journal article·2026-08Open access

Microstructural and micro-mechanical properties of FeCoNiCuAlx (x = 0.6–1.2) high-entropy alloy coatings regulated by Al element

Zhenqiao Zhang, Zhijie Zhang, Bo Zhu, Yingying Wang, Zhonghan Yu, Wenjuan Xing, Hu Huang, Yongfeng Qian, Puhong Xu, Hongwei Zhao

Abstract

To overcome the limited wear resistance and interfacial mismatch of high-strength 316 L stainless steel under wear conditions, FeCoNiCuAl x (x = 0.6–1.2) dual-phase high-entropy alloy coatings were fabricated by plasma cladding. An Al-induced strategy based on phase transformation and lattice-distortion strengthening was proposed to regulate both the coating matrix and the metallurgical bonding interface. This strategy provides a route for linking microstructural design with mechanical-property optimization. XRD, FESEM, EBSD, high-speed nanoindentation mapping, and nanoscratch tests were used to characterize the coatings. The results showed that increasing Al content promoted the transformation from a single FCC phase to an FCC + BCC dual-phase structure. The increased BCC fraction enhanced hardness and stiffness and promoted a more uniform mechanical response. The coating hardness increased from 3.5 GPa to 7.5 GPa, and the elastic modulus rose from approximately 155 GPa to over 195 GPa. Additionally, the interface transition zone widened with increasing Al content. The columnar grains transitioned from FCC to FCC + BCC dual-phase columnar grains. The interface hardness gradually transitioned from 3.0 GPa at the substrate to a maximum of 6.7 GPa at the coating, reflecting a significant and continuous gradient matching capability. Combined with the low residual stress measurement results, this indicates the formation of a favorable compositional–microstructural–mechanical property gradient matching, which is beneficial for reducing the risk of interfacial failure. Nanoscratch tests further showed that as Al increased, the scratches became narrower and shallower, and the material removal rate increased, with the wear mechanism gradually shifting from plowing dominance to a plowing-microcutting synergy. When Al reached 1.2, the material removal rate further increased, and micro-cracks appeared, indicating a trade-off between “increased strength and brittleness risk.” This study establishes the intrinsic relationship between Al content, phase structure, interface gradient, and wear mechanism. These findings provide quantifiable guidance for the composition design and interface reliability optimization of DHEA coatings.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: High Entropy Alloys Studies · High-Temperature Coating Behaviors · Magnesium Alloys: Properties and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (64)

