Thermal spray coatings of Ni–10 wt-%Al composite powder synthesised by low energy mechanical milling
Source abstract
Abstract
Ni–10 wt-%Al composite powders, as a self-bonding spray material, were prepared by low energy mechanical milling process and then sprayed by plasma and flame spray techniques. The phase identification, microstructure, hardness and adhesion strength of the coatings were investigated by X-ray diffraction, SEM, ASTM E384-99 and ASTM C633-01 respectively. The size and microstructure of powder particles are two important parameters for thermal spraying. Morphological and microstructural investigation of the Ni–10 wt-%Al powders showed that the powder particles after 23 h of milling time had the optimum properties with respect to their size and microstructure. X-ray diffraction patterns of powder particles included only the elemental Ni and Al peaks without any traces of oxides or intermetallics phases. Powder particles produced by mechanical milling had a fine lamellar structure consisting of pure Al and Ni layers. This structure encourages the Ni/Al exothermic reaction during flight in plasma spraying. The adhesive tests also showed that the plasma and flame failure were cohesive, that is, within the coating itself, because adhesive on steel in both coatings is much higher than cohesive.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Advanced materials and composites · Intermetallics and Advanced Alloy Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Material Engineering, Isfahan University of Technology, Isfahan 84156 83111, Iran
References (28)
Show source-provided references
1. Unger R. H.: Proc. Natl Thermal Spray Conf., OH, USA, ASM International, Cincinnati, October 1988, 147, 321–324.
2. Pawlowski L. · 1995
3. 10.1016/S0257-8972(02)00018-X10.1016/S0257-8972(02)00018-X ↗
4. 10.1016/S0257-8972(01)01594-810.1016/S0257-8972(01)01594-8 ↗
5. 10.1007/s11666-997-0068-710.1007/s11666-997-0068-7 ↗
6. Knotek O., Lugscheider E., and Eschnauer H. R.: Proc. 7th Int. Metal Spray Conf., London, September 1973, Welding Institute, 72.
7. Sampath S., Gudrnundsson B., Tiwari R., and Herman H.: Proc. 3rd Natl Thermal Spray Conf., Long Beach, May 1990, ASM International, 357.
8. 10.1016/S0966-9795(02)00088-210.1016/S0966-9795(02)00088-2 ↗
9. Allan M. L. · BNL Report · 1998
10. 10.1016/S0257-8972(99)00511-310.1016/S0257-8972(99)00511-3 ↗
11. Rangaswamy S. · US patent no. 5 385 789 · 1995
12. 10.1016/S0921-5093(03)00110-210.1016/S0921-5093(03)00110-2 ↗
13. Dittrich F. J. · US patent no. 3436248 · 1969
14. 10.1016/S1359-6454(99)00059-210.1016/S1359-6454(99)00059-2 ↗
15. Rangaswamy S. · US patent no. 5631044 · 1997
16. Suryanarayana C. · Frog. Mater. Sci. · 2001 · 46 · 1
17. El-Eskandarany M. S. · 2001
18. 10.1007/BF0053997510.1007/BF00539975 ↗
19. ASTM E384-99 · 2002
20. ASTM C633-01 · 2001
21. Smyth R. T.: Proc. 7th Int. Metal Spray Conf., London, UK, September 1973, Welding Institute, 89-95.
22. Nelson R. L., Woodhead J. L., and Wassell L. L.: Proc. 7th Int. Metal Spray Conf., London, UK, September 1973, Welding Institute, 96-101.
23. 10.1016/S0921-5093(01)01986-410.1016/S0921-5093(01)01986-4 ↗
24. 10.1016/j.msea.2003.08.02310.1016/j.msea.2003.08.023 ↗
25. 10.1016/S0257-8972(03)00202-010.1016/S0257-8972(03)00202-0 ↗
26. 10.1016/S0925-8388(01)01905-310.1016/S0925-8388(01)01905-3 ↗
27. Shimizu Y., Sato M., and Kobayashi M.: Proc. 4th Thermal Spray Conf., Pittsburgh, PA, USA, May 1991, ASM International, 257-262.
28. 10.1007/BF0264900310.1007/BF02649003 ↗