Friction behaviour of anodic oxide film on aluminum impregnated with molybdenum sulfide compounds

M. Maejima, K. Saruwatari, M. Takaya

Surface and Coatings Technology· Volume 132· Issue 2-3
Publisher page

Abstract

In order to improve the lubricity and wear resistance of aluminum anodic oxide films, it is necessary to ensure the film layers are dense to prevent cracking, and to harden the films as well as reduce the shear stress of the film surfaces. From this view point, lubricious, hard anodic oxide films have been studied in the past, but fully satisfactory results have yet to be realized. In this paper, we report on our study of the re-anodizing of anodic oxide film in an aqueous solution of (NH)MoS. Molybdenum sulfide and compounds filled the 20-nm diameter pores of the film, creating internal stress which compressed the film, suppressing the occurrence of cracks and reducing the friction coefficient.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Anodic Oxide Films and Nanostructures · Corrosion Behavior and Inhibition · Concrete Corrosion and Durability

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (16)

Show source-provided references
1. L.B. Sargent, Jpn. Soc. Ceram. Ind. Mechanical Properties of Ceramics. Gihodo shuppan 56 (1979) pp. 25–34.
2. Sasada · J. Inst. Elec. Eng. Jpn. · 1997 · 117 · 84310.1541/ieejjournal.117.843 ↗
3. Takaya · J. Surf. Finish Soc Jpn. · 1990 · 41 · 210.4139/sfj.41.2 ↗
4. Hafer · Plating · 1958 · 45 · 623
5. Johnson · Plating · 1962 · 49 · 986
6. Kanematsu · J. Surf. Finish. Soc. Jpn. · 1961 · 12 · 306
7. Itoh · J. Surf. Finsh. Soc. Jpn. · 1968 · 1119 · 504
8. Koizumi · J. Surf. Finish. Soc. Jpn. · 1972 · 23 · 45210.4139/sfj1950.23.452 ↗
9. Fukushima · Tokyo Metro Ind. Cent. Rep. · 1960 · 10 · 42
10. Isawa · Inst. Phys. Chem. Res. Jpn. · 1960 · 36 · 685
11. Maclin · Metal Finish · 1961 · 59 · 55
12. Baba · J. Surf. Finish. Soc. Jpn. · 1979 · 30 · 4410.4139/sfj1950.30.44 ↗
13. Mizuki · J. Surf. Finish. Soc. Jpn.’ · 1979 · 28 · 44
14. Rasmussenji · Galvanotechnik. · 1994 · 85 · 2176
15. Ohkubo · J. Surf. Finish. Soc. Jpn. · 1982 · 33 · 5010.4139/sfj1950.33.50 ↗
16. H. Iimachi; Kinzoku–zairyo, nikkann kogyo shinbunsha 6 (1976) pp. 50.