Degradation characteristics of thermal barrier coatings for hot corrosion and CaO–MgO–Al2O3–SiO2
Source abstract
Abstract
Abstract Hot corrosion and CaO–MgO–Al2O3–SiO2 (CMAS) resistance of thermal barrier coatings (TBCs) are required in an industrial gas turbine employed with impure fuels and high turbine inlet temperatures. Therefore, various TBC systems with different structural combinations were investigated in thermochemical aspects of hot corrosion and CMAS causing the degradation of TBCs. Four types of 8 wt% yttria-stabilized zirconia (8YSZ), namely dense microstructure (8YSZ), porous microstructure (C–8YSZ), no monoclinic phase (NoM–8YSZ), and low thermal conductivity (low-k), were employed to prepare topcoats using an atmospheric plasma spray on the two bondcoats coated by a vacuum plasma spray with feedstocks of NiCoCrAlY and NiCoCrAlY+Hf + Si. Hot corrosion components penetrated through the whole topcoat layer at 1000 °C however did not infiltrate to the bondcoat layers because of the thermally grown oxide layer formed between the topcoat and the bondcoat. In addition, the elements Hf and Si contained in the bondcoat composition suppressed diffusion of β phase aluminum. In the visual inspection after the hot corrosion at 1000 °C and CMAS test at 1250 °C, the TBC system with the NoM–YSZ topcoat layer showed a sound condition without failure unlike other TBCs, and no monoclinic phase after hot corrosion and the CMAS test, indicating that the phase stability plays a critical role in TBCs' lifetime in the hot corrosion and CMAS environments.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Nuclear Materials and Properties · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (50)
Show source-provided references
1. U.S. Energy Information Administration. Table ES1.B. Total electric power industry summary statistics, year-to-date 2020 and 2019. https://www.eia.gov/electricity/monthly/epm_table_grapher.php?t=epmt_es1b, 2019 (accessed February 27, 2019).
2. Enhancing power output and profitability through energy-efficiency techniques and advanced materials in today’s industrial gas turbines10.1186/s40712-014-0002-y ↗
3. Integrated gasification combined cycle—a review of IGCC technology10.1080/00908319608908789 ↗
4. Efficient use of energy by utilizing gas turbine combined systems, Appl10.1016/S1359-4311(00)00033-8 ↗
5. Assessment of integrated gasification combined cycle technology competitiveness10.1016/j.rser.2007.06.010 ↗
6. IGCC update: are we there yet ?
7. S. Can Gulen, Gas Turbine for Electric Power Generation, Cambridge University Press, Cambridge, 2019, 75–118.
8. Thermodynamic assessment of the ZrO2–YO1.5 system10.1111/j.1151-2916.1991.tb07142.x ↗
9. Cooling rate effects on the tetragonal to monoclinic phase transformation in aged plasma-sprayed yttria partially stabilized zirconia, surf10.1016/0257-8972(91)90171-R ↗
10. Phase and microstructural stability of solution precursor plasma sprayed thermal barrier coatings10.1016/j.msea.2004.04.042 ↗
11. Mechanisms-based scaling laws for the durability of thermal barrier coatings, Prog
12. Effects of phase constituents/microstructure of thermally grown oxide on the failure of EB-PVD thermal barrier coating with NiCoCrAlY bond coat, Surf10.1016/j.surfcoat.2005.08.140 ↗
13. A microstructural observation of near-failure thermal barrier coating: a study by photostimulated luminescence spectroscopy and transmission electron microscopy10.1016/j.tsf.2004.02.046 ↗
14. A study of the microstructure and oxidation behavior of alumina/yttria-stabilized zirconia (Al2O3/YSZ) thermal barrier coatings
15. Effects of hydrogen annealing, sulfur segregation and diffusion on the cyclic oxidation resistance of superalloys: a review10.1016/0040-6090(94)90335-2 ↗
16. High pressure turbine deposition in land-based gas turbines with various synfuels10.1115/1.2181181 ↗
17. J.M. Crosby, S. Lewis, J.P. Bons, W.G. Ali, T.H. Fletcher, Effects of temperature and particle size on deposition in land-based turbines, J. Eng. Gas Turbines Power, 2008, 130(5), 051503(1–9).10.1115/1.2903901 ↗
18. Novel thermal barrier coatings that are resistant to high-temperature attack by glassy deposits10.1016/j.actamat.2007.08.028 ↗
