Influence of bondcoat pre-treatment and surface topology on the lifetime of EB-PVD TBCs
Source abstract
Abstract
Abstract In the present study two types of bondcoats (BC) were used, a NiCoCrAlY overlay coating produced by electron beam physical vapor deposition (EB-PVD) and a platinum aluminide diffusion coating (Ni,Pt)–Al. The coatings were deposited onto nickel-base IN100 and Rene142 substrates and were pre-treated in vacuum or Ar–H gas mixture prior to the deposition of an EB-PVD yttria partially stabilized zirconia top coat. The specimens were thermal cyclically tested in air at 1100 °C (50 min at 1100 °C/10 min forced air cooling). The microstructures of the thermally grown oxide (TGO) layers prior and after testing were examined by scanning electron microscopy and electron energy dispersive spectroscopy. Heat-treatment in Ar–H significantly improved the lifetime of the thermal barrier coatings (TBC) system with IN100+PtAl BC, whereas reduced lifetimes were found on IN100+NiCoCrAlY BC and Rene142+PtAl. High Y-contents of the NiCoCrAlY BC significantly reduced TBC lifetimes. Furthermore, the results for IN100+PtAl and Rene142+PtAl demonstrated that early TBC failure was associated with high TGO surface roughness of the metal/oxide interface, indicating that surface roughness has a significant effect on TBC system performance.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Semiconductor materials and devices · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (17)
Show source-provided references
1. Nelson · J. Therm. Spray Technol. · 1997 · 6 · 18710.1007/s11666-997-0009-5 ↗
2. Rigney · J. Therm. Spray Technol. · 1997 · 6 · 16710.1007/s11666-997-0008-6 ↗
3. Maricocchi · J. Therm. Spray Technol. · 1997 · 6 · 19310.1007/s11666-997-0012-x ↗
4. Leyens · Zeitschrift für Metallkunde · 2001 · 92 · 762
5. Schulz · Surf. Coat. Technol. · 2001 · 146–147 · 11710.1016/S0257-8972(01)01481-5 ↗
6. Warnes · Surf. Coat. Technol. · 1997 · 1 · 94
7. Wright · Mater. Sci. Eng. A · 1998 · 245 · 19110.1016/S0921-5093(97)00850-2 ↗
8. Leushake · Surf. Coat. Technol. · 1997 · 94–95 · 13110.1016/S0257-8972(97)00490-8 ↗
9. Pint · Mater. Sci. Eng. A · 1998 · 245 · 20110.1016/S0921-5093(97)00851-4 ↗
10. EB-PVD TBC lifetime response to various BC pre-treatments
11. H. Lau, C. Leyens, U. Schulz, C. Friedrich, Effects of TGO surface topology and bondcoat annealing on TBC performance, International Symposium on Advanced Thermal Barrier Coatings and Titanium Aluminides for Gas Turbines TURBOMAT 2002—Proceedings, session TBC II, published by German Aerospace Center (DLR), 2002, pp. 193–196
12. Vaidyanathan · Surf. Coat. Technol. · 2000 · 133–134 · 2810.1016/S0257-8972(00)00891-4 ↗
13. H. Lau, C. Leyens, U. Kaden, et al., Influence of bondcoat pre-treatment on the thermal cyclic lifetime of EBPVD TBCs, Materials Week 2001—Proceedings, session K3: Advanced Ceramic Materials-Coatings Ed. Werkstoffwoche-Partnerschaft GbR, published by Werkstoff-Informationsgesellschaft mbH, Frankfurt, 2002, pp. 1–8
14. Schilbe · Surf. Coat. Technol. · 2000 · 133–134 · 3510.1016/S0257-8972(00)00870-7 ↗
15. Mumm · Acta Materialia · 2001 · 49 · 232910.1016/S1359-6454(01)00071-4 ↗
16. Evans · Prog. Mater. Sci. · 2001 · 46 · 50510.1016/S0079-6425(00)00020-7 ↗
17. Kofstad · 1983 · 153–165 and 343–348