bio-inspired super-hydrophobic surface with excellent self-cleaning, stability and corrosion resistance10.1007/s42235-019-0002-y ↗
26. Facile preparation of robust superhydrophobic ceramic surfaces with mechanical stability, durability, and self-cleaning function10.1016/j.apsusc.2021.151875 ↗
27. Research on the influence of micro-morphology on the hydrophobicity of material surface10.1016/j.colcom.2021.100556 ↗
28. Anti-corrosion superhydrophobic surfaces of Al alloy based on micro-protrusion array structure fabricated by laser direct writing10.1016/j.jallcom.2021.160649 ↗
29. Anti-icing performance of superhydrophobic surface fabricated by femtosecond laser composited dual-layers coating10.1016/j.enbuild.2020.110175 ↗
30. Superhydrophobic brass surfaces with tunable water adhesion fabricated by laser texturing followed by heat treatment and their anti-corrosion ability10.1016/j.apsusc.2021.151596 ↗
31. Improvement of corrosion resistance of H59 brass through fabricating superhydrophobic surface using laser ablation and heating treatment10.1016/j.corsci.2020.109186 ↗
32. Bionic design of tools in cutting: reducing adhesion, abrasion or friction
33. Heat treatment temperature effect on wettability of laser-machined aluminum surface10.1007/s11665-021-06202-4 ↗
34. Investigation on anisotropic tribological properties of superhydrophobic/superlipophilic lead bronze surface textured by femtosecond laser10.1016/j.apsusc.2021.152223 ↗
35. Icing delay of sessile water droplets on superhydrophobic titanium alloy surfaces10.1016/j.colsurfa.2021.126587 ↗
36. Superhydrophobic TC4 alloy surface fabricated by laser micro-scanning to reduce adhesion and drag resistance10.1016/j.surfcoat.2020.125707 ↗
37. Laser-chemical treated superhydrophobic surface as a barrier to marine atmospheric corrosion10.1016/j.surfcoat.2020.126255 ↗
38. An extremely efficiency method to achieve stable superhydrophobicity on the surface of additive manufactured NiTi alloys: “ultrasonic fluorination”10.1016/j.apsusc.2022.155947 ↗
39. Multi-scale pseudoelasticity of NiTi alloys fabricated by laser additive manufacturing10.1016/j.msea.2021.141600 ↗
40. Effect of Ni content on the transformation behavior and mechanical property of NiTi shape memory alloys fabricated by laser powder bed fusion10.1016/j.optlastec.2020.106653 ↗
41. Laser-induced wettability gradient surface on NiTi alloy for improved hemocompatibility and flow resistance10.1016/j.msec.2020.110847 ↗
42. Switchable wettability control of titanium via facile nanosecond laser-based surface texturing10.1016/j.surfin.2021.101122 ↗
43. Fabrication of microholes array on titanium foil by a femtosecond laser and a surface’s wettability switching10.3788/COL202119.082201 ↗
44. Spontaneous dewetting transitions of droplets during icing & melting cycle10.1038/s41467-022-28036-x ↗
45. Electrochemical behavior and microstructural characterization of lanthanum-doped titanium-zirconium-molybdenum alloy10.1016/j.jallcom.2018.05.338 ↗
46. Corrosion resistance and biocompatibility of graphene oxide coating on the surface of the additively manufactured NiTi alloy
47. The corrosion resistance, biocompatibility and biomineralization of the dicalcium phosphate dihydrate coating on the surface of the additively manufactured NiTi alloy10.1016/j.jmrt.2022.01.063 ↗
48. Microstructures and properties of laser cladding Al-TiC-CeO2 composite coatings10.3390/ma11020198 ↗
49. Graphene oxide/hydroxyapatite composite coatings on additively manufactured NiTi alloy for biomedical applications10.1016/j.ceramint.2023.11.041 ↗
50. Antibacterial activity of additive manufactured NiTi alloy improved by zinc oxide-doped DCPD-PCL composite coating10.1016/j.ceramint.2023.10.174 ↗
51. Effect of compressive stress on cavitation erosion-corrosion behavior of nickel-aluminum bronze alloy10.1016/j.ultsonch.2022.106143 ↗
52. Influence of ultrasonic combined supercritical-CO(2) electrodeposition process on copper film fabrication: electrochemical evaluation10.1016/j.ultsonch.2021.105555 ↗
53. Ultrasonic assisted rapid preparation of superhydrophobic stainless steel surface and its application in oil/water separation10.1016/j.ultsonch.2021.105848 ↗