Room temperature deposition of (Ti,Al)N and (Ti,Al)(C,N) coatings by pulsed laser deposition for tribological applications
Source abstract
Abstract
Abstract Titanium–aluminium based nitride (Ti,Al)N and carbonitride (Ti,Al)(C,N) hard coating systems possess excellent tribological behaviour in metal cutting and polymer forming contacts. In the present work (Ti,Al)N and (Ti,Al)(C,N) coatings were deposited by employing the pulsed laser deposition (PLD) technique. A pulsed Nd:YAG laser with 1064 nm wavelength was used for the vaporization of TiAl targets in low-pressure N2 or N2/C2H2, atmospheres at room temperature. The highly ionized metal vapour was deposited onto polished substrates (molybdenum, AISI D2). The coatings were characterized by light-microscopy, scanning electron microscopy, X-ray diffraction and hardness tests. The variation of the deposition parameters causes a change of the chemical composition, the texture and crystallinity of the coatings and, consequently, the mechanical properties and tribological behaviour. The latter was characterized in pin-on-disc tests at room temperature by using coated discs and uncoated AISI 52100 (DIN 100Cr6) steel and alumina pins as counterparts. The results demonstrate the excellent industrial applicability of these coatings for cold-forming operations: very low-wear rates were found for the (Ti,Al)N coatings. In contrast, the (Ti,Al)(C,N) coatings possess low-friction coefficients of approximately 0.2. As an outstanding advantage of these coatings, which were deposited at the room temperature by the PLD process, their excellent adhesion to the substrate can be pointed out, reaching the highest level (HF 1) in the Rockwell indentation test.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research · Boron and Carbon Nanomaterials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (24)
Show source-provided references
1. Holmberg · 1994
2. Huang · Surf. Coat. Technol. · 1996 · 81 · 16410.1016/0257-8972(95)02479-4 ↗
3. PalDey · Mater. Sci. Eng. A · 2003 · 342 · 5810.1016/S0921-5093(02)00259-9 ↗
4. Heim · Surf. Coat. Technol. · 1998 · 98 · 155310.1016/S0257-8972(97)00303-4 ↗
5. Kawata · Thin Solid Films · 2001 · 390 · 6410.1016/S0040-6090(01)00939-7 ↗
6. J.M. Lackner, W. Waldhauser, R. Ebner, B. Major, T. Schöberl, Morphological, structural and tribological characterisation of pulsed laser deposited titanium nitride coatings, Praktische Metallographie, accepted
7. J.M. Lackner, C. Stotter, W. Waldhauser, R. Ebner, W. Lenz, M. Beutl, Surf. Coat. Technol. 174–175 (2003) 40210.1016/S0257-8972(03)00392-X ↗
8. Lackner · Galvanotechnik · 2003 · 94 · 1226
9. Chrisey · 1994
10. Acquaviva · Thin Solid Films · 2000 · 379 · 4510.1016/S0040-6090(00)01350-X ↗
11. Morimoto · Appl. Surf. Sci. · 1998 · 127–129 · 99410.1016/S0169-4332(97)00780-0 ↗
12. R. Ebner, W. Waldhauser, W. Lenz, Proceeding of Materials Week 2001, Munich, 2001
13. Lii · Surf. Coat. Technol. · 1998 · 99 · 19710.1016/S0257-8972(97)00104-7 ↗
14. Thornton · J. Vac. Sci. Technol. · 1974 · 11 · 66610.1116/1.1312732 ↗
15. Münz · J. Vac. Sci. Technol. A · 1986 · 4 · 271710.1116/1.573713 ↗
16. Pinkas · Thin Solid Films · 1999 · 355–356 · 38010.1016/S0040-6090(99)00667-7 ↗
17. Lüth · 1995
18. Ensinger · Surf. Coat. Technol. · 1994 · 65 · 9010.1016/S0257-8972(94)80014-6 ↗
19. Karlsson · Surf. Coat. Technol. · 2000 · 126 · 110.1016/S0257-8972(00)00518-1 ↗
20. H. Jehn, G. Reiners, N. Siegel, DIN-Fachbericht 39, Charakterisierung dünner Schichten, Beuth-Verlag, Berlin, 1993
21. Huang · Surf. Coat. Technol. · 1995 · 71 · 25910.1016/0257-8972(94)02320-P ↗
22. Zhou · Thin Solid Films · 1999 · 339 · 20310.1016/S0040-6090(98)01364-9 ↗
23. Yoon · Surf. Coat. Technol. · 2002 · 161 · 23710.1016/S0257-8972(02)00474-7 ↗
24. Ronkainen · Surf. Coat. Technol. · 1990 · 43–44 · 88810.1016/0257-8972(90)90029-C ↗