Show source-provided references
1. Nanostructured high-entropy alloys with multiple principal elements: novel alloy design concepts and outcomes10.1002/adem.200300567 ↗
2. Microstructural development in equiatomic multicomponent alloys10.1016/j.msea.2003.10.257 ↗
3. Enhanced strength and ductility in a high-entropy alloy via ordered oxygen complexes10.1038/s41586-018-0685-y ↗
4. Metastable high-entropy dual-phase alloys overcome the strength-ductility trade-off10.1038/nature17981 ↗
5. Outstanding radiation resistance of tungsten-based high-entropy alloys10.1126/sciadv.aav2002 ↗
6. Microstructural stability and mechanical behavior of FeNiMnCr high entropy alloy under ion irradiation10.1016/j.actamat.2016.05.007 ↗
7. Effects of compositional complexity on the ion-irradiation induced swelling and hardening in Ni-containing equiatomic alloys10.1016/j.scriptamat.2016.03.030 ↗
8. Recent advances on environmental corrosion behavior and mechanism of high-entropy alloys10.1016/j.jmst.2020.11.044 ↗
9. Corrosion behavior of an equiatomic CoCrFeMnNi high-entropy alloy compared with 304 stainless steel in sulfuric acid solution10.1016/j.corsci.2018.02.031 ↗
10. Nanostructuring as a route to achieve ultra-strong high- and medium-entropy alloys with high creep resistance10.1016/j.jallcom.2020.154656 ↗
11. Irradiation induced creep in nanocrystalline high entropy alloys10.1016/j.actamat.2019.10.022 ↗
12. Nanomechanical studies of high-entropy alloys10.1557/jmr.2018.155 ↗
13. Microstructures and properties of high-entropy alloys10.1016/j.pmatsci.2013.10.001 ↗
14. Natural-mixing guided design of refractory high-entropy alloys with as-cast tensile ductility10.1038/s41563-020-0750-4 ↗
15. Nanostructured high-entropy materials10.1557/jmr.2020.33 ↗
16. Strengthening mechanisms in high entropy alloys: fundamental issues10.1016/j.scriptamat.2020.06.019 ↗
17. Microstructure evolution and critical stress for twinning in the CrMnFeCoNi high-entropy alloy10.1016/j.actamat.2016.07.038 ↗
18. Stacking fault strengthening in CoCrFeMnNi high-entropy alloy10.1063/5.0149734 ↗
19. Designing high entropy alloys with dual fcc and bcc solid-solution phases: structures and mechanical properties10.1007/s11661-019-05131-1 ↗
20. Promising properties and future trend of eutectic high entropy alloys10.1016/j.scriptamat.2020.06.022 ↗
21. A new approach to multi-phase formulation for the solidification of alloys10.1016/j.physd.2012.01.006 ↗
22. Achieving dual-phase structure and improved mechanical properties in AlCoCrFeTi0.5 high-entropy alloys by addition of Ni10.1016/j.msea.2021.142194 ↗
23. The regulating effect and mechanism of magnetic field on the synthesis of FeCoNiCuAl dual-phase high entropy alloy
24. Effect of valence electron concentration on stability of fcc or bcc phase in high entropy alloys10.1063/1.3587228 ↗
25. High-entropy alloy: challenges and prospects10.1016/j.mattod.2015.11.026 ↗
26. Research and progress of laser cladding: process, materials and applications
27. Temperature Gradient and Solidification Rate Simulation Model of the Microstructure of Laser-Cladded 27SiMn10.3390/met13101682 ↗
28. A review on coatings deposited by extreme high-speed laser cladding: processes, materials, and properties10.1016/j.optlastec.2023.109472 ↗
29. Development in PTA Surface Modifications – A Review10.2478/adms-2020-0009 ↗
30. Through-thickness microstructure and wear resistance of plasma transferred arc Stellite 6 cladding: Effect of substrate10.1016/j.cirpj.2023.01.014 ↗
31. Efficient Multi-Material and High Deposition Coating including Additive Manufacturing by Tandem Plasma Transferred Arc Welding for Functionally Graded Structures10.3390/met12081336 ↗
32. Review on wear resistance of laser cladding high-entropy alloy coatings10.1016/j.jmrt.2023.11.138 ↗
33. Tribology behavior in laser cladded dual-phase AlxCoCrFeNiMn(1-x) high entropy alloys influenced by hierarchical interface architecture10.1016/j.surfcoat.2023.129895 ↗
34. Microstructure and tribological properties of AlCoCrFeNi2.1 dual-phase high-entropy alloy enhanced by laser remelting10.1007/s11665-024-10219-w ↗
35. Properties of atomized AlCoCrFeNi high-entropy alloy powders and their phase-adjustable coatings prepared via plasma spray process10.1016/j.apsusc.2019.01.203 ↗
36. Effect of Dilution on Microstructure and Phase Transformation of AlCrFeMnNi High-Entropy Alloy by Resonant Ultrasonic Vibration-Assisted Laser Cladding10.3390/ma18030695 ↗
37. Microstructure and wear behavior of plasma cladded Ni-based alloy coating on copper under different preheating temperature10.1016/j.jmrt.2023.01.092 ↗
38. Kurz · 1998
39. High entropy alloys for energy conversion and storage: A review of grain boundary wetting phenomena10.3390/en15197130 ↗
40. Davis · 2001
41. Steen · 2010
42. Toyserkani · 2004
43. Microstructure and high-temperature wear behavior of CoCrFeNiWx high-entropy alloy coatings fabricated by laser cladding10.1016/j.triboint.2022.107574 ↗
44. Microstructure characterization and high-temperature wear mechanism of high-entropy alloy matrix composite coating fabricated by laser cladding10.1016/j.apsusc.2024.161032 ↗
45. Nanotwin’s formation and growth in an AlCoCuFeNi high-entropy alloy10.1016/j.scriptamat.2015.11.032 ↗
46. Fast and high-throughput synthesis of medium-and high-entropy alloys using radio frequency inductively coupled plasma10.1002/adem.202001116 ↗
47. The effect of Al on the phase formation and micromechanical property of FeCoNiCuAlx (x = 0.6–1.2)10.1016/j.matchar.2025.115929 ↗
48. Temperature gradient driving interdiffusion interface and composition evolution in Ni–Al–Cr alloys10.1007/s12598-022-02024-y ↗
49. On the effect of steel substrate alloying elements on the in-situ formation of intermediate thermal diffusion barrier layers10.1016/j.matchemphys.2019.122231 ↗
50. Enhanced migration of mono-vacancies in AlxFeCoCrNi high entropy alloys10.1016/j.jallcom.2024.177704 ↗
51. Deformation Enhanced Diffusion in Aluminium Alloys10.1007/s11661-020-05960-5 ↗
52. Thermodynamic modelling of growth-restriction effects in aluminium alloys10.1016/j.actamat.2004.11.024 ↗
53. Evaluation of microstructure and mechanical property variations in AlxCoCrFeNi high entropy alloys produced by a high-throughput laser deposition method10.1016/j.intermet.2018.01.021 ↗
54. The redistribution of solute atoms during the solidification of metals10.1016/0001-6160(53)90126-6 ↗
55. Theory of microstructural development during rapid solidification10.1016/0001-6160(86)90056-8 ↗
56. Microstructure development during rapid alloy solidification10.1557/s43577-024-00717-6 ↗
57. Modeling Phase Selection and Extended Solubility in Rapid Solidified Alloys10.1007/s11661-023-07221-7 ↗
58. Measurement of hardness and elastic modulus by instrumented indentation: Advances in understanding and refinements to methodology10.1557/jmr.2004.19.1.3 ↗
59. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
60. Effects of the deflection angle of the indenter on the material removal and damage evolution of fused silica during scratching10.1016/j.jmapro.2024.03.037 ↗
61. Electrodeposited metallic glasses with superlative wear resistance10.1016/j.msea.2021.141315 ↗
62. Effects of the indenter orientation and the crystallographic orientation on the scratch characteristics of FeCoCrMnNi high entropy alloy10.1016/j.wear.2024.205694 ↗
63. Material removal behaviors of FCC metals in nanoscale and microscale scratching: theoretical model and experiments10.1016/j.jmatprotec.2022.117855 ↗
64. The scratch behaviour of AlXCoCrFeNi (x=0.3 and 1.0) high entropy alloys10.1016/j.wear.2019.03.026 ↗