Oxidation resistance of Pt-modified γ/γ′ Ni-Al at 1150°C
Source abstract
Abstract
Nickel aluminide coatings are used to protect the surfaces of turbine engine hot-stage components. Increasing service temperatures are driving the need for improved performance coatings, which grow and retain thin, protective alumina scales. This paper describes the oxidation resistance of platinum-modified, two-phase (γ/γ') Ni-22Al materials at 1150 °C in air. Under isothermal conditions, a composition of Ni-22Al-30Pt (at.%) oxidises with the same parabolic rate constant as β-NiAl. The addition of hafnium reduces the rate by an order of magnitude. The protective oxide formed is in all cases α-Al 2 O 3 . Focused ion beam (FIB) milling was used to examine the very thin scales. In 100 h of reaction, a hafnium-free Ni-Al-Pt material grew a roughly uniform scale 4-5 μm thick, decorated with numerous oxide whiskers. At the same time, a coating containing 0.5 at.% Hf grew a very thin (<0.5 μm) oxide over which developed a network of ridges about 1 μm high. The effects of hafnium are discussed in terms of oxide transport properties. Possible explanations for the beneficial effects of platinum are also considered.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Catalytic Processes in Materials Science · Intermetallics and Advanced Alloy Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (17)
Show source-provided references
1. Bouhanek · Mater. Sci. Forum · 2001 · 369–372 · 61510.4028/www.scientific.net/MSF.369-372.615 ↗
2. Gleeson · Mater. Sci. Forum · 2004 · 461–464 · 21310.4028/www.scientific.net/MSF.461-464.213 ↗
3. Zhang · Surf. Coat. Technol. · 2005 · 200 · 125910.1016/j.surfcoat.2005.07.086 ↗
4. Izumi · Mater. Sci. Forum · 2006 · 522–523 · 22110.4028/www.scientific.net/MSF.522-523.221 ↗
5. Hayashi · Mater. Sci. Forum · 2006 · 522–523 · 22910.4028/www.scientific.net/MSF.522-523.229 ↗
6. Pint · Surf. Coat. Technol. · 2006 · 201 · 385210.1016/j.surfcoat.2006.07.244 ↗
7. Hayashi · Acta Mater. · 2005 · 53 · 331910.1016/j.actamat.2005.03.046 ↗
8. Kartono · Scr. Mater. · 2007 · 57 · 64710.1016/j.scriptamat.2007.06.018 ↗
9. Kartono · Mater. Corros. · 2008 · 59 · 45510.1002/maco.200804127 ↗
10. Hayashi · Oxid. Met. · 2009 · 71 · 510.1007/s11085-008-9125-y ↗
11. Pettit · Trans. AIME · 1967 · 239 · 1296
12. Copland · 2005
13. Kartono · 2005 · 43
14. Stringer · Mater. Sci. Eng. · 1989 · A120 · 12910.1016/0921-5093(89)90730-2 ↗
15. Prescott · Oxid. Met. · 1992 · 38 · 23310.1007/BF00666913 ↗
16. Pint · 2003 · 9
17. Haynes · Oxid. Met. · 2002 · 58 · 51310.1023/A:1020525123056 ↗