journal article·2015-04

Electrochemical behaviour of X80 pipeline steel with alumina coating

M. Huang, M-X. Zhang, Y. Wang, P. Zhang, A-J. Xu

Surface Engineering· Volume 31· Issue 4
Publisher page

Abstract

X80 pipeline steel was firstly aluminised at a relative low temperature then treated by a microarc oxidation process. Electrochemical behaviour of X80 pipeline steel before and after the combined treatment was evaluated by electrochemical tests in different solution. Results show that ceramics coating composed of α-Al2O3 and γ-Al2O3 can be obtained on the surface of X80 pipeline steel by the combined treatment. In neutral 3·5% NaCl solution and alkaline solution (pH = 9), X80 pipeline steel with ceramics coating shows a higher corrosion potential and a lower corrosion current density than pure steel and the X80 pipeline steel treated by one-step aluminising. However, aluminising coating presents a better corrosion protection for X80 pipeline steel than that of ceramic coating in acidic solution with pH = 5. γ-Al2O3 is considered as the main reason for the corrosion resistance degradation of ceramic coating in acidic solution.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals · High-Temperature Coating Behaviors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Zhejiang Provincial Key Laboratory for Cutting Tools Taizhou University, Taizhou 318000, China

School of Materials Science and Engineering Xi'an Shiyou University, Xi'an 710065, China

References (18)

Show source-provided references
1. 10.1016/S1006-706X(10)60076-310.1016/S1006-706X(10)60076-3 ↗
2. 10.1016/j.msea.2007.11.14610.1016/j.msea.2007.11.146 ↗
3. 10.1016/S0257-8972(96)02862-910.1016/S0257-8972(96)02862-9 ↗
4. 10.1016/j.corsci.2012.08.04810.1016/j.corsci.2012.08.048 ↗
5. 10.1016/j.matdes.2013.06.00210.1016/j.matdes.2013.06.002 ↗
6. 10.1016/j.surfcoat.2011.01.02310.1016/j.surfcoat.2011.01.023 ↗
7. 10.1016/j.surfcoat.2010.06.01510.1016/j.surfcoat.2010.06.015 ↗
8. 10.1016/j.surfcoat.2005.10.03610.1016/j.surfcoat.2005.10.036 ↗
9. 10.1016/j.materresbull.2012.09.01710.1016/j.materresbull.2012.09.017 ↗
10. 10.1016/j.surfcoat.2009.10.02310.1016/j.surfcoat.2009.10.023 ↗
11. 10.1016/j.apsusc.2010.11.18710.1016/j.apsusc.2010.11.187 ↗
12. 10.1016/j.apsusc.2013.12.02810.1016/j.apsusc.2013.12.028 ↗
13. 10.1016/j.scriptamat.2008.01.03310.1016/j.scriptamat.2008.01.033 ↗
14. 10.1016/S1003-6326(10)60563-810.1016/S1003-6326(10)60563-8 ↗
15. 10.1016/j.apsusc.2011.01.04710.1016/j.apsusc.2011.01.047 ↗
16. 10.1016/j.powtec.2013.07.00210.1016/j.powtec.2013.07.002 ↗
17. 10.1016/j.jallcom.2011.08.10310.1016/j.jallcom.2011.08.103 ↗
18. Wang Y · J. Mater. Sci. Technol. · 2009 · 25 · 513