Abstract
Abstract Smooth copper coatings containing well-distributed silicon nitride particles were obtained by co-electrodeposition in acidic sulfate bath. The cathodic current density did not show significant influence on incorporated particle volume fraction, whereas the increase of particle concentration in the bath led to its decrease. The increase of stirring rate increased the amount of embedded particles. The microhardness of the composite layers was higher than that of pure copper deposits obtained under the same conditions due to dispersion-strengthening and copper matrix grain refinement and increased with the increase of incorporated particle volume fraction. The microhardness of composites also increased with the increase of current density due to copper matrix grain refining. The composite coatings presented higher strength but lower ductility than pure copper layers. Pure copper and composite coatings showed the same corrosion resistance in 0.5 wt.% H2SO4 solution at room temperature.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electrodeposition and Electroless Coatings · Corrosion Behavior and Inhibition · Copper Interconnects and Reliability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (33)
Show source-provided references
1. Hovestad · J. Appl. Electrochem. · 1995 · 25 · 51910.1007/BF00573209 ↗
2. Musiani · Electrochim. Acta · 2000 · 45 · 339710.1016/S0013-4686(00)00438-2 ↗
3. Celis · J. Electrochem. Soc. · 1977 · 124 · 150810.1149/1.2133102 ↗
4. Buelens · J. Appl. Electrochem. · 1983 · 13 · 54110.1007/BF00617528 ↗
5. Hayashi · J. Electrochem. Soc. · 1993 · 140 · 36210.1149/1.2221051 ↗
6. Stankovic · Surf. Coat. Technol. · 1996 · 81 · 22510.1016/0257-8972(95)02486-7 ↗
7. Wang · Surf. Coat. Technol. · 1998 · 106 · 16210.1016/S0257-8972(98)00522-2 ↗
8. Gan · J. Mater. Sci. · 2007 · 42 · 525610.1007/s10853-006-0369-0 ↗
9. Abdullin · Prot. Met. · 1997 · 33 · 196
10. Medeliene · Pol. J. Chem. · 2004 · 78 · 1305
11. Benea · Mater. Corros. · 2000 · 51 · 49110.1002/1521-4176(200007)51:7<491::AID-MACO491>3.0.CO;2-C ↗
12. Mangam · Mater. Chem. Phys. · 2010 · 120 · 63110.1016/j.matchemphys.2009.12.017 ↗
13. Medeliene · Surf. Coat. Technol. · 2006 · 200 · 612310.1016/j.surfcoat.2005.09.036 ↗
14. Jin · Key Eng. Mater. · 2005 · 291–292 · 53710.4028/www.scientific.net/KEM.291-292.537 ↗
15. Guo · J. Mater. Sci. Technol. · 2006 · 22 · 51410.1179/174328406X100680 ↗
16. Tang · J. Appl. Polym. Sci. · 1998 · 69 · 115910.1002/(SICI)1097-4628(19980808)69:6<1159::AID-APP13>3.0.CO;2-O ↗
17. Zhu · Mater. Lett. · 2004 · 58 · 163410.1016/j.matlet.2003.08.040 ↗
18. Thiemig · Electrochim. Acta · 2007 · 52 · 736210.1016/j.electacta.2007.06.009 ↗
19. Medeliene · Mater. Sci. · 2008 · 14 · 29
20. Heisterkamp · 2003
21. H.R.Z. Sandim, Preparation of Nb-TiO2 alloys by powder metallurgy and its microstructural characterization, PhD Thesis, University of São Paulo, 1996.
22. 1978
23. Montgomery · 2005
24. Ross · 1996
25. Berçot · Surf. Coat. Technol. · 2002 · 157 · 28210.1016/S0257-8972(02)00180-9 ↗
26. Willson · J. Tech. Proc. Amer. Electroplaters. Soc. · 1964 · 51 · 92
27. Robin · J. Appl. Electrochem. · 2010 · 40 · 50710.1007/s10800-009-0022-0 ↗
28. Safranek · 1974
29. Garcia · Surf. Coat. Technol. · 2001 · 148 · 17110.1016/S0257-8972(01)01336-6 ↗
30. Ma · Corros. Sci. · 2003 · 45 · 86710.1016/S0010-938X(02)00175-0 ↗
31. Quartarone · Corros. Sci. · 2003 · 45 · 71510.1016/S0010-938X(02)00134-8 ↗
32. 1992 · Vol. 13
33. Dini · 1993