Development of anodization technique on zirconium silicide material for reproducing micro/nanosurface structure: Application to nuclear accident tolerant fuel cladding
Source abstract
Abstract
Abstract Zirconium silicide (ZrSi2) surfaces with micro/nanoscale structures were fabricated using an anodization technique with different working solutions. The surface structures evolved depending on the reaction time, and the resulting surface structures were characterized using scanning electron microscopy. For all three solutions, the anodization conditions for producing micro/nano surface structures with the superhydrophilicity were successfully found. The etching rate and thickness were controlled depending on the type of solutions. In the organic bath-based ammonium fluoride (NH4F) solutions, the etching thickness was significantly reduced in comparison to that using a water bath-based hydrofluoric acid (HF) solution. Superior oxidation resistance of ZrSi2 was maintained for all superhydrophilic, anodized ZrSi2 surfaces at 700 °C air oxidation regardless of the type of solution. The superhydrophilic, anodized ZrSi2 surfaces significantly increased the Leidenfrost temperature by inducing liquid-solid contact between the heated surface and coolant. We expect the developed surfaces to be useful in future nuclear fuel cladding material applications for ensuring the safety of nuclear reactors.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Nuclear Materials and Properties · Fuel Cells and Related Materials · Semiconductor materials and devices
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (63)
Show source-provided references
1. In-reactor corrosion performance of ZIRLO™ and zircaloy-4
2. Accident tolerant fuels for LWRs: a perspective10.1016/j.jnucmat.2013.12.005 ↗
3. High temperature oxidation of fuel cladding candidate materials in steam–hydrogen environments10.1016/j.jnucmat.2013.05.047 ↗
4. Breakaway phenomenon of Zr-based alloys during a high-temperature oxidation10.1016/j.jnucmat.2007.02.011 ↗
5. Air oxidation of Zircaloy-4, M5® and ZIRLO™ cladding alloys at high temperatures10.1016/j.jnucmat.2011.04.012 ↗
6. Prototypical experiments relating to air oxidation of Zircaloy-4 at high temperatures10.1016/j.jnucmat.2009.04.018 ↗
7. Research and development methodology for practical use of accident tolerant fuel in light water reactors10.1016/j.net.2015.12.004 ↗
8. Alloy selection for accident tolerant fuel cladding in commercial light water reactors
9. Powers · 2015
10. Neutronic analysis of candidate accident-tolerant cladding concepts in pressurized water reactors
11. Development status of accident-tolerant fuel for light water reactors in Korea10.1016/j.net.2015.11.011 ↗
12. Preliminary safety analysis of the PWR with accident-tolerant fuels during severe accident conditions10.1016/j.anucene.2015.02.040 ↗
13. High temperature steam-oxidation behavior of arc ion plated Cr coatings for accident tolerant fuel claddings10.1016/j.surfcoat.2015.09.022 ↗
14. Adhesion property and high-temperature oxidation behavior of Cr-coated Zircaloy-4 cladding tube prepared by 3D laser coating10.1016/j.jnucmat.2015.06.030 ↗
15. Microstructure and mechanical strength of surface ODS treated Zircaloy-4 sheet using laser beam scanning10.5516/NET.07.2014.027 ↗
16. Fabrication and material issues for the application of SiC composites to LWR fuel cladding10.5516/NET.07.2012.084 ↗
17. Characterization of SiC-SiC composites for accident tolerant fuel cladding10.1016/j.jnucmat.2015.08.020 ↗
18. Multilayer (TiN, TiAlN) ceramic coatings for nuclear fuel cladding10.1016/j.jnucmat.2016.05.021 ↗
19. Zirconium-silicide coating on zircaloy-4 substrate for accident tolerance: effects on oxidation resistance and boiling10.1016/j.anucene.2018.11.019 ↗
20. Magnetron sputter deposition of zirconium-silicide coating for mitigating high temperature oxidation of zirconium-alloy10.1016/j.surfcoat.2017.03.018 ↗
21. Development of zirconium-silicide coatings for improved performance zirconium-alloy fuel cladding
22. Thermodynamic assessment of the Si-Zr system10.1016/0364-5916(94)90036-1 ↗
23. Can corrosion and CRUD actually improve safety margins in LWRs?10.1016/j.anucene.2013.07.019 ↗
24. The effect of capillary wicking action of micro/nano structures on pool boiling critical heat flux10.1016/j.ijheatmasstransfer.2011.08.044 ↗
25. Wetting and evaporation phenomena of water droplets on textured surfaces10.1016/j.ijheatmasstransfer.2015.06.046 ↗
26. Effect of surface wettability on boiling and evaporation10.1016/j.energy.2004.05.004 ↗
27. Effect of nanoparticle deposition on capillary wicking that influences the critical heat flux in nanofluids
