Microstructure and oxidation resistance of Si-modified aluminide coatings prepared by slurry sintering on K447A superalloy
Bibliographic record
Abstract
No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.
Source: Not provided · Quality: missing
Research context
OpenAlex topics: Intermetallics and Advanced Alloy Properties · High-Temperature Coating Behaviors · Material Properties and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (40)
Show source-provided references
1. Effect of Si addition to improve the performance of type II and type I hot corrosion resistance of aluminide coating10.1016/j.corsci.2022.110937 ↗
2. nickel-based superalloys
3. A review of gas turbine engine with inter-stage turbine burner10.1016/j.paerosci.2020.100695 ↗
4. Review of modern low emissions combustion technologies for aero gas turbine engines10.1016/j.paerosci.2017.08.001 ↗
5. Approach for statistical analysis of oxide- and sulfate-induced hot corrosion of advanced alloys10.1016/j.corsci.2022.110892 ↗
6. Influence of microstructure on the oxidation behaviour of the Ni-based single crystal superalloy AM1 between 850 and 1050°C in air10.1016/j.corsci.2024.111872 ↗
7. Oxidation performance of aluminide coating on Inconel 783 bolts for ultra-supercritical steam turbine application10.1016/j.corsci.2021.110033 ↗
8. Research progress on aluminized coatings for high temperature blades
9. Improving oxidation resistance of aluminide coatings by alloying elements from underlying superalloys10.1016/j.corsci.2024.112568 ↗
10. Self healing in coatings at high temperatures
11. Chlorine-induced high-temperature corrosion of the Pt-modified aluminide coating in simulated marine environment10.1016/j.corsci.2023.111493 ↗
12. The role of silicon in corrosion-resistant high temperature coatings10.1016/0040-6090(82)90578-8 ↗
13. Microstructure and hot corrosion behaviors of two co modified aluminide coatings on a Ni-based superalloy at 700 °C10.1016/j.apsusc.2014.05.043 ↗
14. Chromium and reactive element modified aluminide diffusion coatings on superalloys: environmental testing10.1149/1.2056220 ↗
15. Effects of coating growth mode on the oxidation behavior of a hybrid Pt/Ru-modified aluminide coating at 1200°C10.1016/j.corsci.2023.111608 ↗
16. Effect of Si and Cr on formation of aluminide coatings on Ti6Al4V alloy by low temperature aluminizing: wear and oxidation behavior10.1016/j.surfcoat.2025.132207 ↗
17. Single-phase Si-modified β-NiAl coatings with molten Na2SO4+NaCl salts-induced corrosion behavior at 700 and 900°C10.1016/j.jmst.2025.02.084 ↗
18. Cyclic oxidation behaviour of co/Si co-doped β-NiAl coating on nickel based superalloys10.1016/j.corsci.2018.01.032 ↗
19. The effect of silicon on thermal shock performance of aluminide-thermal barrier coatings10.1016/j.corsci.2013.05.025 ↗
20. Oxidation and microstructure evolution of Al-Si coated Ni3Al based single crystal superalloy with high Mo content10.1016/j.apsusc.2014.11.076 ↗
21. Oxidation behaviour of the nickel-based superalloy DZ125 hot-dipped with Al coatings doped by Si10.1016/j.corsci.2016.07.020 ↗
22. Microstructure evaluation of Si-modified aluminide coatings on IN625 deposited by slurry aluminizing process10.1016/j.surfcoat.2024.131592 ↗
23. Thermal–mechanical fatigue behaviour of a new single crystal superalloy: effects of Si and Re alloying10.1016/j.actamat.2015.03.060 ↗
24. Microstructures of thin and thick slurry aluminide coatings on Inconel 69010.1016/j.surfcoat.2007.06.056 ↗
25. Cyclic oxidation and mechanical behaviour of slurry aluminide coatings for steam turbine components10.1016/j.surfcoat.2006.11.033 ↗
26. Potential thermal barrier coating systems from Al microparticles. Mechanisms of coating formation on pure nickel10.1016/j.matchemphys.2012.03.053 ↗
27. Mechanisms of formation of diffusion aluminide coatings on nickel-base superalloys10.1007/BF00604047 ↗
28. Preparation and microstructure evolution of Ni-Al-Pt bong cotings
29. Phase transformation of Ni2Al3 to NiAl. I. Ion irradiation induced10.1063/1.334546 ↗
30. The Al-Ni-Si phase diagram. Part II: phase equilibria between 33.3 and 66.7 at.% Ni10.1016/j.intermet.2004.01.009 ↗
31. Substrate effect on the high-temperature oxidation behavior of a Pt-modified aluminide coating. Part I: influence of the initial chemical composition of the coating surface10.1007/s11085-006-9024-z ↗
32. Effect of water vapour on morphology of the Si/Ti-rich phase at the interface between oxide layer and aluminide coating10.1016/j.corsci.2019.108240 ↗
33. Unraveling β-NiAl degradation in aluminide coatings: a comparative study of isothermal oxidation and vacuum heat treatment10.1016/j.corsci.2025.112946 ↗
34. Concentration of point defects and site occupancy behavior in ternary NiAl alloys10.1016/j.msea.2003.09.010 ↗
35. Understanding dopants (Pt, Re, Hf, Zr, Y) on NiAl grain boundary diffusion and NiAl/Al2O3 interfacial adhesion10.1016/j.corcom.2024.07.004 ↗
36. The effect of silicon on cyclic oxidation behavior of aluminide coatings on superalloy IN-738LC
37. Experimental investigation of phase equilibria in the Ni-Cr-Si ternary system10.1007/s11669-014-0279-9 ↗
38. Cyclic oxidation–guidelines for test standardization, aimed at the assessment of service behaviour
39. The effect of TCP morphology on the development of aluminide coated superalloys10.1016/j.msea.2005.01.005 ↗
40. On the role of μ phase during high temperature creep of a second generation directionally solidified superalloy10.1016/j.msea.2010.04.090 ↗