Tribological studies on laser surface melted Hastelloy C-276

M Hashim, K E Sarath Raghavendra Babu, M Duraiselvam, H Natu, V Muthupandi, K Sivaprasad, K R Rajith

Surface Engineering· Volume 29· Issue 7
Publisher page

Abstract

Hastelloy C-276 was laser surface melted in a nitrogen environment in order to improve the wear resistance. The metallurgical characterisation was performed using optical microscopy, scanning electron microscopy with electron dispersive spectroscopy (EDS) and X-ray diffraction analysis. At a particular laser power and scan speed combination, significant grain refinement was achieved with finely dispersed cell-like structure which improved the hardness up to 390 HV0·3. The EDS point analysis indicated nitrogen diffusion at the cost of nickel depletion. The absence of Cr2N or CrN is a positive aspect in preserving the intrinsic corrosion characteristics of the alloy. The wear rates of the laser treated specimens were significantly lower by a factor of 2·5. Potentiodynamic polarisation corrosion test on the laser treated specimens also exhibited reduced corrosion rates compared to the base material.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research · Advanced Materials Characterization Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Production Engineering National Institute of Technology, Tiruchirappalli, Tamil Nadu, India

Department of Technical Education, Andhra Pradesh, India

Magod Laser Machining Private Limited Bangalore, India

Department of Metallurgical and Materials Engineering National Institute of Technology, Tiruchirappalli, Tamil Nadu, India

References (17)

Show source-provided references
1. 10.1016/j.phpro.2010.08.03410.1016/j.phpro.2010.08.034 ↗
2. 10.1016/S0169-4332(02)00421-X10.1016/S0169-4332(02)00421-X ↗
3. 10.1179/026708410X1245934971993610.1179/026708410X12459349719936 ↗
4. 10.1007/BF0240285410.1007/BF02402854 ↗
5. 10.1016/j.apsusc.2008.04.04210.1016/j.apsusc.2008.04.042 ↗
6. 10.1179/1743294411Y.000000005110.1179/1743294411Y.0000000051 ↗
7. 10.1016/S0169-4332(99)00257-310.1016/S0169-4332(99)00257-3 ↗
8. 10.1007/978-1-84996-062-5_610.1007/978-1-84996-062-5_6 ↗
9. 10.1179/1743294412Y.000000004910.1179/1743294412Y.0000000049 ↗
10. 10.1179/1743294411Y.000000002310.1179/1743294411Y.0000000023 ↗
11. 10.1179/026708408X32950610.1179/026708408X329506 ↗
12. 10.1179/174329407X26060910.1179/174329407X260609 ↗
13. ‘Standard test method for wear testing with a pin-on-disk apparatus’, G99-05, ASTM, West Conshohocken, PA, USA, 2010.
14. ‘Standard Reference test method for making potentiostatic and potentiodynamic anodic polarization measurements 1’, G61-04, ASTM, West Conshohocken, PA, USA, 2011.
15. 10.1007/s11661-011-0978-310.1007/s11661-011-0978-3 ↗
16. 10.1016/j.matdes.2012.10.02410.1016/j.matdes.2012.10.024 ↗
17. Schweitzer PA: ‘Fundamentals of corrosion: mechanisms, causes, and preventative methods’, 1st edn, 32–35; 2010, Boca Raton, FL, CRC Press/Taylor & Francis Group.10.1201/9781420067712 ↗