Surface smoothing and periodic microstructuring of additively manufactured scalmalloy® by sequential continuous-wave polishing and direct laser interference patterning
Source abstract
Abstract
Laser Powder Bed Fusion is gaining industrial prominence due to its ability to create complex parts with reduced material waste. Scalmalloy® stands out as a possible replacement for titanium, offering high strength and thermal conductivity while maintaining low component weight. Nevertheless, parts produced by this method normally exhibit high surface roughness, characterized by partially melted particles and surface irregularities. In addition, low surface roughness is also a prerequisite for the further fabrication of well-defined microstructures that can enhance surface functions based on mimicking natural examples. This work combines surface smoothing by continuous-wave laser re-melting with the fabrication of periodic textures using Direct Laser Interference Patterning to tailor surface topography. Initial laser polishing trials achieve a substantial reduction of as-built Ra roughness from approximately (Ra) ~14 μm to 1–2 μm but generated subsurface pores. The porosity is mitigated by adjusting laser power and feed rate. The polished samples are subsequently microstructured by DLIP using a picosecond pulsed laser, producing structure depths up to 3.0 μm with a homogeneity of approximately 82%. Finally, the performance of the combined process is analyzed in terms of energy consumption and target surface parameters to improve process sustainability. • CW laser polishing reduces Scalmalloy surface roughness from ~14 μm to ~1.5–2 μm at low cumulative fluence. • Subsurface porosity forms in Scalmalloy® at high laser power during polishing. • DLIP using a picosecond pulsed laser produces 6 μm-period line textures with depths up to ~3 μm and ~80% homogeneity on polished surfaces. • Pattern quality deteriorates when the pulse-to-pulse overlap during DLIP exceeds ~99%. • A multi-objective cost function enables energy-based selection of parameters for sequential laser polishing and DLIP.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Laser Material Processing Techniques · Laser-Ablation Synthesis of Nanoparticles
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (64)
Show source-provided references
1. A review on metal additive manufacturing for intricately shaped aerospace components10.1016/j.cirpj.2022.07.005 ↗
2. A review of technological improvements in laser-based powder bed fusion of metal printers10.1007/s00170-020-05361-3 ↗
3. Laser powder bed fusion of aluminum, titanium and nickel-based alloys: materials and design investigations
4. A methodology for the rapid qualification of additively manufactured materials based on pore defect structures10.1007/s40192-024-00343-9 ↗
5. Metal additive manufacturing in aerospace: a review10.1016/j.matdes.2021.110008 ↗
6. New aluminum alloys specifically designed for laser powder bed fusion: a review10.3390/ma12071007 ↗
7. High-performance aluminum-based materials processed by laser powder bed fusion: process, microstructure, defects and properties coordination
8. Microstructure and mechanical property considerations in additive manufacturing of aluminum alloys10.1557/mrs.2016.214 ↗
9. Development and applications of aluminum alloys for aerospace industry10.1016/j.jmrt.2023.09.274 ↗
10. Palm · 2006
11. Additive manufacturing of Scalmalloy ® satellite parts
12. Effect of powder spreading parameters on laser absorption behavior and processability of high-strength aluminum alloy fabricated by laser powder bed fusion10.1002/adem.202401588 ↗
13. Influence of contour scans on surface roughness and pore formation using Scalmalloy® manufactured by laser powder bed fusion (PBF-LB)10.1002/mawe.202000287 ↗
14. Surface roughness in laser powder bed fusion – interdependency of surface orientation and laser incidence
15. Surface characteristics and roughness of laser powder bed fusion processed parts, laser powder bed fusion of additive manufacturing technology, springer nature Singapore
16. Laser polishing of laser powder bed fusion AlSi10Mg parts—influence of initial surface roughness on achievable surface quality
17. A study of the laser powder bed fusion manufactured surface roughness prediction and optimization based on artificial neural network
18. Process optimization for up-facing surface finish of AlSi10Mg alloy produced by Laser Powder Bed Fusion
19. Enhancing fatigue life of metal parts produced by high-speed laser powder bed fusion through in situ surface quality improvement
20. Effect of Hirtisation treatment on surface quality and mechanical properties of AlSi10Mg samples produced by laser powder bed fusion
21. Karimialavijeh · 2024
22. Surface post-treatments for metal additive manufacturing: Progress, challenges, and opportunities
23. Fatigue properties of Scalmalloy® processed by laser powder bed fusion in as-built, chemically and conventionally machined surface condition
24. Laser polishing: a review of a constantly growing technology in the surface finishing of components made by additive manufacturing10.1007/s00170-022-08840-x ↗
25. Laser polishing for improving fatigue performance of additive manufactured Ti-6Al-4V parts10.1016/j.optlastec.2020.106639 ↗
