journal article·2025-06Open access

Unravelling the potential of non-reactively sputtered (Ti,Al)N coatings

Balint Istvan Hajas, Sarah Christine Bermanschläger, Alexander Kirnbauer, Tomasz Wojcik, Szilard Kolozsvári, Paul Heinz Mayrhofer

Abstract

Non-reactive magnetron sputtering was used to synthesize (Ti,Al)N coatings from a TiN/AlN (50 % AlN) composite target, with a detailed investigation into how process parameters influence phase formation, hardness, and thermal stability. Optimizing pulse parameters, such as increasing reverse pulse on-time ( t on-r ) to 8016 ns or pulse frequency ( f p ) to 250 kHz, effectively suppressed the hcp phase observed under reference conditions ( f p = 50 kHz, t on- r = 496 ns, substrate temperatures T s = 600 °C, sputter power density P t = 8.6 W/cm 2 , substrate bias U b = −50 V). Lower T s (≤ 450 °C) or P t (3.4 W/cm 2 ) also mitigate hcp phase formation, while higher T s or P t (up to 18.6 W/cm 2 ) amplified it. Similarly, increasing U b to −100 V allows to prepare single-phase fcc structured (Ti,Al)N with H up to 39.8 ± 2.1 GPa. By adding 5–10 % N 2 to the Ar working gas, the hcp phase formation can be avoided, achieving coatings with H = 38.3 ± 1.4 GPa. Detailed in-situ XRD as well as TEM studies reveal that coatings with a single-phase fcc structure provide a superior thermal stability during vacuum annealing treatments, particularly those deposited with U b = −100 V. These retain their fcc structure up to 1100 °C and reach 44.7 ± 2.3 GPa through age hardening. This study underscores the critical role of suppressing hcp phase formation to enhance both hardness and thermal stability. Optimizing deposition parameters enables the tailoring of (Ti,Al)N coatings for demanding high-temperature applications. • Single- and multiphase (TiAl)N coatings produced by non-reactive sputtering • Highest hardness H = 39.8 GPa observed in single phase fcc coating • Age hardening leads to H = 44.7 GPa after annealing at 1100 °C • Annealing at 1200 °C leads to significant decrease in hardness for all samples
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Semiconductor materials and devices · Diamond and Carbon-based Materials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (35)

Show source-provided references
1. High rate thick film growth
2. Titanium nitride PVD coating technology10.1179/sur.1985.1.2.93 ↗
3. R.F. reactively sputtered TiN: Characterization and adhesion to materials of technical interest10.1016/0040-6090(84)90379-1 ↗
4. First-principles study of the effect of nitrogen vacancies on the decomposition pattern in cubic Ti(1-x)Al(x)N(1-y)
5. Titanium aluminum nitride films: a new alternative to TiN coatings10.1116/1.573713 ↗
6. Self-organized nanostructures in the Ti-Al-N system10.1063/1.1608464 ↗
7. Thermal stability of arc evaporated high aluminum-content Ti1-xAlxN thin films
8. Materials science-based guidelines to develop robust hard thin film materials10.1016/j.pmatsci.2024.101323 ↗
9. Fundamental aspects in non-reactive and reactive magnetron discharges10.1088/0963-0252/12/4/318 ↗
10. Vacancy hardening in single-crystal TiN(x)(001) layers10.1063/1.1568521 ↗
11. Recent developments in plasma assisted physical vapour deposition10.1088/0022-3727/33/18/201 ↗
12. Influence of bipolar pulsed DC magnetron sputtering on elemental composition and10.1016/j.surfcoat.2008.08.042 ↗
13. Structure, chemistry, and mechanical properties of non-reactively sputtered Ti-Al-N10.1016/j.matdes.2025.113803 ↗
14. Influence of oxygen impurities on growth morphology, structure and mechanical properties of Ti–Al–N thin films10.1016/j.tsf.2016.01.039 ↗
15. Decomposition pathways in age hardening of Ti-Al-N films
16. Effect of internal interfaces on hardness and thermal stability of Nanocrystalline Ti0.5Al0.5N coatings10.1007/s11661-010-0204-8 ↗
17. Thermal stability and oxidation resistance of Ti–Al–N coatings10.1016/j.surfcoat.2011.12.028 ↗
18. Chapter 5 - the low pressure plasma processing environment
19. In situ site-specific specimen preparation for atom probe tomography10.1016/j.ultramic.2006.06.008 ↗
20. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
21. Effects of nitrogen flow rate on the microstructure and mechanical and tribological properties of TiAlN films prepared via reactive magnetron sputtering10.1016/j.ceramint.2023.03.108 ↗
22. Phase formation and mechanical properties of reactively and non-reactively sputtered Ti-B-N hard coatings10.1016/j.surfcoat.2021.127327 ↗
23. Microstructural control of TiC/a-C nanocomposite coatings10.1016/j.actamat.2007.10.025 ↗
24. Time-averaged and time-resolved ion fluxes related to reactive HiPIMS deposition of Ti-Al-N films10.1016/j.surfcoat.2021.127638 ↗
25. Strain evolution during spinodal decomposition of TiAlN thin films10.1016/j.tsf.2012.04.059 ↗
26. Phase stability and elasticity of TiAlN10.3390/ma4091599 ↗
27. Unprecedented thermal stability of inherently metastable titanium aluminum nitride by point defect engineering10.1080/21663831.2016.1233914 ↗
28. Ar + H2 plasma etching for improved adhesion of PVD coatings on steel substrates10.1016/j.vacuum.2011.10.028 ↗
29. Influence of varying nitrogen partial pressures on microstructure, mechanical and optical properties of sputtered TiAlON coatings10.1016/j.actamat.2016.08.007 ↗
31. Effect of nitrogen partial pressure on characteristic and mechanical properties of hard coating TiAlN film
32. Martínez-Martínez · 2016
33. Influence of substrate bias voltage on microstructure and mechanical characteristics of TiAlSiN coating deposited by high power impulse magnetron sputtering (HiPIMS)10.1016/j.surfcoat.2023.129351 ↗
34. Surface characteristics for the TiAlN coatings deposited by high power impulse magnetron sputtering technique at the different bias voltages10.1016/j.jallcom.2016.07.013 ↗
35. Spectral evidence of spinodal decomposition, phase transformation and molecular nitrogen formation in supersaturated TiAlN films upon annealing10.1016/j.actamat.2011.06.039 ↗