Abstract
Abstract The (Ba 0.75 Sr 0.25 )(Zr 0.25 Ti 0.75 )O 3 (BSZT) thin films were grown on (100) SrTiO 3 :1.0 wt.% Nb single crystal substrates by pulsed laser deposition. Highly (001)-oriented BSZT films were achieved. The thickness of as-grown thin films was measured by a surface profiler and was found to be ~ 600 nm. The crystalline structure of the BSZT thin films on (100) SrTiO 3 :Nb substrate was analyzed by an X-ray diffractometer (XRD). The surface morphology and roughness were determined by an atomic force microscopy (AFM) using tapping mode amplitude modulation. The films exhibited a clustered grains characteristic of the grains with size of 80–120 nm. The dielectric properties of Pt/BSZT/SrTiO 3 :Nb capacitors were measured by using an Agilent 4294A impedance analyzers at room temperature. The dielectric constant of BSZT film changes significantly with applied dc bias field and has a high tunability of ~ 44% at an applied field of 600 kV/cm.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Ferroelectric and Piezoelectric Materials · Microwave Dielectric Ceramics Synthesis · Acoustic Wave Resonator Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (18)
Show source-provided references
1. Li · IEEE Trans. Ultrason. Ferroelectr. Freq. Control · 2011 · 58 · 1140
2. Tang · Appl. Phys. A: Mater. Sci. Proc. · 2005 · 81 · 125310.1007/s00339-004-2980-8 ↗
3. Li · Surf. Coat. Tech. · 2011 · 205 · 298910.1016/j.surfcoat.2010.11.009 ↗
4. Zhai · Appl. Phys. Lett. · 2004 · 84 · 313610.1063/1.1715152 ↗
5. Hennings · J. Am. Ceram. Soc. · 1982 · 65 · 53910.1111/j.1151-2916.1982.tb10778.x ↗
6. Weber · J. Am. Ceram. Soc. · 2001 · 84 · 75910.1111/j.1151-2916.2001.tb00738.x ↗
7. Yu · Appl. Phys. Lett. · 2002 · 81 · 128510.1063/1.1498496 ↗
8. Tang · Solid State Commun. · 2004 · 131 · 16310.1016/j.ssc.2004.05.016 ↗
9. Joseph · J. Phys. D: Appl. Phys. · 1999 · 32 · 104910.1088/0022-3727/32/9/317 ↗
10. Tang · Solid State Commun. · 2005 · 136 · 8910.1016/j.ssc.2005.06.034 ↗
11. Joseph · Jpn. J. Appl. Phys. · 1996 · 1 · 17910.1143/JJAP.35.179 ↗
12. Yang · Jpn. J. Appl. Phys. · 1997 · 1 · 18810.1143/JJAP.36.188 ↗
13. Kim · J. Vac. Sci. Technol. B · 2000 · 18 · 21610.1116/1.591175 ↗
14. Tang · J. Crystal Growth · 2005 · 276 · 45310.1016/j.jcrysgro.2004.11.389 ↗
15. Choy · Integr. Ferroelectr. · 2006 · 80 · 10710.1080/10584580600656601 ↗
16. Xia · Appl. Phys. Lett. · 2007 · 91 · 10290410.1063/1.2780083 ↗
17. Fan · Thin Solid Films · 2010 · 518 · 361010.1016/j.tsf.2009.09.051 ↗
18. Tang · Surf. Coat. Tech. · 2002 · 161 · 16910.1016/S0257-8972(02)00520-0 ↗