26. Marimuthu · Int. J. Mach. Tools Manuf. · 2015 · 95 · 9710.1016/j.ijmachtools.2015.05.002 ↗
27. CO2 laser polishing of laser-powder bed fusion produced AlSi10Mg parts10.1016/j.surfcoat.2021.127291 ↗
28. In-situ laser polishing additive manufactured AlSi10Mg: effect of laser polishing strategy on surface morphology, roughness and microhardness10.3390/ma14020393 ↗
29. Influence of laser polishing on the material properties of aluminium L-PBF components10.3390/met12050750 ↗
30. Laser polishing of additive manufactured aluminium parts by modulated laser power10.3390/mi12111332 ↗
31. Smoothing additive manufactured parts using ns-pulsed laser radiation10.1007/s40964-021-00168-4 ↗
32. Laser-based surface smoothing and subsequently interference patterning of additive manufactured materials to influence their wetting behavior10.1117/12.2608659 ↗
33. State of the art in laser surface texturing, ASMEDC, Manchester
34. Bringing the direct laser interference patterning method to industry: a one tool-complete solution for surface functionalization10.2961/jlmn.2015.03.0019 ↗
35. Laser interference metallurgy—periodic surface patterning and formation of intermetallics10.1016/j.intermet.2004.07.005 ↗
36. High throughput direct laser interference patterning of aluminum for fabrication of super hydrophobic surfaces10.3390/ma12091484 ↗
37. Fabrication of periodic micro-structures by holographic lithography10.3952/physics.v53i4.2765 ↗
38. Tailored wetting of copper using precise nanosecond direct laser interference patterning10.1016/j.optlaseng.2020.106364 ↗
39. The friction of surface textured cylinder liner segments modified by direct laser writing and direct laser interference patterning processes10.1016/j.jmapro.2024.03.008 ↗
40. Effectiveness of direct laser interference patterning and peptide immobilization on endothelial cell migration for cardio-vascular applications: an in vitro study10.3390/nano12071217 ↗
41. Laser-based surface modification and its influence on the topography and wettability of a new additively manufactured aluminum-based alloy10.1117/12.2608668 ↗
42. Fabrication of water- and ice-repellent surfaces on additive-manufactured components using laser-based microstructuring methods10.1002/adem.202101624 ↗
43. Surface functionalization of additively manufactured titanium alloy for orthopaedic implant applications10.1016/j.jmapro.2023.07.015 ↗
44. Two-step laser post-processing for the surface functionalization of additively manufactured Ti-6Al-4V parts10.3390/ma13214872 ↗
45. On the investigation of a sustainable two step laser-based surface treatment for the functionalization of additive manufactured Ti–6Al–4V components10.1002/adem.202501224 ↗
46. Topography analysis and homogeneity quantification of laser-patterned periodic surface structures
47. Process defects and in situmonitoring methods in metal powder bed fusion: a review10.1088/1361-6501/aa5c4f ↗
48. Design surfaces by laser Remelting10.1016/j.phpro.2011.03.053 ↗
49. Pulsed laser polishing of selective laser melted aluminium alloy parts10.1016/j.apsusc.2021.149887 ↗
50. Effect of heat treatment and laser surface remelting on AlSi10Mg alloy fabricated by selective laser melting10.1007/s00170-018-03272-y ↗
51. Effect of porosity distribution on the strength and strain-to-failure of laser-powder bed fusion printed Ti–6Al–4V
52. Impact of surface and pore characteristics on fatigue life of laser powder bed fusion Ti–6Al–4V alloy described by neural network models10.1038/s41598-021-99959-6 ↗
53. Fatigue life of laser powder bed fusion (L-PBF) AlSi10Mg alloy: Effects of surface roughness and porosity10.1007/s40964-024-00759-x ↗
54. Microstructural, porosity and mechanical properties of lap joint laser welding for 5182 and 6061 dissimilar aluminum alloys under different place configurations10.1016/j.matdes.2020.108625 ↗
55. Microstructural formation and characterization mechanisms of selective laser melted Al–Si–Mg alloys with increasing magnesium content10.1016/j.msea.2019.02.015 ↗
56. The influence of post-treatment on micropore Evolution and mechanical performance in AlSi10Mg alloy manufactured by laser powder bed fusion10.3390/ma17174319 ↗
57. Microstructure and properties of additively manufactured Al–Ce–Mg alloys10.1038/s41598-021-86370-4 ↗
58. Mechanical properties of high Mg-content Al-Mg-Sc-Zr alloy fabricated by selective laser melting10.1007/s12540-020-00907-2 ↗
59. A review on porosity formation in aluminum-based alloys10.3390/ma16052047 ↗
60. Single- and multiscale laser patterning of 3D printed biomedical titanium alloy: toward an enhanced adhesion and early differentiation of human bone marrow stromal cells
61. Influence of polarization angle on LIPSS formation and ablation efficiency in direct laser interference patterning of metals10.1038/s41598-025-07657-4 ↗
62. Optimized strategy for fabricating high-aspect-ratio periodic structures over large areas using ps-direct laser interference patterning10.1002/adem.202500570 ↗
63. Micro-fabrication of high aspect ratio periodic structures on stainless steel by picosecond direct laser interference patterning10.1016/j.jmatprotec.2017.09.039 ↗
64. Pulse duration and wavelength effects on the surface topography of direct laser interference patterning treated titanium specimen