Micro-abrasive wear mechanisms of P/M AISI M2 steel with different surface treatments
Source abstract
Abstract
Abstract Boriding, heat treatment (quenching and tempering) and PVD (Physical Vapor Deposition) film deposition were applied to P/M (Powder Metallurgy) AISI M2 steel. Four sample conditions were produced: Quenched and tempered AISI M2 (QT), Borided AISI M2 (B), Quenched and tempered AISI M2 + Film (QTF) and Borided AISI M2 + Film (BF). The samples were characterized by X-ray diffraction (XRD), scanning electron microscopy (SEM) and the Vickers microhardness test. The load applied in the micro-abrasion tests (fixed-ball) was 0.49 N and abrasive slurry concentration was 0.1 g/cm3. Silicon dioxide (SiO2) abrasive powders (approximately 80% of particles between 1 and 5 μm) were used in the abrasion experiments. Wear coefficient and mechanisms of all conditions were compared. The XRD analysis revealed the presence of a biphasic layer of borides (FeB and Fe2B phases) on the borided samples. The film thickness was 2.1 ± 0.4 μm and the hardness of the multilayered AlTiN/CrN film was about 3912 HV0.025. The borided layer thickness was 46.5 ± 5.1 μm and the hardness average of 2162 HV0.025. The wear mechanism for the QT and QTF samples was two-body abrasion (grooving abrasion). There was a reduction on the signs of grooving abrasion for the B and BF samples due to the increase in plastic deformation resistance.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Metal Alloys Wear and Properties · Diamond and Carbon-based Materials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. Effect of pressure on abrasive wear mode transitions in micro-abrasive wear tests of WC-Co P2010.1016/j.triboint.2012.06.028 ↗
2. Micro-abrasive wear of PVD duplex and single-layered coatings10.1016/S0257-8972(01)01189-6 ↗
3. Effect of surface topography on the dynamics of the abrasive particles during micro-abrasion10.1016/j.wear.2014.12.011 ↗
4. Three-body abrasive wear testing of soft materials10.1016/S0043-1648(99)00183-0 ↗
5. Analysis of perforating and non-perforating micro-scale abrasion tests on coated substrates10.1016/j.surfcoat.2005.01.015 ↗
6. Methods of data analysis for the micro-scale abrasion test on coated substrates10.1016/j.surfcoat.2003.10.010 ↗
7. Transitions between two-body and three-body abrasive wear: influence of test conditions in the microscale abrasive wear test10.1016/S0043-1648(98)00358-5 ↗
8. Influence of heat treatments on the micro-abrasion wear resistance of a super-duplex stainless steel10.1016/j.wear.2010.12.087 ↗
9. Wear-mode mapping for the micro-scale abrasion test10.1016/S0043-1648(03)00073-5 ↗
10. Impact wear and abrasion resistance of CrN, AlCrN and AlTiN PVD coatings10.1016/j.surfcoat.2012.08.077 ↗
11. Micro-abrasion of filled and unfilled polyamide 11 coatings10.1016/j.wear.2004.08.008 ↗
12. The effect of steel substrate pre-hardening on structural, mechanical, and tribological properties of magnetron sputtered TiN and TiAlN coatings10.1016/j.wear.2016.02.007 ↗
13. The effects of conventional heat treatment and boronizing on abrasive wear and corrosion of SAE 1010, SAE 1040, D2 and 304 steels10.1016/S0301-679X(02)00069-5 ↗
14. Abrasive wear resistance of boronized carbon and low-alloy steels10.1016/j.jmatprotec.2005.12.006 ↗
15. Abrasive wear behavior of boronized AISI 8620 steel10.1016/j.wear.2009.03.006 ↗
16. Research on wear characteristics of AISI 1035 steel boronized at various parameters10.1108/00368791111116366 ↗
17. Micro-abrasive wear mechanisms of borided AISI 1020 steel10.1016/j.triboint.2017.03.017 ↗
18. Investigation of borided layers contribution on the wear resistance and adhesion of TiN coatings
19. Mechanical properties of boronized AISI W4 steel10.1016/S0257-8972(01)01409-8 ↗
20. Mechanism of thermochemical growth of iron borides on iron10.1023/B:JMSC.0000012924.74578.87 ↗
21. Study of microcracks morphology produced by Vickers indentation on AISI 1045 borided steels10.1016/j.msea.2007.04.052 ↗
22. Tribological behaviour of borided H13 steel with different boriding agents10.1179/1743294414Y.0000000423 ↗
23. Effects of boronizing process on the surface roughness and dimensions of AISI 1020, AISI 1040 and AISI 271410.1016/j.jmatprotec.2008.04.040 ↗
24. Effect of laser surface modification on the micro-abrasive wear resistance of coated cemented carbide tools10.1016/j.wear.2013.01.035 ↗
25. Friction coefficient and abrasive wear modes in ball-cratering tests conducted at constant normal force and constant pressure-preliminary results10.1016/j.wear.2009.01.055 ↗
26. Relationship between tes severity and wear mode transition in micro-abrasive wear tests10.1016/j.wear.2007.01.099 ↗