journal article·2025-12Open access

Effect of seawater flow velocity on the damage tolerance of thermally sprayed aluminium coatings

Adriana Castro-Vargas, Shiladitya Paul

Abstract

This work focuses on the effect of seawater flow velocity on the corrosion performance of Thermally Sprayed Aluminium (TSA) Coating obtained by twin-wire arc spraying. Hollow cylindrical coupons were machined from an S355 steel rod and coated with 300 μm-thick TSA (AA 1050). An intentional defect was machined on the outer surface to expose the substrate. Polarisation Resistance (PR) measurements were carried out to calculate the corrosion rate. Open Circuit Potential (OCP) was also monitored. An analytical rotator was employed for testing TSA-coated steel cylindrical coupons without and with damage at 50 rpm (3 cm/s), 600 rpm (38 cm/s) and 1000 rpm (63 cm/s) for 10 days in synthetic seawater (SSW) at 18 ± 2 °C. Tests under stagnant conditions were also conducted. SEM examination and Raman spectroscopy identified calcareous deposits on the exposed steel and Al oxides/hydroxides on the coating. Removal of aluminium corrosion products from the coupon surface due to the SSW flow exposes fresh coating surfaces to the electrolyte, increasing the coating corrosion rate. Hydrodynamic conditions strongly influenced the composition and precipitation rate of the calcareous deposits on the exposed steel in TSA-coated steel with intentional damage. After testing, the exposed steel had limited clusters of calcareous deposits. Aluminium is consumed to protect the exposed steel, while the flow enhances oxygen availability at the coating surface. • OCP variations in TSA without damage result from seawater flow removing aluminium corrosion products. • The removal of aluminium corrosion products exposes a fresh coating surface, which accelerates the corrosion rate. • Seawater flow velocity, intentional damage, and limited calcareous deposits resulted in a high corrosion rate in TSA. • The damage tolerance of TSA relies on the precipitation rate, stability, and type of calcareous deposits on the exposed steel. • TSA consumption by galvanic action will continue until calcareous deposits form, limiting oxygen reduction in the defect.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Corrosion Behavior and Inhibition · Erosion and Abrasive Machining

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (49)

Show source-provided references
1. The expected dynamics of the European offshore wind sector in the climate change context10.3390/jmse11101967 ↗
2. WindEurope
3. Review of the current status, technology and future trends of offshore wind farms10.1016/j.oceaneng.2020.107381 ↗
4. Metallic coatings in offshore wind sector—a mini review10.1038/s41529-024-00480-8 ↗
5. DNV, DNVGL-RP-0416 · 2016
6. DNV, DNV-ST-0119 · 2021
7. ISO, ISO/WD 25249. Corrosion protection of offshore wind structures, (Under development).
8. Use of thermally sprayed aluminium (TSA) coatings to protect offshore structures in submerged and splash zones10.1016/j.surfcoat.2019.04.048 ↗
9. Prediction of thermal spray coatings performance in marine environments by combination of laboratory and field tests10.3390/coatings11030320 ↗
10. In-situ imaging and electrochemical monitoring of damaged thermal spray aluminium coating in synthetic seawater10.1016/j.electacta.2023.142847 ↗
11. Effect of damage on the corrosion performance of Thermal Spray Aluminium (TSA) coating in synthetic seawater10.3390/app13021109 ↗
12. Sacrificial thermally sprayed aluminium coatings for marine environments: a review10.3390/coatings10030267 ↗
13. Veritas · 2010
14. Effect of seawater constituents on the performance of thermal spray aluminum in marine environments10.1002/maco.201810764 ↗
15. Assessing extreme environmental loads on offshore structures in the North Sea from high-resolution ocean currents, waves and wind forecasting10.3390/jmse9101052 ↗
16. Corrosion of thermally sprayed aluminum in flowing seawater
17. Preparation of steel substrates before application of paints and related products. Visual assessment of surface cleanliness
18. Paul · 2015 · 321
19. ASTM · 2021
20. Baboian · 2002
21. Determination of the corrosion rate of thermally spayed aluminum (TSA) in simulated marine service, OnePetro
22. Comparing cold spray with thermal spray coating technologies
23. Beyond traditional coatings: a review on thermal-sprayed functional and smart coatings10.1007/s11666-019-00857-1 ↗
24. Electrochemical calcareous deposition in seawater. A review10.1007/s10311-020-01002-z ↗
25. Role of hydrate phases of calcium carbonate on the scaling phenomenon10.1016/S0011-9164(01)00216-8 ↗
26. Novel inorganic membranes based on magnetite-containing silica porous glasses for ultrafiltration: structure and sorption properties10.3390/membranes13030341 ↗
27. Raman microspectroscopy of some iron oxides and oxyhydroxides10.1002/(SICI)1097-4555(199711)28:11<873::AID-JRS177>3.0.CO;2-B ↗
28. A study of calcareous deposits on cathodically protected mild steel in artificial seawater10.3390/met5010439 ↗
29. Appendix VI - Raman bands sorted by name
30. A Raman and infrared spectroscopic study of the sulphate mineral aluminite Al2 (SO4)(OH)4· 7H2O10.1016/j.saa.2015.04.011 ↗
31. Native alunogen: a Raman spectroscopic study of a well-described specimen10.1016/j.molstruc.2017.12.021 ↗
32. Comparison of Raman spectra in characterizing gibbsite, bayerite, diaspore and boehmite10.1002/jrs.736 ↗
33. New insight into the preferred valency of interlayer anions in hydrotalcite-like compounds: the effect of Mg/Al ratio10.1016/j.clay.2018.01.013 ↗
34. Raman spectroscopy of hydrotalcites with sulphate, molybdate and chromate in the interlayer10.1002/jrs.1385 ↗
35. Study of cathodic reactions in defects of thermal spray aluminium coatings on steel in artificial seawater10.1016/j.corsci.2021.109514 ↗
36. Raman spectroscopy of high salinity brines and ices10.1016/j.icarus.2021.114759 ↗
37. Chemistry, electrochemistry,and electrochemical applications. aluminum
38. 9 - corrosion and protection of aluminum alloys in seawater
39. Anodic alloys degradation exposed to different flow conditions in natural seawater10.1149/1.3268413 ↗
40. Quevedo · 2008
41. Characterization of calcareous deposits in artificial sea water by impedance techniques—I. Deposit of CaCO3 without Mg(OH)210.1016/S0013-4686(97)00303-4 ↗
42. Characterization of calcareous deposits in artificial sea water by impedances techniques: 2-deposit of Mg (OH)2 without CaCO310.1016/S0013-4686(99)00403-X ↗
43. Calcareous scales formed by cathodic protection—an assessment of characteristics and kinetics10.1016/S0022-0248(02)01532-4 ↗
44. Characterization of calcareous deposits in artificial seawater by impedance techniques: 3—deposit of CaCO3 in the presence of Mg (II)10.1016/S0013-4686(03)00075-6 ↗
45. Natural deposit coatings on steel during cathodic protection and hydrogen ingress10.3390/coatings5040816 ↗
46. Mechanistic insights into electrodeposition in seawater at variable electrochemical potentials
47. Khudsen
48. Kinetics and characterisation of calcareous deposits under cathodic protection in natural sea water10.4028/www.scientific.net/MSF.289-292.1163 ↗
49. Electrochemical scaling of stainless steel in artificial seawater: role of experimental conditions on CaCO3 and Mg (OH)2 formation10.1016/j.desal.2012.07.011 ↗