Formation and evolution of phosphorus-containing species during high-temperature oxidation of TiAl dipped in a low-concentrated phosphoric acid solution
Source abstract
Abstract
Abstract TiAl samples were dipped in a low-concentrated phosphoric acid solution, air dried, then heated to 800 °C under argon gas before oxidation under reconstituted air at this temperature. At the end of the heating ramp, sample surfaces were covered by a titanium pyrophosphate (TiP 2 O 7 ) layer, well adhered to the substrate. This pyrophosphate was shown to be detectable from 400 °C. Chemical reactions have been proposed for the formation of this compound. TiP 2 O 7 coating strongly increased the oxidation resistance of TiAl at 800 °C for 100 h. After 100 h, a transition period occurred leading to the change of TiP 2 O 7 into TiO 2 , which was achieved after 230 h, total mass gain always remaining below that of raw substrate. This evolution was demonstrated not resulting from a thermal decomposition of pyrophosphate compound.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Intermetallics and Advanced Alloy Properties · MXene and MAX Phase Materials · Inorganic Chemistry and Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (34)
Show source-provided references
1. Kawabata · Acta Met. · 1985 · 33 · 135510.1016/0001-6160(85)90245-7 ↗
2. Lipsitt · Metall. Trans. · 1975 · 6A · 199110.1007/BF03161822 ↗
3. Wu · Intermetallics · 2006 · 14 · 111410.1016/j.intermet.2005.10.019 ↗
4. Rahmel · Mater. Corros. · 1995 · 46 · 27110.1002/maco.19950460503 ↗
5. Lasalmonie · Intermetallics · 2006 · 14 · 112310.1016/j.intermet.2006.01.064 ↗
6. Becker · Oxid. Met. · 1992 · 38 · 42510.1007/BF00665663 ↗
7. Maurice · Acta Mater. · 2007 · 55 · 331510.1016/j.actamat.2007.01.030 ↗
8. Yang · Bull. College Eng., N.T.U. · 2003 · 89 · 3
9. Yoshihara · Intermetallics · 1995 · 3 · 35710.1016/0966-9795(95)94254-C ↗
10. Jiang · Scr. Mater. · 2002 · 46 · 63910.1016/S1359-6462(02)00042-8 ↗
11. Lu · J. Mater. Res. · 2007 · 22 · 148610.1557/JMR.2007.0188 ↗
12. Anada · Mater. Trans., JIM · 1995 · 36 · 53310.2320/matertrans1989.36.533 ↗
13. Perez · Mat. Sci. Eng. A · 2000 · 284 · 13810.1016/S0921-5093(00)00755-3 ↗
14. Kaczmarek · Surf. Coat. Technol. · 2007 · 201 · 616710.1016/j.surfcoat.2006.08.144 ↗
15. Talaka · Mat. Sci. Forum · 2007 · 534-536 · 158910.4028/www.scientific.net/MSF.534-536.1589 ↗
16. Zhang · Corros. Sci. · 2007 · 49 · 359810.1016/j.corsci.2007.03.025 ↗
17. Wu · Intermetallics · 2005 · 13 · 87910.1016/j.intermet.2005.01.014 ↗
18. Li · Intermetallics · 2003 · 11 · 14310.1016/S0966-9795(02)00193-0 ↗
19. Perez · Surf. Coat. Technol. · 2005 · 191 · 29310.1016/j.surfcoat.2004.04.066 ↗
20. Schumacher · Oxid. Met. · 2000 · 54 · 31710.1023/A:1004606513758 ↗
21. Zschau · Nucl. Instrum. Methods Phys. Res., B · 2008 · 266 · 244110.1016/j.nimb.2008.03.024 ↗
22. Donchev · J. Alloys Compd. · 2008 · 452 · 710.1016/j.jallcom.2006.12.157 ↗
23. Retallick · Intermetallics · 1998 · 6 · 33510.1016/S0966-9795(97)00096-4 ↗
24. Guy Lorin, « La phosphatation des métaux », Ed. Eyrolles, Paris 1973.
25. Krasicka-Cydzik · Corros. Sci. · 2004 · 46 · 248710.1016/j.corsci.2004.01.012 ↗
26. Nakahira · J. Ceram. Soc. Japan · 2006 · 114 · 4610.2109/jcersj.114.46 ↗
27. Yang · Acta Mater. · 2002 · 50 · 69110.1016/S1359-6454(01)00390-1 ↗
28. Wu · Intermetallics · 2007 · 15 · 14510.1016/j.intermet.2006.04.003 ↗
29. Marcu · Appl. Catal., A Gen. · 2002 · 227 · 30910.1016/S0926-860X(01)00947-4 ↗
30. Marcu · J. Mol. Catal., A Chem. · 2003 · 203 · 24110.1016/S1381-1169(03)00376-5 ↗
31. Shi · Microporous Mesoporous Mater. · 2006 · 88 · 23210.1016/j.micromeso.2005.09.013 ↗
32. Kuo · Mater. Chem. Phys. · 2005 · 93 · 36110.1016/j.matchemphys.2005.03.023 ↗
33. Krogh Andersen · Inorg. Chem. · 1998 · 37 · 431310.1021/ic9801894 ↗
34. Szirtes · J. Therm. Anal. Calorim. · 2003 · 73 · 20910.1023/A:1025150011743 ↗