journal article·2006-05

Surface characterization of copper electroless deposition on atomic layer deposited palladium on iridium and tungsten

Young-Soon Kim, Jiho Shin, Joong-Hee Cho, Gregory A. Ten Eyck, De-Li Liu, Samuk Pimanpang, Toh-Ming Lu, Jay J. Senkevich, Hyung-Shik Shin

Surface and Coatings Technology· Volume 200· Issue 20-21
Publisher page

Abstract

Abstract Iridium and tungsten refractory metals possess high melting points, hardness, and good electrical resistivity. Palladium has been recently deposited on W and Ir via atomic layer deposition and it is also an appropriate catalyst for the electroless deposition of copper. Palladium was deposited at 80 ± 5 °C with a PdII(hfac)2 sublimation temperature of 46.0 ± 0.5 °C using 13 sccm Ar as a carrier gas, and 105 sccm H2 as a reducing gas on Ir and W substrates for 150 cycles. The thickness of Pd was 20 and 30 A on Ir and W substrates, respectively, with a low surface roughness. For the Cu electroless process, ethylenediamine-tetraacetic acid (EDTA) was used as a chelating agent, glyoxylic acid as a reducing agent, and additional chemicals such as polyethylene glycol and 2,2′dipyridine as surfactant and stabilizer respectively. Electroless Cu was undertaken at 60 °C with good adhesion to iridium and tungsten with Pd as a catalytic layer.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Electrodeposition and Electroless Coatings · Copper Interconnects and Reliability · Electrocatalysts for Energy Conversion

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (28)

Show source-provided references
1. Hanna · Mater. Lett. · 2004 · 58 · 10410.1016/S0167-577X(03)00424-5 ↗
2. Miura · Surf. Coat. Technol. · 2003 · 169–170 · 9110.1016/S0257-8972(03)00165-8 ↗
3. Kim · J. Magn. Magn. Mater. · 2004 · 271 · 3910.1016/j.jmmm.2003.09.012 ↗
4. Yuan · Physica, E, Low-Dimens. Syst. Nanostruct. · 2004 · 23 · 7510.1016/j.physe.2004.01.011 ↗
5. Wang · Appl. Surf. Sci. · 2002 · 199 · 5210.1016/S0169-4332(02)00473-7 ↗
6. Yu · Polymers · 2002 · 43 · 413710.1016/S0032-3861(02)00263-X ↗
7. Honma · J. Electrochem. Soc. · 1994 · 141 · 73010.1149/1.2054800 ↗
8. Shacham-Diamand · Electrochem. Solid-State Lett. · 2000 · 3 · 27910.1149/1.1391124 ↗
9. Wang · Electrochem. Solid-State Lett. · 2003 · 6 · C3810.1149/1.1541255 ↗
10. Kim · J. Electrochem. Soc. · 2004 · 151 · C9710.1149/1.1633269 ↗
11. Kohn · Appl. Surf. Sci. · 2003 · 212-213 · 36710.1016/S0169-4332(03)00116-8 ↗
12. Park · J. Electrochem. Soc. · 2002 · 149 · C2810.1149/1.1423642 ↗
13. Kim · Appl. Surf. Sci. · 2003 · 210 · 23110.1016/S0169-4332(03)00158-2 ↗
14. Yun · Korean J. Chem. Eng. · 1996 · 13 · 51010.1007/BF02706002 ↗
15. Chyan · J. Electrochem. Soc. · 2003 · 150 · C34710.1149/1.1565138 ↗
16. Hara · Eletrochem. Solid-State Lett. · 2003 · 6 · C810.1149/1.1527410 ↗
17. Azizi · Appl. Surf. Sci. · 2004 · 228 · 32010.1016/j.apsusc.2004.01.026 ↗
18. Lim · Solid-State Electron. · 2001 · 45 · 208310.1016/S0038-1101(01)00192-7 ↗
19. Schrott · Appl. Phys. Lett. · 1994 · 64 · 158210.1063/1.111846 ↗
20. Senkevich · Chem. Vap. Depos. · 2003 · 9 · 25810.1002/cvde.200306246 ↗
21. Ten Eyck · Chem. Vap. Depos. · 2005 · 11 · 6010.1002/cvde.200306312 ↗
22. Kim · J. Electrochem. Soc. · 2005 · 152 · C37610.1149/1.1899285 ↗
23. Lanford · Nucl. Instrum. Methods Phys. Res., B Beam Interact. Mater. Atoms · 1998 · 136-138 · 117710.1016/S0168-583X(97)00734-9 ↗
24. Jezewski · Chem. Vap. Depos. · 2003 · 9 · 30510.1002/cvde.200304155 ↗
25. Kim · J. Electrochem. Soc. · 2005 · 152 · C8910.1149/1.1850377 ↗
26. Moulder · 1992
27. Powell · Appl. Surf. Sci. · 1995 · 89 · 14110.1016/0169-4332(95)00027-5 ↗
28. Senkevich · Colloids Surf., A Physicochem. Eng. Asp. · 2003 · 221 · 2910.1016/S0927-7757(03)00094-3 ↗