journal article·2018-09

Hybrid high power impulse and radio frequency magnetron sputtering system for TiCrSiN thin film depositions: Plasma characteristics and film properties

Bih-Show Lou, Yung-Chin Yang, Yi-Xiang Qiu, Wahyu Diyatmika, Jyh-Wei Lee

Publisher page

Abstract

Abstract TiCrSiN thin films were successfully grown using a hybrid approach in which a high power impulse magnetron sputtering (HiPIMS) power was combined with a radio frequency (RF) power. Different Si contents were obtained by changing the RF power of Si target. The ion energy distribution functions (IEDFs) showed that the energy tails of all sputtered ions from the targets and sputtering gases shifted to a higher energy tails when the Si target power increased from 50 to 150 W. The peak power density of the TiCr target powered by HiPIMS and the corresponding Si content in the films increased from 1214 to 1350 W/cm2 and from 0.2 to 17.9 at.%, respectively, as the Si target power increased from 50 to 150 W. The Si atoms were in the form of amorphous Si3N4 phase. The Si content showed a major influence on the microstructure, adhesion and mechanical properties of TiCrSiN film. Although a nanocomposite microstructure was formed when the Si content was 17.9 at.%, lower hardness and acceptable adhesion property were obtained due to a microstructure consisting of small TiN nanograins embedded in a large amount of soft amorphous silicon nitride matrix. The hardness of TiCrSiN film reached a maximum hardness of 31.1 GPa at Si = 6.7 at.% due to the refined microstructure and grain boundary hardening effect.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research · GaN-based semiconductor devices and materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (27)

Show source-provided references
1. Electronic and mechanical properties of nanocrystalline composites when approaching molecular size10.1016/S0040-6090(96)09480-1 ↗
2. Recent progress in the superhard nanocrystalline composites: towards their industrialization and understanding of the origin of the superhardness10.1016/S0257-8972(98)00618-5 ↗
3. Effects of Al and V additions on mechanical response in thick TiSiCN nanocomposites deposited using plasma-enhanced magnetron sputtering10.7567/JJAP.52.11NJ10 ↗
4. Towards hard yet self-lubricious CrAlSiN coatings10.1016/j.jallcom.2014.08.132 ↗
5. The microstructure and mechanical properties evaluation of CrTiAlSiN coatings: effects of silicon content10.1016/j.tsf.2017.07.058 ↗
6. Structure and mechanical property evaluation of Cr–Ti–B–N coatings10.1016/j.tsf.2013.02.095 ↗
7. Influences of target poisoning on the mechanical properties of TiCrBN thin films grown by a superimposed high power impulse and medium frequency magnetron sputtering10.1016/j.surfcoat.2017.06.081 ↗
8. Synthesis and mechanical properties of quaternary Ti–Cr–Si–N nanocomposite coatings deposited by closed field unbalanced middle frequency magnetron sputtering10.1016/j.jallcom.2012.03.074 ↗
9. Synthesis and mechanical evaluation of quaternary Ti–Cr–Si–N coatings deposited by a hybrid method of arc ion plating and sputtering techniques10.1016/j.surfcoat.2005.08.023 ↗
10. High power impulse magnetron sputtering discharge10.1116/1.3691832 ↗
11. Deposition rates of high power impulse magnetron sputtering: physics and economics10.1116/1.3299267 ↗
12. Hybrid HIPIMS and DC magnetron sputtering deposition of TiN coatings: deposition rate, structure and tribological properties10.1016/j.surfcoat.2013.07.003 ↗
13. Improving HiPIMS deposition rates by hybrid RF/HiPIMS co-sputtering, and its relevance for NbSi films10.1016/j.surfcoat.2014.02.007 ↗
14. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
15. The ion energy distributions and ion flux composition from a high power impulse magnetron sputtering discharge10.1016/j.tsf.2006.04.051 ↗
16. Metal plasmas for the fabrication of nanostructures10.1088/0022-3727/40/8/S06 ↗
17. Adding high time resolution to charge-state-specific ion energy measurements for pulsed copper vacuum arc plasmas
18. Tailoring the nanostructure of Ti–Si–N thin films by HiPIMS in deep oscillation magnetron sputtering (DOMS) mode10.1016/j.surfcoat.2014.12.065 ↗
19. Influence of Si contents on the microstructure, mechanical and tribological properties of Cr–Si–N coatings10.1016/j.ceramint.2015.12.019 ↗
20. Effects of Si content and free Si on oxidation behavior of Ti–Si–N coating layers10.1016/S0040-6090(03)01083-6 ↗
21. Effect of duty cycles on the deposition and characteristics of high power impulse magnetron sputtering deposited TiN thin films10.1016/j.surfcoat.2014.03.011 ↗
22. Structure and properties of CrSiN nanocomposite coatings deposited by hybrid modulated pulsed power and pulsed dc magnetron sputtering10.1016/j.surfcoat.2012.11.053 ↗
23. Structural analysis of sputtered (W-C)1−xMx (M = Fe, Co) films with 0 ≦ x ≦ 0.2010.1016/0257-8972(93)90123-6 ↗
24. A quantitative study of the hardness of a superhard nanocrystalline titanium nitride/silicon nitride coating10.1016/j.scriptamat.2005.02.024 ↗
25. HiPIMS deposition of silicon nitride for solar cell application10.1016/j.surfcoat.2018.03.025 ↗
26. Mechanical and tribological behavior of silicon nitride and silicon carbon nitride coatings for total joint replacements10.1016/j.jmbbm.2013.05.002 ↗
27. Microstructure control in TiAlN/SiNx multilayers with appropriate thickness ratios for improvement of hardness and anti-corrosion characteristics10.1016/j.vacuum.2012.02.052 ↗