Effect of dew point on the reactive wetting of a C-2Mn-1.3Si (wt%) advanced high strength steel during continuous galvanizing
Source abstract
Abstract
Abstract The effect of oxygen partial pressure on the reactive wetting of a Fe-0.1C-2Mn-1.3Si (wt%) advanced high strength steel during continuous galvanizing was determined. The steel was intercritically annealed at 1093 K (820 °C) for 120 s in a N2–5 vol% H2 process atmosphere, where the oxygen potential was controlled by varying the process atmosphere dew points at 223 K (−50 °C), 243 K (−30 °C) and 278 K (+5 °C). All samples were immersed in a 0.2 wt% dissolved Al continuous galvanizing bath at 733 K (460 °C) for 4 s. For the 243 K (−30 °C) and 278 K (+5 °C) dew point atmospheres, a well-developed Fe-Al intermetallic layer, indicative of good reactive wetting, was observed due to the presence of either thin or plate/nodule-like oxides on the steel surface after annealing. This external oxide morphology facilitated contact between the Zn-alloy bath and the substrate via a variety of mechanisms, including interfacial infiltration through cracks due to thermal coefficient of expansion mismatch between the external oxide and substrate and aluminothermic reduction, which resulted in Fe dissolution from the substrate and consequent formation of the observed Fe-Al intermetallics. On the other hand, the poor reactive wetting observed for the samples annealed under the 223 K (−50 °C) dew point atmosphere was due to the formation of a thick, compact oxide layer on the steel surface, which provided an effective barrier between the substrate and Zn bath, preventing contact between the two phases and the required Fe dissolution from the substrate surface.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · High-Temperature Coating Behaviors · Metallurgical Processes and Thermodynamics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (48)
Show source-provided references
1. Tamarelli · 2011
2. A review on recent approaches in the field of hot dip zinc galvanizing process10.1016/j.surfcoat.2014.12.054 ↗
3. Diffusive phase transformation in hot dip galvanizing10.4028/www.scientific.net/MSF.155-156.527 ↗
4. The change of steel surface chemistry regarding oxygen partial pressure and dew point10.1016/j.apsusc.2012.12.103 ↗
5. Selective oxidation and reactive wetting during hot-dip galvanizing of a 1.0 pct Al-0.5 pct Si TRIP-assisted steel10.1007/s11661-011-0983-6 ↗
6. Effect of continuous galvanizing heat treatments on the microstructure and mechanical properties of high Al-low Si transformation induced plasticity steels10.1007/s11661-010-0185-7 ↗
7. Relation between microstructure and adhesion of hot dip galvanized zinc coatings on dual phase steel10.1016/j.actamat.2012.02.003 ↗
8. Influence of gas atmosphere dew point on the selective oxidation and the reactive wetting during hot dip galvanizing of CMnSi TRIP steel10.1007/s11661-012-1392-1 ↗
9. Selective oxidation and reactive wetting during galvanizing of a CMnAl TRIP-assisted steel10.1007/s11661-011-0685-0 ↗
10. Reactive wetting during hot-dip galvanzing of high manganese alloyed steel10.1016/j.surfcoat.2010.11.053 ↗
11. Galvanizability of high-strength steels for automotive applications10.1007/s11661-001-1042-5 ↗
12. Galvanisability of silicon free CMnAl TRIP steels10.1179/026708303225009300 ↗
13. Galvanizability of advanced high-strength steels 1180TRIP and 1180CP10.1007/s11661-009-9880-7 ↗
14. Thermodynamic analysis of selective oxidation behavior of Si and Mn-added steel during recrystallization annealing10.2355/isijinternational.49.564 ↗
15. Effect of Si content on wettability of dual phase high strength steels by liquid Zn-0.23 wt.% Al10.1007/s12540-011-0812-x ↗
16. Selective oxidation and reactive wetting of 1.0 Pct Si-0.5 Pct Al and 1.5 Pct Si TRIP-assisted steels10.1007/s11661-010-0192-8 ↗
17. Effect of annealing atmosphere on the galvanizing behavior of a dual-phase steel10.1016/j.msea.2006.09.116 ↗
18. On the in-situ aluminothermic reduction of manganese oxides in continuous galvanizing baths10.1016/j.surfcoat.2012.09.038 ↗
19. Development of Continuous Galvanization-compatible Martensitic Steel
20. Application of thermodynamics and Wagner model on two problems in continuous hot-dip galvanizing10.1016/j.apsusc.2009.08.095 ↗
21. Selective oxidation and reactive wetting during galvanizing of a CMnAl TRIP-assisted steel10.1007/s11661-011-0685-0 ↗
22. Fe solubility in the Zn-rich corner of the Zn-Al-Fe system for use in continuous galvanizing and galvannealing10.1007/s11663-007-9028-3 ↗
23. Reactive wetting of high Mn steels during continuous hot-dip galvanizing10.1016/j.actamat.2011.02.027 ↗
24. The role of surface oxides on annealed high-strength steels in hot-dip galvanizing10.1016/j.corsci.2013.01.039 ↗
25. Bellhouse · 2010
26. Selective oxidation of a C-2Mn-1.3Si (wt pct) advanced high strength steel during continuous galvanizing heat treatments10.1007/s11661-018-4854-2 ↗
27. ASTM A 653/A 653M – 05 · 2005
28. Effect of Annealing Parameters on Selective Oxidation and Reactive Wetting of CMnSi Advanced High Strength Steel
29. XPS and EELS characterization of Mn2SiO4, MnSiO3 and MnAl2O410.1016/j.apsusc.2016.03.235 ↗
30. Oxidation states of Mn and Fe in various compound oxide systems10.1016/j.micron.2005.12.004 ↗
31. High resolution electron energy loss spectroscopy of manganese oxides: application to Mn3O4 nanoparticles10.1016/j.matchar.2010.09.001 ↗
32. Ahnn · 1983
33. Brundle · 1992
34. On the transition of internal to external selective oxidation on CMnSi TRIP steel10.1007/s11661-014-2442-7 ↗
35. Effect of dew point on the surface selective oxidation and subsurface microstructure of TRIP-aided steel10.1016/j.surfcoat.2011.08.038 ↗
36. Reaktionstypen bei der oxydation von legierungen
37. Birks · 2006
38. Simmons · 1971
39. Wanke · 1973 · 25 · 252
40. Callister · 2007
41. Effect of Bath Al on Interfacial Layer Formation for Continuous Galvanized Mn-containing Steels
42. Oikawa · 1983 · 48 · 7
43. Thermodata
44. Numerical simulation of internal oxidation of steels during annealing treatments10.1007/s11085-005-5718-x ↗
45. Critical evaluation and optimization of the thermodynamic properties and phase diagrams of the MnO-SiO2 and CaO-SiO2 systems10.1179/cmq.1994.33.1.13 ↗
46. Numerical implementation and application of an extended model for diffusion and precipitation of chemical elements in metallic matrices10.1007/s11085-010-9193-7 ↗
47. Kinetics of internal oxidation of Mn-steel alloys10.1007/s11085-014-9490-7 ↗
48. Implementation and application of some nonlinear models of diffusion/reaction in solids10.1016/j.finel.2017.04.004 ↗