Wet oxidation of Ti34Si23N43 thin films with and without pre-annealing
Source abstract
Abstract
Abstract Films of a ternary alloy of composition Ti 34 Si 23 N 43 and of a structure consisting of homogeneously distributed ∼2 nm sized TiN-like grains in an amorphous matrix were deposited by reactive magnetron sputtering to thicknesses of 250–1000 nm and then oxidized with steam at 600, 800, or 1000°C, with and without first annealing the film in vacuum at 800°C for 1 h. The microstructure of the nitride and the oxide was analyzed by X-ray diffraction and plan-view transmission electron microscopy. The thickness of the grown oxide scale was monitored by backscattering spectrometry. At 600 and 800°C, the oxide scale has the composition of Ti 20 Si 13 O 67 , corresponding to a full and lossless oxidation of Ti and Si to TiO 2 and SiO 2 . During that process, the nano-grains in the alloy grow several-fold. The oxide is also a two-phase mixture of TiO 2 nano-grains in an amorphous matrix. As a function of the oxidation duration, t , the oxide grows in a log( t )-like fashion. Pre-annealing in vacuum reproduces the growth of TiN grains in the alloy observed during oxidation. This structural change does not alter the log( t )-type dependence but drastically reduces the rate of oxidation. The observations are interpreted as resulting from the compositional changes of the matrix induced by the growth of the TiN grains in the alloy.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Advanced ceramic materials synthesis · MXene and MAX Phase Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. Posadowski · Thin Solid Films · 1988 · 162 · 11110.1016/0040-6090(88)90199-X ↗
2. Onodera · IEEE Electron. Dev. Lett. EDL · 1988 · 9 · 41710.1109/55.763 ↗
3. Asai · J. Vac. Sci. Technol. B · 1988 · 6 · 152610.1116/1.584207 ↗
4. Kolawa · J. Vac. Sci. Technol. A · 1990 · 8 · 300610.1116/1.576620 ↗
5. Li · Plasma Chem. Plasma Process. · 1992 · 12 · 28710.1007/BF01447027 ↗
6. Dauksher · J. Vac. Sci. Technol. B · 1995 · 13 · 310310.1116/1.588331 ↗
7. Linder · Sensors and Actuators A · 1997 · 61 · 38710.1016/S0924-4247(97)80294-4 ↗
8. de Reus · Microelectronics Reliability · 1998 · 38 · 125110.1016/S0026-2714(98)00149-8 ↗
9. Kacsich · J. Appl. Phys. · 1999 · 85 · 187110.1063/1.369342 ↗
10. Kacsich · Thin Solid Films · 1999 · 349 · 110.1016/S0040-6090(99)00178-9 ↗
11. Sun · J. Appl. Phys. · 1997 · 81 · 65610.1063/1.364133 ↗
12. Doolittle · Nucl. Instrum. Meth. B · 1985 · 9 · 34410.1016/0168-583X(85)90762-1 ↗
13. Cullity · 1978
14. Deal · J. Appl. Phys. · 1965 · 36 · 377310.1063/1.1713945 ↗
15. Davies · Proc. R. Soc. A · 1954 · 225 · 44310.1098/rspa.1954.0214 ↗
16. Suni · J. Electrochem. Soc. · 1983 · 130 · 121010.1149/1.2119919 ↗
17. Habraken · Mater. Sci. Eng. R · 1994 · 12 · 12310.1016/0927-796X(94)90006-X ↗
18. Fourrier · J. Electrochem. Soc. · 1991 · 138 · 108410.1149/1.2085720 ↗
19. Pokela · J. Appl. Phys. · 1991 · 70 · 282810.1063/1.349345 ↗
20. Suni · J. Electrochem. Soc. · 1983 · 130 · 121010.1149/1.2119919 ↗
21. Deal · J. Appl. Phys. · 1965 · 36 · 377010.1063/1.1713945 ↗
22. Veprek · J. Electrochem. Soc. · 1996 · 96-5 · 619
23. Veprek · Surf. Coat. Technol. · 1996 · 86–87 · 39410.1016/S0257-8972(96)02988-X ↗
24. Diserens · Surf. Coat. Technol. · 1999 · 120–121 · 15810.1016/S0257-8972(99)00481-8 ↗
25. Grill · J. Mater. Res. · 1999 · 14 · 160410.1557/JMR.1999.0215 ↗
26. Veprek · Thin Solid Films · 1998 · 317 · 44910.1016/S0040-6090(97)00665-2 ↗