Abstract
Titanium nitride (TiN) coatings were deposited on mild steel (MS) by direct current reactive magnetron sputtering. With the aim of improving the corrosion resistance of TiN, an additional nickel interlayer was brush plated on the steel substrates before TiN film formation. The phases have been identified with X-ray diffraction analysis. The hardness values of TiN layers were found to increase with the increase in thickness of the Ni interlayer. The wear track investigations of TiN layers showed that the TiN/MS system was worn out by abrasive wear mechanism while on the film with Ni interlayer is by adhesive wear. It was found that the TiN/Ni/MS stack had a weaker tendency towards corrosion and higher corrosion resistance in 3·5%NaCl than the bare MS substrate, Ni/MS and TiN/MS specimen.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Metal and Thin Film Mechanics · GaN-based semiconductor devices and materials · Diamond and Carbon-based Materials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
ECMS Division, Central Electrochemical Research Institute, Karaikudi 630006, India;, Email: subramanianb3@gmail.com
ECMS Division, Central Electrochemical Research Institute, Karaikudi 630006, India
Department of Mechanical EngineeringA.C. College of Engineering and Technology, Karaikudi 630006, India
Department of PhysicsNational Institute of Technology, Trichy 620015, India
Department of PhysicsThanthai Hans Rover College, Perambalur – 621212, India
References (29)
Show source-provided references
1. Hems J. · Semicond Int. · 1990 · 12 · 100
2. 10.1116/1.57289910.1116/1.572899 ↗
3. 10.1016/j.ceramint.2003.12.04210.1016/j.ceramint.2003.12.042 ↗
4. 10.1016/j.microrel.2007.01.01410.1016/j.microrel.2007.01.014 ↗
5. 10.1002/1527-2648(200101)3:1/2<49::AID-ADEM49>3.0.CO;2-H10.1002/1527-2648(200101)3:1/2<49::AID-ADEM49>3.0.CO;2-H ↗
6. 10.1016/j.tsf.2005.08.20310.1016/j.tsf.2005.08.203 ↗
7. 10.1063/1.12296310.1063/1.122963 ↗
8. 10.1016/S0257-8972(02)00652-710.1016/S0257-8972(02)00652-7 ↗
9. Na H. D. · Surf Coat. Technol. · 2003 · 41 · 169
10. 10.1016/S0257-8972(96)02870-810.1016/S0257-8972(96)02870-8 ↗
11. 10.1016/S0010-938X(02)00223-810.1016/S0010-938X(02)00223-8 ↗
12. 10.1080/00202967.2004.1187157310.1080/00202967.2004.11871573 ↗
13. 10.1016/S0257-8972(99)00551-410.1016/S0257-8972(99)00551-4 ↗
14. 10.1016/S0040-6090(00)01258-X10.1016/S0040-6090(00)01258-X ↗
15. 10.1016/S0257-8972(01)01041-610.1016/S0257-8972(01)01041-6 ↗
16. 10.1149/1.153471110.1149/1.1534711 ↗
17. 10.1016/S0257-8972(01)01041-610.1016/S0257-8972(01)01041-6 ↗
18. 10.1016/j.cap.2006.09.00310.1016/j.cap.2006.09.003 ↗
19. 10.1063/1.12662610.1063/1.126626 ↗
20. 10.1116/1.58221910.1116/1.582219 ↗
21. 10.1063/1.12662610.1063/1.126626 ↗
22. Rickerby D. S., and Bull S. J.: Proc. 16th Leeds-Lyon Symp. on ‘Tribology: mechanics of coatings’, (ed. Dowson D. et al), 337; 1990, Amsterdam, Elsevier.
23. Thornton J. A. · J. Vac. Sci. Technol. A · 1986 · 4 · 230910.1116/1.573628 ↗
24. 10.1016/0257-8972(88)90014-X10.1016/0257-8972(88)90014-X ↗
25. 10.1116/1.57406210.1116/1.574062 ↗
26. 10.1016/0257-8972(93)90259-Q10.1016/0257-8972(93)90259-Q ↗
27. 10.1080/00202967.2000.1187129910.1080/00202967.2000.11871299 ↗
28. Ko K. H. · Korean J. Mater. Res. · 1995 · 5 · 960
29. 10.1016/S0254-0584(98)00071-610.1016/S0254-0584(98)00071-6 ↗