The effect of humidity on friction behavior of hydrogenated HIPIMS W-C:H coatings
Source abstract
Abstract
Abstract The study of the effect of humidity on friction behavior in HiPIMS (High Power Impulse Magnetron Sputtering) W-C:H coating/steel ball system confirmed the formation of transfer layer adhered to the ball and consisting of hydrogenated carbon, ferritungstate and small amounts of tungsten (sub)oxides and iron oxides. The corresponding mechano(tribo)chemical reactions driven by flash temperature in the sliding asperities involved oxidation, water vapor dissociation and carbon hydrogenation. Such composition agreed with the results of modelling based on the minimization of free Gibbs energy in the mutually interacting thermochemical reactions. The applicability of modelling to friction was attributed to fast reactions among microscopic asperities eliminating kinetical factors. In inert atmospheres, oxidation and hydrogenation were suppressed and friction seemed to be controlled by the amount of additional carbon.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (44)
Show source-provided references
1. Tribological performance and tribochemistry of nanocrystalline WC/amorphous diamond-like carbon composites10.1016/S0040-6090(98)01456-4 ↗
2. Deposition and some properties of nanocrystalline WC and nanocomposite WC/a-C: H coatings10.1016/S0040-6090(03)00324-9 ↗
3. Microstructure, adhesion and tribological properties of W-C: hx coatings deposited on M2 and WC substrates10.1016/j.msea.2006.06.008 ↗
4. Nanoscale multilayer WC/C coatings developed for nanopositioning, part II: friction and wear10.1016/j.tsf.2005.03.020 ↗
5. Influence of surface topography of arc-deposited TiN and sputter deposited WC/C on the initial material transfer tendency and friction characteristics under dry sliding conditions10.1016/j.surfcoat.2008.12.011 ↗
6. Sliding friction of nanocomposite WC1-x/C coatings: transfer films and its influence on tribology10.1166/jnn.2009.NS23 ↗
7. The effect of air humidity on tribological behaviours of W-C: H coatings with different tungsten contents sliding against bearing steel10.1016/j.wear.2012.08.009 ↗
8. Identification of the wear mechanism on WC/C nanostructured coatings
9. Nanoindentation, AFM, and tribological properties of thin nc-WC-a-C coatings10.1016/j.jeurceramsoc.2012.01.037 ↗
10. Effects of WC phase contents on the microstructure, mechanical and tribological behaviors of WC/a-C superlattice coatings10.1016/j.apsusc.2015.09.181 ↗
11. Microstructure, mechanical and tribological properties of WC/a-C: H coatings deposited by cathodic arc ion-plating10.1016/j.vacuum.2016.07.023 ↗
12. Investigation of post-deposition annealing effects on microstructure, mechanical and tribological properties of WC/a-C nanocomposite coatings10.1007/s11249-016-0699-2 ↗
13. Hydrogen content influence on tribological properties of nc-WC/a-C: H coatings10.1016/j.diamond.2016.01.007 ↗
14. WC/C: H films synthesized by an hybrid reactive magnetron sputtering/Plasma enhanced chemical vapor deposition process: an alternative to Cr(VI) based chromium plating10.1016/j.tsf.2016.09.002 ↗
15. Mechanical and tribological properties of the high target utilization sputtering W-C coatings on different substrates10.1016/j.ijrmhm.2016.12.015 ↗
16. The comparison of structure and properties in DC magnetron sputtered and HiPIMS W-C: H coatings with different hydrogen content10.1016/j.ceramint.2018.09.219 ↗
17. Tribological behavior of hydrogenated W-C/a-C: H coatings deposited by three different sputtering techniques10.1590/0366-6913201965s12577 ↗
18. Hybrid PVD-PECVD W-C: H coatings prepared by different sputtering techniques: the comparison of deposition processes, composition and properties10.1016/j.surfcoat.2019.07.078 ↗
19. Room and high temperature tribological behaviour of W-DLC coatings produced by DCMS and hybrid DCMS-HiPIMS configuration10.3390/coatings10040319 ↗
20. Hydrogenation and hybridization in hard W-C:H coatings prepared by hybrid PVD-PECVD method with methane and acetylene10.1016/j.ijrmhm.2020.105211 ↗
21. Characterization of wear surfaces in dry sliding of steel and alumina on hydrogenated and hydrogen-free carbon films10.1016/0925-9635(94)90147-3 ↗
22. Characterization of transfer layers on steel surfaces sliding against diamond like hydrocarbon films in dry nitrogen10.1016/0257-8972(95)02518-9 ↗
23. Evidence of graphitization of diamond-like carbon films during sliding wear10.1023/A:1018641304944 ↗
24. Effect of source gas chemistry on tribological performance of diamond-like carbon films10.1016/S0925-9635(99)00361-1 ↗
25. Friction control of diamond-like carbon coatings10.1016/S0257-8972(97)00275-2 ↗
26. Tribochemistry between hydrogen and diamond-like carbon films10.1016/S0257-8972(01)01398-6 ↗
27. Role of third bodies in friction and wear of protective coatings10.1116/1.1599869 ↗
28. Monitoring transfer films and friction instabilities with in situ raman tribometry10.1023/A:1021942830132 ↗
29. Microstructure and mechanical properties of W-C: H coatings deposited by pulsed reactive magnetron sputtering10.1016/j.surfcoat.2011.03.062 ↗
30. Transfer layer evolution during friction in HiPIMS W-C coatings10.1016/j.wear.2021.204123 ↗
31. Theoretical analysis of absorption and resonant raman scattering spectra of trans-(CH)x10.1103/PhysRevB.30.876 ↗
32. Transpolyacetylene chains in hydrogenated amorphous carbon films free of nanocrystalline diamond10.1063/1.1538349 ↗
33. Hydrogen incorporation processes in nanodiamond films studied by isotopic induced modifications of Raman spectra10.1063/1.2358104 ↗
34. Raman microspectroscopy and vibrational sum frequency generation spectroscopy as probes of the bulk and surface compositions of size resolved sea spray aerosol particles10.1039/c3cp43899f ↗
35. The role of hydrogen in tribological properties of diamond-like carbon films10.1016/S0257-8972(01)01417-7 ↗
36. Friction of diamond-like carbon films in different atmospheres10.1016/S0043-1648(03)00336-3 ↗
37. The effects of deposition conditions on hydrogenation, hardness and elastic modulus of W-C: H coatings10.1016/j.jeurceramsoc.2019.12.062 ↗
38. Role of oxygen atmosphere in high temperature sliding behaviour of W containing diamond-like carbon (W-DLC)10.1016/j.surfcoat.2017.06.093 ↗
39. Raman spectrum of graphite10.1063/1.1674108 ↗
40. Bonding in hydrogenated diamond-like carbon by Raman spectroscopy10.1016/j.diamond.2004.10.030 ↗
41. Origin of 1150 cm-1 Raman mode in nanocrystalline diamond
42. Raman microspectroscopy of soot and related carbonaceous materials: spectral analysis and structural information10.1016/j.carbon.2005.02.018 ↗
43. Raman spectroscopy of ferritungstite: experimental and model spectra10.1007/BF00205216 ↗
44. Polyacetylene: myth and reality10.3390/ma11020242 ↗