Study of high temperature oxidation kinetics of Co–Al coating on superalloy
Source abstract
Abstract
Nanostructured Co–Al coating on Superni-718 substrate was deposited by dc/rf magnetron sputtering. The high temperature oxidation kinetics of Co–Al coating on superalloy substrate was studied after 100 h of cyclic oxidation in air environment at 700–900°C. FE-SEM/EDS, AFM and XRD were used to characterise the microstructure, surface morphology and phase constituents of as deposited and oxidised coatings. The results indicate that the Co–Al coated superalloy substrate has higher oxidation resistance at 900°C. The presence of β-CoAl intermetallic phase in the Co–Al coating, the formation of Al2O3 and spinel phases such as CoCr2O4 and CoAl2O4 in the oxide scale are considered to be the reasons for the higher oxidation resistance shown by the Co–Al coated superalloy substrate after 100 h of cyclic oxidation in air at 900°C. Further, the oxide scale formed on the coated sample exhibits good spallation resistance during cyclic oxidation test at 900°C.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Intermetallics and Advanced Alloy Properties · Catalytic Processes in Materials Science
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Metallurgical and Materials Engineering National Institute of Technology Srinagar Hazratbal, Srinagar, Kashmir 190006, India
Department of Metallurgical and Materials Engineering Indian Institute of Technology Roorkee, Roorkee 247667, India
Institute Instrumentation Centre, Indian Institute of Technology Roorkee, Roorkee 247667, India
References (17)
Show source-provided references
1. 10.1179/174329409X45116410.1179/174329409X451164 ↗
2. 10.1179/026708410X1245934972013210.1179/026708410X12459349720132 ↗
3. 10.1179/026708409X1249036042596310.1179/026708409X12490360425963 ↗
4. 10.1179/026708410X1255077305814410.1179/026708410X12550773058144 ↗
5. Mahesh RA · Corros. Eng. Sci. Technol. · 2008 · 42 · 142
6. 10.1179/026708409X36493910.1179/026708409X364939 ↗
7. 10.1179/174329408X29824710.1179/174329408X298247 ↗
8. 10.1179/026708408X37527110.1179/026708408X375271 ↗
9. 10.1179/026708408X32947010.1179/026708408X329470 ↗
10. 10.1007/s11085-010-9189-310.1007/s11085-010-9189-3 ↗
11. 10.1016/j.jallcom.2008.04.09110.1016/j.jallcom.2008.04.091 ↗
12. 10.1179/026708408X33906410.1179/026708408X339064 ↗
13. 10.1007/s11085-010-9217-310.1007/s11085-010-9217-3 ↗
14. 10.1016/j.surfcoat.2007.08.02210.1016/j.surfcoat.2007.08.022 ↗
15. 10.1116/1.57260410.1116/1.572604 ↗
16. Viswanathan R, Purgert R: Proc. 8th Int. Conf. on ‘Creep and fatigue at elevated temperatures’, San Antonio, TX, USA, July 2007, ASME, Paper CREEP 2007-26826.
17. 10.1016/j.msea.2007.04.10810.1016/j.msea.2007.04.108 ↗