journal article·2025-09Open access

Laser surface treatment of WSC coatings for selective crystallization of the TMD phase

Jorge Caessa, Albano Cavaleiro, E.L. Silva, Todor Vuchkov

Abstract

Low friction in WSC coatings—comprising a WS 2 phase embedded within an amorphous carbon matrix—relies on sliding-induced WS 2 crystallization, process that typically requires prolonged running-in periods. Laser treatments can alternatively induce WS 2 crystallization prior to sliding, without compromising the structural integrity of the amorphous carbon matrix. However, current laser processing approaches are often imprecise and lack systematic optimization of the process parameters, as most research focuses on material ablation and topography modification, rather than structural transformations. This study systematically optimized the laser treatment of WSC coatings (~50 at. % C) under near-ideal conditions (WSCIR1-WSCIR3) to identify key variables and thresholds governing WS 2 phase crystallization and amorphous carbon graphitization. We adjusted laser parameters—average power, pulse duration, and repetition rate—and refined derived quantities such as energy per pulse, fluence, and power density. Geometrical, structural, and mechanical changes to the WSC coatings were then analyzed using optical microscopy, profilometry, ball cratering, Raman spectroscopy, X-ray diffraction, and nanoindentation. Increased laser exposure darkened and expanded the dimensions (diameter, height, depth) of the treated zones, and enhanced WS 2 crystallization—while maintaining coating hardness and elastic modulus due to minimal amorphous carbon graphitization. Our findings establish critical thresholds and present a precise, scalable pathway for engineering WSC coatings, potentially eliminating the need for extended running-in periods.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research · High-Temperature Coating Behaviors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (73)