19. The mechanics of coating delamination in thermal gradients, surf10.1016/j.surfcoat.2007.03.029 ↗
20. Degradation of thermal barrier coatings by fuel impurities and CMAS: thermochemical interactions and mitigation approaches10.1007/s11666-009-9424-0 ↗
21. CMAS corrosion of EBPVD TBCs: identifying the minimum level to initiate damage10.1016/j.ijrmhm.2009.07.005 ↗
22. Air-plasma-sprayed thermal barrier coatings that are resistant to high-temperature attack by glassy deposits10.1016/j.actamat.2010.09.013 ↗
23. Jet engine coatings for resisting volcanic ash damage10.1002/adma.201004783 ↗
24. Comparison of NaVO3+CMAS mixture and CMAS corrosion to thermal barrier coatings10.1016/j.corsci.2020.108968 ↗
25. Effects of laser glazing on CMAS corrosion behavior of Y2O3 stabilized ZrO2 thermal barrier coatings10.1016/j.corsci.2019.06.025 ↗
26. Some aspects of the hot corrosion of thermal barrier coatings10.1007/BF02646315 ↗
27. Burner rig evaluation of ceramic coatings with vanadium-contaminated fuels, trans
28. Corrosion of thermal barrier coatings by vanadium and sulfur compounds10.1179/mht.2000.17.3.004 ↗
29. Investigation of reactions between vanadium oxide and plasma-sprayed yttria-stabilized zirconia coatings10.1016/j.jeurceramsoc.2008.09.016 ↗
30. A comparative study on hot corrosion resistance of three types of thermal barrier coatings: YSZ, YSZ+Al2O3 and YSZ/Al2O310.1016/j.msea.2007.06.001 ↗
31. P. Mohan, Environmental degradation of oxidation resistant and thermal barrier coatings for fuel-flexible gas turbine application, dissertation for doctor degree of philosophy, 2010.
32. Zirconates as new materials for thermal barrier coatings10.1111/j.1151-2916.2000.tb01506.x ↗
33. Infiltration-inhibiting reaction of gadolinium zirconate thermal barrier coatings with CMAS melts10.1111/j.1551-2916.2007.02175.x ↗
34. Degradation of yttria-stabilized zirconia thermal barrier coatings by vanadium pentoxide, phosphorus pentoxide, and sodium sulfate10.1111/j.1551-2916.2007.01941.x ↗
35. An investigation on hot corrosion behavior of YSZ-Ta2O5 in Na2SO4+V2O5 salt at 1100 °C, Corros
36. Hot corrosion behavior of NiCoCrAlYTa coating deposited on Inconel alloy substrate by high velocity oxy-fuel spraying upon exposure to molten V2O5-containing salts, Corros
37. Hot corrosion behavior of Sc2O3–Y2O3–ZrO2 thermal barrier coatings in presence of Na2SO4 + V2O5 molten salt, Corros
38. A delamination mechanism for thermal barrier coatings subject to calcium–magnesium–alumino-silicate (CMAS) infiltration10.1016/j.actamat.2004.11.028 ↗
39. Correlation between the mechanical properties and splat microstructures of an air plasma sprayed thermal barrier coating10.1299/jmmp.2.1275 ↗
40. Stress relaxation of low pressure plasma-sprayed NiCrAlY alloys10.1016/0921-5093(93)90575-Y ↗
41. TGO growth behavior in TBCS with APS and HVOF bond coats, Surf10.1016/j.surfcoat.2007.09.042 ↗
42. Oxidation of high-temperature coatings, Proc
43. D.K. Gupta, D.S. Duvall, A Silicon and Hafnium Modified Plasma Sprayed MCrAlY Coating for Single Crystal Superalloys, the Metallurgical Society, Warrendale, Pennsylvania, 1984, 711–720.10.7449/1984/Superalloys_1984_711_720 ↗
44. Variation of thermal barrier coating lifetime characteristics with thermal durability evaluation methods10.1007/s11666-018-0784-1 ↗
45. Overview on advanced thermal barrier coatings, Surf10.1016/j.surfcoat.2010.08.151 ↗
46. Gadolinium zirconate/YSZ thermal barrier coatings: plasma spraying, microstructure, and thermal cycling behavior10.1111/jace.13204 ↗
47. G. Dwivedi, V. Viswanathan, S. Sampath, A. Shyam, and E. Lara-Curzio, Fracture toughness of plasma-sprayed thermal barrier ceramics: influence of processing, Microstructure, and Thermal Aging, J Am Ceram Soc, 2014, 9(9), 2736–2744.10.1111/jace.13021 ↗
48. Hot corrosion behavior of Yb2Zr2O7 ceramic coated with V2O5 at temperatures of 600–800°C in air10.1016/j.corsci.2010.06.007 ↗
49. High-temperature hot corrosion behavior of gadolinium zirconate by vanadium pentoxide and sodium sulfate in air10.1016/j.jeurceramsoc.2010.05.002 ↗
50. Hot corrosion behavior of V2O5-coated Gd2Zr2O7 ceramic in air at 700–850 °C10.1016/j.jeurceramsoc.2009.01.001 ↗