journal article·2018-08

The corrosion behaviours of plasma-sprayed Fe-based amorphous coatings

Chaoping Jiang, Wangqiang Liu, Gui Wang, Yongnan Chen, Yazhe Xing, Chunhua Zhang, Matthew Dargusch

Surface Engineering· Volume 34· Issue 8
Publisher page

Abstract

Fe-based amorphous coatings are increasingly recognised as promising candidates for the protection of coal-fired boilers against corrosion. The present study prepared Fe-based amorphous coatings on a T91 substrate by plasma spraying technology. The corrosion behaviour of the coating in hot Na 2 SO 4 + K 2 SO 4 salts at 700°C was investigated, and measurements of the mean mass gain were performed after each cycle to establish the hot corrosion kinetics of the coatings using the thermogravimetric technique. The coated specimens, especially specimens with 380-μm-thick coatings, exhibited lower mean gain rates at all operating cycles as compared to the uncoated T91 samples. The highest hot corrosion resistance was a result of the amorphous composite microstructure and high Cr and Ni elemental contents, which contributed to the formation of the protective oxides of chromium and nickel such as Cr 2 O 3 , NiO and NiCr 2 O 4 .
Source: crossref · Quality: baseline

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Metallic Glasses and Amorphous Alloys · Diamond and Carbon-based Materials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

School of Materials Science and Engineering, Chang'an University, Xi'an, China

Centre for Advanced Materials Processing and Manufacture, School of Mechanical and Mining Engineering, The University of Queensland, St Lucia, Australia

School of Automobile, Chang'an University, Xi'an, China

Funding

Chang an university · Natural Science Foundation of Shaanxi Province

References (25)

Show source-provided references
1. International Energy Agency (IEA). Key energy statistics; 2009. See also: http://www.iea.org.
2. 10.1016/j.fuel.2010.06.01310.1016/j.fuel.2010.06.013 ↗
3. 10.1016/j.fuel.2010.05.00810.1016/j.fuel.2010.05.008 ↗
4. 10.1016/S0257-8972(00)00523-510.1016/S0257-8972(00)00523-5 ↗
5. 10.1016/j.supflu.2012.08.01510.1016/j.supflu.2012.08.015 ↗
6. 10.1016/j.surfcoat.2012.01.06010.1016/j.surfcoat.2012.01.060 ↗
7. 10.1016/j.corsci.2003.09.02610.1016/j.corsci.2003.09.026 ↗
8. 10.1016/j.corsci.2005.04.00610.1016/j.corsci.2005.04.006 ↗
9. 10.1179/1743294414Y.000000033810.1179/1743294414Y.0000000338 ↗
10. 10.1179/026708409X1249036042596310.1179/026708409X12490360425963 ↗
11. 10.1016/j.surfcoat.2015.03.02210.1016/j.surfcoat.2015.03.022 ↗
12. Science and Technology Review. Lawrence Livermore National Laboratory; 2009.
13. 10.31399/asm.cp.itsc1999p047410.31399/asm.cp.itsc1999p0474 ↗
14. 10.1016/S0257-8972(01)01679-610.1016/S0257-8972(01)01679-6 ↗
15. 10.1080/0950083050047971810.1080/09500830500479718 ↗
16. 10.1016/j.corsci.2015.01.02210.1016/j.corsci.2015.01.022 ↗
17. 10.1016/j.corsci.2006.05.00310.1016/j.corsci.2006.05.003 ↗
18. 10.1016/j.corsci.2011.05.06210.1016/j.corsci.2011.05.062 ↗
19. 10.1016/j.jallcom.2007.11.08310.1016/j.jallcom.2007.11.083 ↗
20. 10.1016/j.corsci.2013.01.00410.1016/j.corsci.2013.01.004 ↗
21. 10.1016/j.intermet.2012.03.02610.1016/j.intermet.2012.03.026 ↗
22. 10.1016/S0257-8972(02)00468-110.1016/S0257-8972(02)00468-1 ↗
23. 10.1361/105996306X14716210.1361/105996306X147162 ↗
24. 10.1016/j.surfcoat.2008.10.01310.1016/j.surfcoat.2008.10.013 ↗
25. 10.1016/S0921-5093(02)00072-210.1016/S0921-5093(02)00072-2 ↗