Show source-provided references
1. Bilateral phonon transport modulation of Bi-layer TMDCs (MX2, M=Mo, W; X=S)10.1016/j.ijthermalsci.2022.107669 ↗
2. Synergetic effects of surface texturing and solid lubricants to tailor friction and wear – a review10.1016/j.triboint.2020.106792 ↗
3. Synthesis and structural properties of Mo-Se-C sputtered coatings10.1016/j.surfcoat.2007.08.019 ↗
4. Comparative study of the tribological behavior of self-lubricating W-S-C and Mo-Se-C sputtered coatings10.1016/j.wear.2008.04.011 ↗
5. Synthesis and properties of W-Se-C coatings deposited by PVD in reactive and non-reactive processes10.1016/j.vacuum.2009.03.030 ↗
6. Friction of self-lubricating W-S-C sputtered coatings sliding under increasing load10.1002/ppap.200731402 ↗
7. The tribological behavior of W-S-C films in pin-on-disk testing at elevated temperature10.1016/j.vacuum.2007.04.010 ↗
8. Tribological behaviour of C-alloyed transition metal dichalcogenides (TMD) coatings in different environments10.1007/s10999-007-9034-2 ↗
9. Self-lubricating W-S-C nanocomposite coatings
10. A revised interpretation of the mechanisms governing low friction tribolayer formation in alloyed-TMD self-lubricating coatings
11. On the microstructural, mechanical and tribological properties of Mo-Se-C coatings and their potential for friction reduction against rubber10.3390/ma14061336 ↗
12. Influence of laser structural patterning on the tribological performance of C-alloyed W-S coatings10.1016/j.surfcoat.2020.125822 ↗
13. Combining multi-scale surface texturing and DLC coatings for improved tribological performance of 3D printed polymers10.1016/j.surfcoat.2023.129682 ↗
14. Bio-inspired functional surfaces based on laser-induced periodic surface structures10.3390/ma9060476 ↗
15. Laser engineering of biomimetic surfaces10.1016/j.mser.2020.100562 ↗
16. Laser surface texturing of materials for surface functionalization: a holistic review10.1016/j.surfcoat.2025.131818 ↗
17. Use of the roughness parameters Ssk and Sku to control friction—a method for designing surface texturing10.1080/10402004.2016.1159358 ↗
18. A critical assessment of surface texturing for friction and wear improvement10.1016/j.wear.2016.11.020 ↗
19. Laser surface texturing and related techniques for enhancing tribological performance of engineering materials: a review10.1016/j.jmapro.2020.02.009 ↗
20. Nonlinear optics of two-dimensional transition metal dichalcogenides10.1002/inf2.12024 ↗
21. Optical limiting and theoretical modelling of layered transition metal dichalcogenide nanosheets10.1038/srep14646 ↗
22. Temperature-dependent optical constants of monolayer MoS2, MoSe2, WS2, and WSe2: spectroscopic ellipsometry and first-principles calculations
23. Surface Characteristics of Polymers with Different Absorbance after UV Picosecond Pulsed Laser Processing Using Various Repetition Rates10.3390/polym12092018 ↗
24. The Effect of Laser Pulse Widths on Laser—Ag Nanoparticle Interaction: Femto- to Nanosecond Lasers10.3390/app8010112 ↗
25. S. Parker, Laser: Tissue Interaction and Its Application, Clinical Dentistry International Journal of Laser Dentistry 1 1–8. doi:https://doi.org/10.5005/jp-journals-10022-1001.10.5005/jp-journals-10022-1001 ↗
26. Physical principles of LASER10.1016/j.mpaic.2014.08.003 ↗
27. A review on the research progress of tailoring photoluminescence of monolayer transition metal dichalcogenides10.1016/j.flatc.2017.07.001 ↗
28. Electronic and optical properties of ultra-thin 2D tungsten disulfide for photovoltaic applications10.1016/j.solmat.2017.09.011 ↗
29. Laser beam intensity and wavelength dependent nonlinear absorption in pulse laser deposited WS2 thin films
30. Standing growth mechanism and ultrafast nonlinear absorption properties of WS2 films10.1016/j.optmat.2020.109995 ↗
31. Highest optical gap tetrahedral amorphous carbon10.1016/S0925-9635(01)00591-X ↗
32. Microstructure and optical band gap control of DLC film deposited by pulsed discharge plasma CVD10.1016/j.diamond.2007.08.018 ↗
33. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
34. On the tribological performance of laser-treated self-lubricating thin films in contact with rubber10.1016/j.triboint.2022.107758 ↗
35. Laser-induced graphitized periodic surface structure formed on tetrahedral amorphous carbon films10.1016/j.diamond.2020.107909 ↗
36. Effect of initial sp3 content on bonding structure evolution of amorphous carbon upon pulsed laser annealing10.1016/j.diamond.2012.09.008 ↗
37. Laser treatment of tribological DLC films10.1016/S0925-9635(02)00372-2 ↗
38. Effects of pulse duration in laser processing of diamond-like carbon films10.1016/j.diamond.2005.02.009 ↗
39. Physics of ultra-short laser interaction with matter: from phonon excitation to ultimate transformations10.1016/j.pquantelec.2013.05.001 ↗
40. Identification of individual and few layers of WS2 using Raman Spectroscopy
41. In-situ monitoring of thermal annealing induced evolution in film morphology and film-substrate bonding in a monolayer MoS2 film
42. Laser light induced transformation of molybdenum disulphide-based nanoplatelet arrays10.1038/srep37514 ↗
43. The wettability and tribological behaviour of thin F-doped WS2 films deposited by magnetron sputtering10.1016/j.surfcoat.2019.125033 ↗
44. Comparative study of DC and RF sputtered MoSe2 coatings containing carbon—An approach to optimize stoichiometry, microstructure, crystallinity and hardness10.3390/coatings10020133 ↗
45. Effect of heat treatment on mechanical property of amorphous carbon films by magnetron sputtering10.1016/j.diamond.2022.109328 ↗
46. The effect of CO2 addition to the (C2H2 + H2) gas system on the low-temperature growth of diamond-like carbon (DLC) with prominent nano-diamond phase10.1016/j.matpr.2022.02.396 ↗
47. Interpretation of Raman spectra of disordered and amorphous carbon10.1103/PhysRevB.61.14095 ↗
48. Laser flash synthesis of graphene and its inorganic analogues: An innovative breakthrough with immense promise10.1039/c3ra41149d ↗
49. Graphitization and amorphization of textured carbon using high-energy nanosecond laser pulses10.1016/j.carbon.2016.04.026 ↗
50. Tribological behavior of diamond-like carbon thin films deposited by the pulse laser technique at different substrate temperatures10.1016/j.triboint.2016.07.013 ↗
51. Study of CVD diamond layers with amorphous carbon admixture by Raman scattering spectroscopy10.1515/msp-2015-0067 ↗
52. Multipeak fitting analysis of Raman spectra on DLCH film10.1002/jrs.2234 ↗
53. Role of laser power, wavelength, and pulse duration in laser assisted tin-induced crystallization of amorphous silicon10.1155/2018/1243685 ↗
54. Modification of the amorphous carbon films by the ns-laser irradiation
55. Laser-induced excitation mechanisms and phase transitions in spectrochemical analysis – review of the fundamentals10.1016/j.sab.2021.106091 ↗
56. In-situ thermal stability analysis of amorphous carbon films with different sp3 content10.1016/j.carbon.2018.01.034 ↗
57. Synthesis of vertically stacked, highly oriented WS2 thin films by Electron beam evaporation10.1016/j.tsf.2021.138851 ↗
58. Tribological behavior of RF sputtering WS2 thin films with vacuum annealing10.1016/j.phpro.2011.06.091 ↗
59. Rai · 2019
60. Laser direct growth of graphene on silicon substrate10.1063/1.3675636 ↗
61. Surface and friction characterization of MoS2 and WS2 third body thin films under simulated wheel/rail rolling–sliding contact10.1016/j.wear.2007.04.004 ↗
62. Growth, structure and friction behavior of titanium doped tungsten disulphide (Ti-WS2) nanocomposite thin films10.1016/j.tsf.2009.02.103 ↗
63. Influence of composition, structure and testing atmosphere on the tribological performance of W-S-N coatings10.1016/j.surfcoat.2014.09.061 ↗
64. Nanosecond pulsed laser-generated stress effect inducing macro-micro-nano structures and surface topography evolution10.1016/j.apmt.2019.01.005 ↗
65. The effect of substrate location on the composition, microstructure and mechano-tribological properties of W-S-C coatings deposited by magnetron sputtering10.1016/j.surfcoat.2020.125481 ↗
66. Tribological study of W-S-(C) sputtered coatings sliding against aluminium at elevated temperatures10.1016/j.surfcoat.2024.130750 ↗
67. On the tribological performance of magnetron sputtered W-S-C coatings with conventional and graded composition10.1016/j.surfcoat.2022.128929 ↗
68. Direct laser interference patterning of tetrahedral amorphous carbon films for tribological applications10.1016/j.diamond.2012.12.002 ↗
69. Self-healing WS2 tribofilms: An in-situ appraisal of mechanisms10.1016/j.scriptamat.2021.114124 ↗
70. The role of laser pulse overlap in ultrafast thin film structuring applications10.1007/s00339-018-2045-z ↗
71. Effects of annealing temperature on the microstructure, mechanical and tribological properties of CrAlTiN coatings
72. Effects of substrate temperature on bonding structure and mechanical properties of amorphous carbon films10.1016/S0040-6090(03)01076-9 ↗
73. Historical developments and new trends in tribological and solid lubricant coatings10.1016/j.surfcoat.2003.10.022 ↗