28. Wettability conversion on ZnO nanowire arrays surface modified by oxygen plasma treatment and annealing10.1016/j.cplett.2005.08.039 ↗
29. Electrophoretic deposition (EPD): mechanisms, kinetics, and application to ceramics10.1111/j.1151-2916.1996.tb08929.x ↗
30. Micro/nanostructure evolution of zircaloy surface using anodization technique: application to nuclear fuel cladding modification10.1016/j.apsusc.2012.05.081 ↗
31. Wetting and roughness10.1146/annurev.matsci.38.060407.132434 ↗
32. Titanium dioxide nanotube arrays fabricated by anodizing processes electrochemical properties10.1149/1.2347098 ↗
33. Effects of heat flux on dropwise condensation on a superhydrophobic surface10.1007/s12206-016-0421-1 ↗
34. Enhanced anodization growth of self-organized ZrO2 nanotubes on nanostructured zirconium10.1016/j.surfcoat.2010.10.058 ↗
35. Effect of liquid spreading due to nano/microstructures on the critical heat flux during pool boiling10.1063/1.3555430 ↗
36. Pool boiling CHF enhancement by micro/nanoscale modification of zircaloy-4 surface10.1016/j.nucengdes.2010.07.006 ↗
37. The role of surface energy in heterogeneous bubble growth on ideal surface10.1016/j.ijheatmasstransfer.2016.10.005 ↗
38. Induced liquid-solid contact via micro/nano multiscale texture on a surface and its effect on the Leidenfrost temperature10.1016/j.expthermflusci.2017.01.022 ↗
39. Droplet impact and LFP on wettability and nanostructured surface10.1016/j.expthermflusci.2018.07.029 ↗
40. Experimental study of water droplets on over-heated nano/microstructured zirconium surfaces10.1016/j.nucengdes.2014.06.042 ↗
41. Formation of self-organized Zircaloy-4 oxide nanotubes in organic viscous electrolyte via anodization10.1186/1556-276X-9-553 ↗
42. Fabrication of uniform nanoporous oxide layers on long cylindrical zircaloy tubes by anodization using multi-counter electrodes10.1186/s11671-016-1774-1 ↗
43. Zirconium oxide nanotubes synthesized via direct electrochemical anodization10.1149/1.1857115 ↗
44. Fabrication and characterization of smooth high aspect ratio zirconia nanotubes10.1016/j.cplett.2005.05.065 ↗
45. Self-organized high-aspect-ratio nanoporous zirconium oxides prepared by electrochemical anodization10.1002/smll.200400163 ↗
46. Titanium oxide nanotube arrays prepared by anodic oxidation10.1557/JMR.2001.0457 ↗
47. Dynamics of water droplet on a heated nanotubes surface10.1063/1.4809944 ↗
48. Film boiling heat transfer on a completely wettable surface with atmospheric saturated distilled water quenching10.1016/j.ijheatmasstransfer.2015.09.049 ↗
49. Evolution of multilayered scale structures during high temperature oxidation of ZrSi210.1557/jmr.2016.363 ↗
50. Kinetic model of the oxidation of ZrSi2 powders10.1007/s10973-007-8461-5 ↗
51. Effect of applied voltage and fluoride ion content on the formation of zirconia nanotube arrays by anodic oxidation of zirconium10.1016/j.corsci.2010.11.044 ↗
52. Ionic transport in amorphous anodic titania stabilised by incorporation of silicon species10.1016/S0010-938X(01)00111-1 ↗
53. Controlled fabrication of nanoporous oxide layers on zircaloy by anodization10.1186/s11671-015-1086-x ↗
54. Formation of hexagonally-ordered zircaloy oxide nanostructures with different morphologies using two-step anodization10.1016/j.jallcom.2015.03.214 ↗
55. W. Lee, R. Ji, U. Gösele, K.N.-N. materials, undefined 2006, Fast fabrication of long-range ordered porous alumina membranes by hard anodization, Nature.Com. (n.d.). https://www.nature.com/articles/nmat1717 (accessed March 22, 2019).
56. X. Zhao, W. Zhang, Y. Wang, Q. Liu, J. Yang, … L.Z.-A.S., undefined 2019, Fabrication of Al2O3 by Anodic Oxidation and Hydrothermal Synthesis of Strong-bonding Hydroxyapatite Coatings on its Surface, Elsevier. (n.d.). https://www.sciencedirect.com/science/article/pii/S0169433218332938 (accessed March 22, 2019).10.1016/j.apsusc.2018.11.216 ↗
57. The effect of electrolyte composition on the fabrication of self-organized titanium oxide nanotube arrays by anodic oxidation10.1557/JMR.2005.0020 ↗
58. Fast-rate formation of TiO2 nanotube arrays in an organic bath and their applications in photocatalysis10.1088/0957-4484/21/36/365603 ↗
59. High-temperature and electrochemical oxidation of transition metal silicides10.1007/s11106-009-9124-9 ↗
60. Low temperature formation of insulating layers on silicides by anodic oxidation10.1016/0038-1101(87)90131-6 ↗
61. The structure of plasma-deposited and annealed pseudo-binary ZrO2-SiO2 alloys10.1557/PROC-611-C1.3.1 ↗
62. Microscopic model for enhanced dielectric constants in low concentration SiO2-rich noncrystalline Zr and Hf silicate alloys10.1063/1.1320860 ↗
63. Wicking and spreading of water droplets on nanotubes10.1021/la204073n ↗