Abstract

Abstract In the present study, a-Si/μc-Al/a-Si/SiO 2 /glass specimens were prepared with various combinations of thicknesses of the μc-Al layer and the two a-Si layers. The effects of μc-Al film thickness, a-Si film thickness, the thickness ratio of Al film to Si films, and the annealing temperature on the metal-induced Si crystallization and void defects formed in the sandwich composite specimens were investigated. A transmission electron microscope (TEM) and an X-ray photoelectron spectroscope (XPS) were used to investigate the diffusion mechanism and efficiency of Si crystallization. When the annealing temperature was sufficiently high, the μc-Al grains diffused into the two adjacent Si layers with a fairly even distribution over the entire sandwich structure. Si crystallization was thus significantly enhanced by the sandwich structure. The Hall carrier mobility of the specimen with a structure of a-Si(500 nm)/μc-Al(50 nm)/a-Si(500 nm) was 80.1 cm 2 /Vs and the Al carrier concentration was 1.5 × 10 18 /cm 3 at an annealing temperature of 600 °C; no voids were found in the sandwich structure. An increase in the top layer (a-Si) thickness is advantageous for Si crystallization; however, an increase in the third layer (a-Si) thickness degrades Si crystallization. For a given Al film thickness, an excessive increase in the thicknesses of the two a-Si layers degrades Si crystallization even at high annealing temperatures. A thick Al film in combination with two thick a-Si layers leads to a high Hall carrier mobility when the annealing temperature is sufficiently high. An increase in the Si/Al thickness ratio increases the Hall carrier mobility and decreases the Al carrier concentration.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Thin-Film Transistor Technologies · Silicon and Solar Cell Technologies · Silicon Nanostructures and Photoluminescence

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (35)

Show source-provided references
1. Bergmann · Sol. Energy Mater. Sol. Cells · 1997 · 46 · 14710.1016/S0927-0248(97)00006-8 ↗
2. Ishikawa · Jpn. J. Appl. Phys. · 1998 · 37 · 73110.1143/JJAP.37.731 ↗
3. Iverson · Mater. Lett. · 1987 · 5 · 39310.1016/0167-577X(87)90047-4 ↗
4. Nast · Appl. Phys. Lett. · 1998 · 73 · 321410.1063/1.122722 ↗
5. Herd · J. Non-Cryst. Solids · 1972 · 7 · 30910.1016/0022-3093(72)90267-0 ↗
6. Quli · Mater. Sci. Eng. B-Solid State Mater. Adv. Technol. · 1999 · B67 · 13910.1016/S0921-5107(99)00172-5 ↗
7. Al-Dhafiri · Thin Solid Films · 2002 · 422 · 1410.1016/S0040-6090(02)00993-8 ↗
8. Cheng · 2001 · 278 · 838
9. Leung · 2001 · 203 · 388
10. Schneider · J. Non-Cryst. Solids · 2004 · 338–340 · 12710.1016/j.jnoncrysol.2004.02.036 ↗
11. Nast · J. Appl. Phys. · 2000 · 88 · 71610.1063/1.373727 ↗
12. Zhao · Appl. Phys. A Mater. Sci. Process · 2004 · A79 · 68110.1007/s00339-003-2247-9 ↗
13. Kurosawa · Appl. Phys. Lett. · 2009 · 95 · 132103-110.1063/1.3241076 ↗
14. Kurosawa · Jpn. J. Appl. Phys. · 2009 · 48 · 03B002-110.1143/JJAP.48.03B002 ↗
15. Wang · Appl. Phys. Lett. · 2006 · 88 · 061910-1
16. Hsu · Jpn. J. Appl. Phys. · 2003 · 42 · 492810.1143/JJAP.42.4928 ↗
17. Sasajima · J. Appl. Phys. · 2009 · 7 · 073501-1
18. Sullivan · Proc. SPIE · 1991 · 1596 · 8310.1117/12.51014 ↗
19. Hashemi · 2005 · 326
20. Yang · J. Appl. Phys. · 2010 · 107 · 103516-1
21. Gupta · Thin Solid Films · 2008 · 516 · 85010.1016/j.tsf.2007.06.202 ↗
22. Nair · Surf. Coat. Technol. · 2008 · 203 · 67510.1016/j.surfcoat.2008.07.014 ↗
23. Zou · Mater. Lett. · 2006 · 60 · 137910.1016/j.matlet.2005.11.037 ↗
24. Cai · Electrochem. Solid State Lett. · 2005 · 8 · G17910.1149/1.1928232 ↗
25. Pereira · Thin Solid Films · 2004 · 451 · 33410.1016/j.tsf.2003.10.124 ↗
26. Peng · Thin Solid Films · 2010 · 518 · 696610.1016/j.tsf.2010.07.038 ↗
27. Nast · J. Appl. Phys. · 2000 · 88 · 12410.1063/1.373632 ↗
28. Han · Appl. Phys. A · 2008 · A91 · 52910.1007/s00339-008-4443-0 ↗
29. Gioti · Appl. Phys. Lett. · 1998 · 73 · 18410.1063/1.121749 ↗
30. Logothetidis · Vacuum · 2000 · 53 · 61
31. Sheeja · Surf. Coat. Technol. · 2000 · 132 · 22810.1016/S0257-8972(00)00848-3 ↗
32. Zhang · Appl. Surf. Sci. · 2007 · 253 · 883510.1016/j.apsusc.2007.04.039 ↗
33. Dutta · Nano Struct. Mater. · 1995 · 6 · 84310.1016/0965-9773(95)00191-3 ↗
34. Aoki · Carbon · 2001 · 39 · 147710.1016/S0008-6223(00)00276-1 ↗
35. Nast · IEEE Trans. Electron. Devices · 1999 · 46 · 206210.1109/16.791997 ↗